(Fwd) Inquiry on maximum temperature (3 messages)
0201 inspection and rework tools (1 message)
0402 pad design (1 message)
63/37 solder paste with silver plated boards (6 messages)
<No subject> (1 message)
A "NEDA" Oriented label... (1 message)
abrasive for cleaning PCB surfaces (2 messages)
AM79C970AVIW Ethernet Controller IC (1 message)
Anti-voiding solder paste (6 messages)
Antwort: [TN] BGA X-ray Cross Section services - Vendors? (1 message)
assembly spacing (3 messages)
ASSY: Component Polarity (11 messages)
ASSY: Component Polarity - part 2 (1 message)
ASSY: Reflow for Through-Hole Devices (8 messages)
bare board serialization (4 messages)
BGA replacement (17 messages)
BGA SMD vs NSMD (2 messages)
BGA solder anomalies (3 messages)
BGA Solderability (13 messages)
BGA warpage - defects in the corners. (7 messages)
BGA X-ray Cross Section services - Vendors? (7 messages)
BGA's on ruggedized assemblies... (10 messages)
Board analysis (2 messages)
board baking (2 messages)
Board Cost (2 messages)
Board defect? Purple spot (5 messages)
BOARD EDGE CLEARANCE (2 messages)
Cell phone antenna enhancers... (6 messages)
Cell phone antenna enhancers...NTC (41 messages)
Cell phone antenna enhances...NTC (10 messages)
Ceramic filled Teflon board (5 messages)
Class 3 Solder Fillets - SMT 25 mil square pin Headers? (5 messages)
Cleaning of No-clean Assemblies (14 messages)
CLEARANCE FRON PWB EDGES (2 messages)
Coating thickness (5 messages)
conductive blind via plug (9 messages)
Conformal Coating (22 messages)
Conformal coating / gluing (7 messages)
Conformal coating BGAs (11 messages)
Crimp Tools (2 messages)
Crimped connections (15 messages)
Cycle Time for Solder Paste Printing (2 messages)
D.O.E (12 messages)
D2PAK devices (4 messages)
Danny Harkins/CSI is out of the office. (1 message)
Dielectric constant for cores and prepeg (1 message)
Dielectric Constants For Core and Prepreg (5 messages)
Dielectric material vs. Solder mask (1 message)
DPMO benchmarking (1 message)
dross disposal (5 messages)
Econonic Boom (1 message)
Electrical Isolation in dbm ? (2 messages)
Electronics Manufacturers Association Meeting (Seattle) (1 message)
ESD and equipment isolation (5 messages)
Eutectic solder paste on silver plated boards (2 messages)
ExposedCu (2 messages)
Film Capacitors...geeze! (6 messages)
Fire Up for IPC Annual Meeting 2002 (3 messages)
First Article Inspection of bare boards (4 messages)
Flip-flop panels (2 messages)
Flux on top of PCBs from wave (4 messages)
fLUX RESIDUE IN NO CLEAN SOLDER WIRE (3 messages)
For Francois in case this didn't get posted to the technet (2 messages)
FPBGA Area Ratio Question (8 messages)
Gold Reclaim (1 message)
good to be back (1 message)
Guidelines or standards for number of missing unused BGA pads allowed (4 messages)
HDI and Sanmina (12 messages)
High lead composition solder paste and rinse water. (9 messages)
high Tg FR4 (1 message)
High Voltage tracking on pbc surface (12 messages)
hole plating peel test (1 message)
Hole routing in PCBs (7 messages)
HTML 3.2 (1 message)
Interesting addition to an ealier discussion (1 message)
IPC-4552 spec for ENIG (2 messages)
IPC-DC Boston area mtg, 21-May (1 message)
Keeping RA and OA flux separate (4 messages)
Locating Jay Brusse (2 messages)
Looking for a capacitance meter (6 messages)
Looking for A Solderability Spec (6 messages)
Looking for A Solderability Spec - No technical content contained (5 messages)
Looking for place who offer classes on ICT/DFT in Bay Area (1 message)
Looking for recent PCB Reliability model (3 messages)
Low Temp BGA Balls (4 messages)
Mark Orlowski/PEMSTAR Inc is out of the office. (1 message)
Mechanical Strength of Solder Joints (1 message)
Metal core PCB's (6 messages)
Mil spec approval (6 messages)
no clean paste for High frequencies (3 messages)
No Clean? (1 message)
NTC - The Gregory's are a team now... (10 messages)
OT Cell phone antenna enhances...NTC (2 messages)
OT- wasn't an experiment.. (3 messages)
Palladium Leads (11 messages)
Palladium Leads - Flux Choices (1 message)
Panelization sanity check needed (6 messages)
Parts List Definition (4 messages)
pcb design (5 messages)
PCB MATERIAL with low OUTGASSING Characteristics.... (1 message)
PCB materials (9 messages)
Plant closures (3 messages)
power traces (1 message)
Productivity Way Up (17 messages)
Productivity Way Up - Off topic (3 messages)
Proposed lifting of component date code restrictions (2 messages)
PTH Vertical Fill Requirement IPC610 Rev. C (8 messages)
Re column grid arrays (2 messages)
Re Hole Fill (2 messages)
ReA610HoleFill (4 messages)
really big boards (15 messages)
really big boards - all humor, no tech value (4 messages)
Recommended solder paste for a 6 layer double-sided board with CSP & BGA packages (1 message)
Reflow Oven Recommendations (2 messages)
Repair/Mod pads (5 messages)
RePalladium Leads (2 messages)
Restoring solderability (6 messages)
resume post (1 message)
Rod Smith/Endicott/IBM is out of the office. (1 message)
safety committee (4 messages)
Sanmina HDI (1 message)
Sanminaized (1 message)
Shear stress on laser vias (1 message)
Side fillet requirements (9 messages)
Solder after reflow on Gold Immersion finish (3 messages)
Solder Defect Rates (1 message)
Solder-UBM Separation (3 messages)
soldermask ring v. full coat for BGA design (5 messages)
Some Advice on PCB tols required (2 messages)
Surrogate Post - Multiple Choice Question (1 message)
SV: [TN] Recommended solder paste for a 6 layer double-sided board with CSP & BGA packages (1 message)
SV: [TN] Vapor phase (6 messages)
Tape & Reel Size for 0402 Components (2 messages)
TechNet Cops are NOT on vacation (1 message)
TechNet Digest - 12 May 2002 to 13 May 2002 (#2002-109) (2 messages)
testing via holes (4 messages)
Texas Designer's Learning Symposium - May 20 - 25, 2002 (1 message)
The Best Opportunity in Texas!!! (1 message)
Thickness of finish (1 message)
Tinning SMD diodes (3 messages)
TM650 (2 messages)
Trough hole soldering (2 messages)
TypeUR conformal coatings (3 messages)
V-groove 031 thick PCB (1 message)
Vacuum ??? (1 message)
vacuum seal and MSD (4 messages)
Vacuum Sealing (2 messages)
Vacuum sealing equipment (3 messages)
Vacuum sealing equipment... (11 messages)
Vapor phase (14 messages)
Via Capacitance (2 messages)
Via Plug (1 message)
Vias-in-pads (4 messages)
VIRUS WARNNING !!!!!!!!!!!!!!!!!!!!!!!!!!!!!!! (2 messages)
Voids in BGA/CSP Balls (1 message)
Voids in fine-pitch BGAs after reflow (3 messages)
Voids on 0.75 mm micro-BGA (2 messages)
Wave solder re-runs/re-work (5 messages)
Wave solder re-runs/re-work exposed copper (5 messages)
[TN} Vacuum Sealing... (2 messages)

LISTSERV Archives

LISTSERV Archives

TECHNET Home

TECHNET Home

Subject Sorted by Subject, Chronologically

From

Date

Size

Re:

Randy Bock Sr.

Wed, 29 May 2002 15:47:36 -0400

119 lines

Re:

Mel Parrish

Wed, 29 May 2002 15:15:20 -0500

146 lines

Re:

<>

Thu, 30 May 2002 08:39:17 +0800

101 lines

New Thread

(Fwd) Inquiry on maximum temperature

(Fwd) Inquiry on maximum temperature

Rick

Tue, 21 May 2002 07:24:55 -0400

46 lines

Re: (Fwd) Inquiry on maximum temperature

Crepeau, Phil

Wed, 22 May 2002 08:02:50 -0700

78 lines

Re: (Fwd) Inquiry on maximum temperature

Mark Roslawski

Wed, 22 May 2002 17:21:52 -0700

104 lines

New Thread

0201 inspection and rework tools

0201 inspection and rework tools

Yu, Rudolph

Fri, 31 May 2002 15:12:14 -0700

28 lines

New Thread

0402 pad design

0402 pad design

Edward S. Wheeler

Thu, 16 May 2002 08:32:00 -0400

29 lines

New Thread

63/37 solder paste with silver plated boards

63/37 solder paste with silver plated boards

Vandendolder, Ron

Thu, 9 May 2002 13:26:38 -0400

32 lines

Re: 63/37 solder paste with silver plated boards

Earl Moon

Thu, 9 May 2002 12:42:22 -0500

27 lines

Re: 63/37 solder paste with silver plated boards

Earl Moon

Thu, 9 May 2002 12:43:38 -0500

23 lines

Re: 63/37 solder paste with silver plated boards

Furrow, Robert Gordon (Bob)

Thu, 9 May 2002 13:59:29 -0400

72 lines

Re: 63/37 solder paste with silver plated boards

Alex Krstic

Thu, 9 May 2002 13:15:49 -0600

60 lines

Re: 63/37 solder paste with silver plated boards

Mike Fenner

Mon, 13 May 2002 10:49:53 +0100

77 lines

New Thread

<No subject>

Dieselberg, Ron

Wed, 29 May 2002 13:56:47 -0400

83 lines

New Thread

A "NEDA" Oriented label...

Re: A "NEDA" Oriented label...

Guy Ramsey

Wed, 1 May 2002 07:05:35 -0400

56 lines

New Thread

abrasive for cleaning PCB surfaces

abrasive for cleaning PCB surfaces

Kris Keating

Thu, 23 May 2002 13:23:00 -0400

32 lines

Re: abrasive for cleaning PCB surfaces

Phil Nutting

Thu, 23 May 2002 13:57:10 -0400

73 lines

New Thread

AM79C970AVIW Ethernet Controller IC

AM79C970AVIW Ethernet Controller IC

<>

Wed, 22 May 2002 13:22:43 +0800

39 lines

New Thread

Anti-voiding solder paste

Anti-voiding solder paste

d. terstegge

Tue, 28 May 2002 12:37:24 +0200

40 lines

Re: Anti-voiding solder paste

Eric Dawson

Tue, 28 May 2002 13:33:55 +0100

55 lines

Re: Anti-voiding solder paste

Earl Moon

Tue, 28 May 2002 07:35:14 -0500

33 lines

Re: Anti-voiding solder paste

<>

Tue, 28 May 2002 08:56:26 EDT

53 lines

Re: Anti-voiding solder paste

rgrant

Tue, 28 May 2002 09:10:22 -0600

121 lines

Re: Anti-voiding solder paste

Sherif Refaat

Wed, 29 May 2002 12:57:00 -0400

94 lines

New Thread

Antwort: [TN] BGA X-ray Cross Section services - Vendors?

Antwort: [TN] BGA X-ray Cross Section services - Vendors?

Frank Kriesch

Fri, 17 May 2002 09:19:57 +0200

126 lines

New Thread

assembly spacing

assembly spacing

<>

Mon, 20 May 2002 17:36:02 EDT

32 lines

Re: assembly spacing

Barry Gallegos

Tue, 21 May 2002 06:58:48 -0600

68 lines

Re: assembly spacing

Guy Ramsey

Tue, 21 May 2002 09:49:18 -0400

69 lines

New Thread

ASSY: Component Polarity

ASSY: Component Polarity

Jack C. Olson

Thu, 30 May 2002 08:35:45 -0500

38 lines

Re: ASSY: Component Polarity

Earl Moon

Thu, 30 May 2002 08:42:19 -0500

38 lines

Re: ASSY: Component Polarity

Mark Charlton

Thu, 30 May 2002 10:03:10 -0400

78 lines

Re: ASSY: Component Polarity

Phil Nutting

Thu, 30 May 2002 10:31:23 -0400

77 lines

Re: ASSY: Component Polarity

<>

Thu, 30 May 2002 11:18:49 EDT

64 lines

Re: ASSY: Component Polarity

Jack C. Olson

Thu, 30 May 2002 21:30:18 -0500

68 lines

Re: ASSY: Component Polarity

<>

Thu, 30 May 2002 23:27:16 EDT

86 lines

Re: ASSY: Component Polarity

Earl Moon

Thu, 30 May 2002 23:52:33 -0500

55 lines

Re: ASSY: Component Polarity

Phil Nutting

Fri, 31 May 2002 08:30:30 -0400

104 lines

Re: ASSY: Component Polarity

Earl Moon

Fri, 31 May 2002 07:57:24 -0500

33 lines

Re: ASSY: Component Polarity

rgrant

Fri, 31 May 2002 08:18:59 -0600

126 lines

New Thread

ASSY: Component Polarity - part 2

Re: ASSY: Component Polarity - part 2

Phil Nutting

Thu, 30 May 2002 10:46:47 -0400

75 lines

New Thread

ASSY: Reflow for Through-Hole Devices

ASSY: Reflow for Through-Hole Devices

Jack C. Olson

Wed, 22 May 2002 10:59:26 -0500

31 lines

Re: ASSY: Reflow for Through-Hole Devices

Woody, Linda L

Wed, 22 May 2002 15:51:48 -0400

68 lines

Re: ASSY: Reflow for Through-Hole Devices

Lee Whiteman

Wed, 22 May 2002 16:20:51 -0400

78 lines

Re: ASSY: Reflow for Through-Hole Devices

Ed Valentine

Wed, 22 May 2002 18:11:25 -0400

67 lines

Re: ASSY: Reflow for Through-Hole Devices

<>

Wed, 22 May 2002 18:32:49 EDT

85 lines

Re: ASSY: Reflow for Through-Hole Devices

<>

Thu, 23 May 2002 08:50:20 EDT

38 lines

Re: ASSY: Reflow for Through-Hole Devices

Atkinson, Neil

Fri, 24 May 2002 08:15:25 +0100

303 lines

Re: ASSY: Reflow for Through-Hole Devices

Mike Fenner

Tue, 28 May 2002 09:05:38 +0100

355 lines

New Thread

bare board serialization

bare board serialization

Mark Hargreaves

Wed, 29 May 2002 16:26:09 -0400

26 lines

Re: bare board serialization

<>

Thu, 30 May 2002 08:44:30 +0800

79 lines

Re: bare board serialization

Dougal Stewart

Thu, 30 May 2002 09:27:18 +0100

63 lines

Re: bare board serialization

Phil Nutting

Thu, 30 May 2002 08:21:56 -0400

65 lines

New Thread

BGA replacement

BGA replacement

<>

Tue, 14 May 2002 10:34:19 -0400

60 lines

Re: BGA replacement

Earl Moon

Tue, 14 May 2002 10:20:48 -0500

33 lines

Re: BGA replacement

Misner, Bruce

Tue, 14 May 2002 09:28:40 -0600

105 lines

Re: BGA replacement

Steve Owen

Tue, 14 May 2002 16:35:48 +0100

110 lines

Re: BGA replacement

Eric Dawson

Tue, 14 May 2002 17:09:07 +0100

69 lines

Re: BGA replacement

Liviu Jurjica-Prundeanu

Tue, 14 May 2002 11:58:58 -0400

106 lines

Re: BGA replacement

Earl Moon

Tue, 14 May 2002 11:32:05 -0500

23 lines

Re: BGA replacement

Jeff Ferry

Tue, 14 May 2002 13:49:07 -0400

122 lines

Re: BGA replacement

Gaby Bogdan

Tue, 14 May 2002 20:51:17 +0200

63 lines

Re: BGA replacement

Tempea, Ioan

Tue, 14 May 2002 14:34:21 -0400

159 lines

Re: BGA replacement

Jeff Ferry

Tue, 14 May 2002 16:20:13 -0400

191 lines

Re: BGA replacement

<>

Wed, 15 May 2002 08:24:20 +0800

148 lines

Re: BGA replacement

Dan R. Johnson

Wed, 15 May 2002 08:21:23 -0700

27 lines

Re: BGA replacement

Earl Moon

Wed, 15 May 2002 11:06:00 -0500

29 lines

Re: BGA replacement

David Douthit

Wed, 15 May 2002 10:12:50 -0700

61 lines

Re: BGA replacement

Earl Moon

Wed, 15 May 2002 12:10:11 -0500

33 lines

Re: BGA replacement

Seth Goodman

Sat, 18 May 2002 17:39:14 -0500

88 lines

New Thread

BGA SMD vs NSMD

Re: BGA SMD vs NSMD

Werner Engelmaier

Wed, 29 May 2002 07:44:57 EDT

32 lines

Re: BGA SMD vs NSMD

<>

Wed, 29 May 2002 10:47:59 EDT

73 lines

New Thread

BGA solder anomalies

BGA solder anomalies

Antonio Souza

Wed, 1 May 2002 10:17:49 -0500

32 lines

Re: BGA solder anomalies

<>

Wed, 1 May 2002 12:08:02 EDT

46 lines

Re: BGA solder anomalies

Wenger, George M.

Wed, 1 May 2002 13:08:27 -0400

77 lines

New Thread

BGA Solderability

BGA Solderability

Denis Lefebvre

Thu, 23 May 2002 07:09:38 -0700

125 lines

Re: BGA Solderability

Beerman, Dennis

Thu, 23 May 2002 10:08:57 -0500

56 lines

Re: BGA Solderability

Houston, Terri

Thu, 23 May 2002 09:24:33 -0600

73 lines

Re: BGA Solderability

Jeff Seeger

Thu, 23 May 2002 13:00:09 -0400

55 lines

Re: BGA Solderability

Earl Moon

Thu, 23 May 2002 12:05:26 -0500

25 lines

Re: BGA Solderability

Houston, Terri

Thu, 23 May 2002 11:48:29 -0600

47 lines

Re: BGA Solderability

rgrant

Thu, 23 May 2002 12:47:41 -0600

57 lines

Re: BGA Solderability

Earl Moon

Thu, 23 May 2002 14:18:38 -0500

34 lines

Re: BGA Solderability

Earl Moon

Thu, 23 May 2002 14:21:44 -0500

27 lines

Re: BGA Solderability

Maddox, Allen T

Fri, 24 May 2002 08:39:37 -0400

67 lines

Re: BGA Solderability

<>

Tue, 28 May 2002 11:01:46 EDT

58 lines

Re: BGA Solderability

<>

Tue, 28 May 2002 11:21:38 EDT

44 lines

Re: BGA Solderability

Earl Moon

Tue, 28 May 2002 11:42:09 -0500

28 lines

New Thread

BGA warpage - defects in the corners.

BGA warpage - defects in the corners.

Henry Rekers

Thu, 16 May 2002 13:34:19 -0700

38 lines

Re: BGA warpage - defects in the corners.

Yu, Rudolph

Thu, 16 May 2002 14:30:18 -0700

70 lines

Re: BGA warpage - defects in the corners.

Jason Gregory

Thu, 16 May 2002 16:36:37 -0500

30 lines

Re: BGA warpage - defects in the corners.

Henry Rekers

Thu, 16 May 2002 15:14:52 -0700

82 lines

Re: BGA warpage - defects in the corners.

Werner Engelmaier

Fri, 17 May 2002 19:33:10 EDT

34 lines

Re: BGA warpage - defects in the corners.

Earl Moon

Sat, 18 May 2002 12:01:29 -0500

30 lines

Re: BGA warpage - defects in the corners.

Werner Engelmaier

Sun, 19 May 2002 20:42:23 EDT

30 lines

New Thread

BGA X-ray Cross Section services - Vendors?

BGA X-ray Cross Section services - Vendors?

Rick Thompson

Thu, 16 May 2002 11:38:32 -0700

40 lines

Re: BGA X-ray Cross Section services - Vendors?

<>

Thu, 16 May 2002 16:01:51 EDT

44 lines

Re: BGA X-ray Cross Section services - Vendors?

<>

Fri, 17 May 2002 09:10:21 +0800

87 lines

Re: BGA X-ray Cross Section services - Vendors?

Ed Popielarski

Fri, 17 May 2002 06:43:32 -0700

39 lines

Re: BGA X-ray Cross Section services - Vendors?

<>

Fri, 17 May 2002 17:39:12 EDT

24 lines

Re: BGA X-ray Cross Section services - Vendors?

Randy Bock Sr.

Sat, 18 May 2002 07:51:53 -0400

57 lines

Re: BGA X-ray Cross Section services - Vendors?

<>

Sun, 19 May 2002 00:17:15 EDT

34 lines

New Thread

BGA's on ruggedized assemblies...

BGA's on ruggedized assemblies...

<>

Tue, 14 May 2002 17:08:59 EDT

46 lines

Re: BGA's on ruggedized assemblies...

<>

Wed, 15 May 2002 09:01:22 +0800

79 lines

Re: BGA's on ruggedized assemblies...

Dave Hillman

Wed, 15 May 2002 09:00:59 -0500

130 lines

Re: BGA's on ruggedized assemblies...

WEEKES, MICHAEL HS-SNS

Wed, 15 May 2002 10:35:19 -0400

111 lines

Re: BGA's on ruggedized assemblies...

Misner, Bruce

Wed, 15 May 2002 09:09:20 -0600

45 lines

Re: BGA's on ruggedized assemblies...

Misner, Bruce

Wed, 15 May 2002 09:25:28 -0600

148 lines

Re: BGA's on ruggedized assemblies...

Werner Engelmaier

Wed, 15 May 2002 18:27:05 EDT

27 lines

Re: BGA's on ruggedized assemblies...

<>

Thu, 16 May 2002 10:35:39 +0800

166 lines

Re: BGA's on ruggedized assemblies...

Earl Moon

Thu, 16 May 2002 05:34:18 -0500

29 lines

Re: BGA's on ruggedized assemblies...

Tom Buschor

Wed, 22 May 2002 12:13:23 -0500

32 lines

New Thread

Board analysis

Board analysis

Bissonnette, Jean-Francois

Tue, 28 May 2002 10:20:48 -0400

52 lines

Re: Board analysis

Tempea, Ioan

Tue, 28 May 2002 11:22:12 -0400

97 lines

New Thread

board baking

board baking

WEEKES, MICHAEL HS-SNS

Tue, 21 May 2002 10:15:31 -0400

36 lines

Re: board baking

Hinners Hans M Civ WRALC/LUGE

Tue, 21 May 2002 11:29:37 -0400

68 lines

New Thread

Board Cost

Board Cost

Marsico, James

Thu, 2 May 2002 10:34:19 -0400

37 lines

Re: Board Cost

WEEKES, MICHAEL HS-SNS

Wed, 15 May 2002 10:58:27 -0400

63 lines

New Thread

Board defect? Purple spot

Board defect? Purple spot

Pelkey, Glenn

Thu, 16 May 2002 10:14:23 -0700

85 lines

Re: Board defect? Purple spot

Robert B. Denbo

Thu, 16 May 2002 12:54:19 -0500

128 lines

Re: Board defect? Purple spot

Robert B. Denbo

Thu, 16 May 2002 14:20:16 -0500

244 lines

Re: Board defect? Purple spot

Bill Decray

Thu, 16 May 2002 15:55:34 -0400

128 lines

Re: Board defect? Purple spot

Pelkey, Glenn

Thu, 16 May 2002 11:53:34 -0700

146 lines

New Thread

BOARD EDGE CLEARANCE

BOARD EDGE CLEARANCE

Marsico, James

Wed, 8 May 2002 07:02:33 -0400

37 lines

Re: BOARD EDGE CLEARANCE

<>

Wed, 8 May 2002 09:11:22 -0700

79 lines

New Thread

Cell phone antenna enhancers...

Cell phone antenna enhancers...

<>

Wed, 29 May 2002 21:56:29 EDT

46 lines

Re: Cell phone antenna enhancers...

Phil Nutting

Thu, 30 May 2002 08:14:34 -0400

95 lines

Re: Cell phone antenna enhancers...

Earl Moon

Thu, 30 May 2002 08:36:39 -0500

39 lines

Re: Cell phone antenna enhancers...

Kasprzak, Bill (sys) USX

Thu, 30 May 2002 10:57:42 -0400

94 lines

Re: Cell phone antenna enhancers...

Marsico, James

Thu, 30 May 2002 11:03:35 -0400

95 lines

Re: Cell phone antenna enhancers...

Earl Moon

Thu, 30 May 2002 10:16:46 -0500

50 lines

New Thread

Cell phone antenna enhancers...NTC

Re: Cell phone antenna enhancers...NTC

Bloomquist, Ken

Thu, 30 May 2002 10:29:45 -0700

37 lines

Re: Cell phone antenna enhancers...NTC

James TerVeen

Thu, 30 May 2002 13:56:50 -0400

88 lines

Re: Cell phone antenna enhancers...NTC

Earl Moon

Thu, 30 May 2002 13:50:46 -0500

33 lines

Re: Cell phone antenna enhancers...NTC

Bissonnette, Jean-Francois

Thu, 30 May 2002 15:03:43 -0400

74 lines

Re: Cell phone antenna enhancers...NTC

Edward S. Wheeler

Thu, 30 May 2002 15:17:44 -0400

75 lines

Re: Cell phone antenna enhancers...NTC

Earl Moon

Thu, 30 May 2002 14:23:19 -0500

33 lines

Re: Cell phone antenna enhancers...NTC

Bloomquist, Ken

Thu, 30 May 2002 13:15:27 -0700

32 lines

Re: Cell phone antenna enhancers...NTC

<>

Thu, 30 May 2002 15:23:25 -0500

46 lines

Re: Cell phone antenna enhancers...NTC

Earl Moon

Thu, 30 May 2002 15:38:44 -0500

45 lines

Re: Cell phone antenna enhancers...NTC

Earl Moon

Thu, 30 May 2002 15:12:22 -0600

63 lines

Re: Cell phone antenna enhancers...NTC

Earl Moon

Thu, 30 May 2002 16:11:04 -0500

23 lines

Re: Cell phone antenna enhancers...NTC

Edward S. Wheeler

Thu, 30 May 2002 17:21:31 -0400

68 lines

Re: Cell phone antenna enhancers...NTC

<>

Thu, 30 May 2002 17:26:47 EDT

73 lines

Re: Cell phone antenna enhancers...NTC

Earl Moon

Thu, 30 May 2002 16:45:47 -0500

23 lines

Re: Cell phone antenna enhancers...NTC

Ken Carlile

Thu, 30 May 2002 18:02:27 -0400

78 lines

Re: Cell phone antenna enhancers...NTC

<>

Thu, 30 May 2002 18:07:14 EDT

67 lines

Re: Cell phone antenna enhancers...NTC

Earl Moon

Thu, 30 May 2002 17:08:26 -0500

63 lines

Re: Cell phone antenna enhancers...NTC

Earl Moon

Thu, 30 May 2002 17:18:39 -0500

24 lines

Re: Cell phone antenna enhancers...NTC

Sauer, Steven T.

Fri, 31 May 2002 07:09:23 -0400

23 lines

Re: Cell phone antenna enhancers...NTC

Randy Bock Sr.

Fri, 31 May 2002 07:30:19 -0400

61 lines

Re: Cell phone antenna enhancers...NTC

Graham Collins

Fri, 31 May 2002 08:36:59 -0400

98 lines

Re: Cell phone antenna enhancers...NTC

Earl Moon

Fri, 31 May 2002 07:51:40 -0500

24 lines

Re: Cell phone antenna enhancers...NTC

Earl Moon

Fri, 31 May 2002 08:04:43 -0500

31 lines

Re: Cell phone antenna enhancers...NTC

Guy Ramsey

Fri, 31 May 2002 09:14:37 -0400

92 lines

Re: Cell phone antenna enhancers...NTC

Mel Parrish

Fri, 31 May 2002 08:20:43 -0500

62 lines

Re: Cell phone antenna enhancers...NTC

Earl Moon

Fri, 31 May 2002 08:24:14 -0500

23 lines

Re: Cell phone antenna enhancers...NTC

Earl Moon

Fri, 31 May 2002 08:28:17 -0500

27 lines

Re: Cell phone antenna enhancers...NTC

Phil Nutting

Fri, 31 May 2002 10:07:13 -0400

67 lines

Re: Cell phone antenna enhancers...NTC

James TerVeen

Fri, 31 May 2002 10:43:57 -0400

103 lines

Re: Cell phone antenna enhancers...NTC

Earl Moon

Fri, 31 May 2002 09:05:47 -0600

95 lines

Re: Cell phone antenna enhancers...NTC

Earl Moon

Fri, 31 May 2002 10:12:09 -0500

30 lines

Re: Cell phone antenna enhancers...NTC

Mike Fenner

Fri, 31 May 2002 16:54:35 +0100

56 lines

Re: Cell phone antenna enhancers...NTC

Randy Bock Sr.

Fri, 31 May 2002 12:12:17 -0400

138 lines

Re: Cell phone antenna enhancers...NTC

Earl Moon

Fri, 31 May 2002 11:43:24 -0500

25 lines

Re: Cell phone antenna enhancers...NTC

Dan R. Johnson

Fri, 31 May 2002 10:13:52 -0700

39 lines

Re: Cell phone antenna enhancers...NTC

Earl Moon

Fri, 31 May 2002 12:32:29 -0500

28 lines

Re: Cell phone antenna enhancers...NTC

Dan R. Johnson

Fri, 31 May 2002 11:50:20 -0700

29 lines

Re: Cell phone antenna enhancers...NTC

Earl Moon

Fri, 31 May 2002 14:14:46 -0500

26 lines

Re: Cell phone antenna enhancers...NTC

Hogg, Blair K.

Fri, 31 May 2002 11:56:29 -0400

123 lines

Re: Cell phone antenna enhancers...NTC

Werner Engelmaier

Fri, 31 May 2002 19:33:01 EDT

31 lines

Re: Cell phone antenna enhancers...NTC

Earl Moon

Fri, 31 May 2002 19:07:54 -0500

28 lines

New Thread

Cell phone antenna enhances...NTC

Re: Cell phone antenna enhances...NTC

Kasprzak, Bill (sys) USX

Fri, 31 May 2002 11:57:33 -0400

141 lines

Re: Cell phone antenna enhances...NTC

Phil Nutting

Fri, 31 May 2002 12:37:36 -0400

223 lines

Re: Cell phone antenna enhances...NTC

Earl Moon

Fri, 31 May 2002 11:37:59 -0500

35 lines

Re: Cell phone antenna enhances...NTC

Earl Moon

Fri, 31 May 2002 12:27:51 -0500

25 lines

Re: Cell phone antenna enhances...NTC

Dave Snyder

Fri, 31 May 2002 10:45:56 -0700

171 lines

Re: Cell phone antenna enhances...NTC

Kasprzak, Bill (sys) USX

Fri, 31 May 2002 13:57:15 -0400

228 lines

Re: Cell phone antenna enhances...NTC

Earl Moon

Fri, 31 May 2002 12:58:40 -0500

42 lines

Re: Cell phone antenna enhances...NTC

Fred Biederman

Fri, 31 May 2002 15:46:13 -0400

74 lines

Re: Cell phone antenna enhances...NTC

Earl Moon

Fri, 31 May 2002 15:30:39 -0500

27 lines

Re: Cell phone antenna enhances...NTC

Steve Kelly

Fri, 31 May 2002 17:34:36 -0700

118 lines

New Thread

Ceramic filled Teflon board

Ceramic filled Teflon board

Phillip Hinton

Thu, 9 May 2002 12:39:51 EDT

50 lines

Re: Ceramic filled Teflon board

Earl Moon

Thu, 9 May 2002 12:03:40 -0500

35 lines

Re: Ceramic filled Teflon board

William Sullivan

Thu, 9 May 2002 12:56:56 -0700

54 lines

Re: Ceramic filled Teflon board

Goh Guan Chye

Fri, 10 May 2002 09:41:27 +0800

77 lines

Re: Ceramic filled Teflon board

Dave Hillman

Fri, 10 May 2002 11:25:18 -0500

63 lines

New Thread

Class 3 Solder Fillets - SMT 25 mil square pin Headers?

Class 3 Solder Fillets - SMT 25 mil square pin Headers?

Krug, Dick

Fri, 3 May 2002 10:04:51 -0400

31 lines

Re: Class 3 Solder Fillets - SMT 25 mil square pin Headers?

Mel Parrish

Fri, 3 May 2002 11:01:56 -0500

76 lines

Re: Class 3 Solder Fillets - SMT 25 mil square pin Headers?

Sauer, Steven T.

Fri, 3 May 2002 12:32:05 -0400

52 lines

Re: Class 3 Solder Fillets - SMT 25 mil square pin Headers?

David White

Fri, 3 May 2002 16:17:33 -0400

78 lines

Re: Class 3 Solder Fillets - SMT 25 mil square pin Headers?

Werner Engelmaier

Sun, 5 May 2002 18:06:10 EDT

32 lines

New Thread

Cleaning of No-clean Assemblies

Cleaning of No-clean Assemblies

Leland Woodall

Wed, 8 May 2002 15:41:50 -0400

43 lines

Re: Cleaning of No-clean Assemblies

Rudy Sedlak

Wed, 8 May 2002 16:57:03 EDT

50 lines

Re: Cleaning of No-clean Assemblies

David Douthit

Wed, 8 May 2002 16:57:59 -0700

72 lines

Re: Cleaning of No-clean Assemblies

Leland Woodall

Wed, 8 May 2002 20:51:42 -0400

101 lines

Re: Cleaning of No-clean Assemblies

DUTTON Phil

Thu, 9 May 2002 11:28:28 +1000

56 lines

Re: Cleaning of No-clean Assemblies

Brian Ellis

Thu, 9 May 2002 09:47:59 +0300

76 lines

Re: Cleaning of No-clean Assemblies

Graham Naisbitt

Thu, 9 May 2002 10:08:59 +0100

130 lines

Re: Cleaning of No-clean Assemblies

Marsico, James

Thu, 9 May 2002 08:26:57 -0400

87 lines

Re: Cleaning of No-clean Assemblies

KIPPING, Michael (York Rd)

Thu, 9 May 2002 14:26:04 +0100

128 lines

Re: Cleaning of No-clean Assemblies

Charlie Pitarys

Thu, 9 May 2002 10:09:17 -0400

266 lines

Re: Cleaning of No-clean Assemblies

<>

Thu, 9 May 2002 11:59:16 EDT

52 lines

Re: Cleaning of No-clean Assemblies

<>

Thu, 9 May 2002 15:29:07 -0500

40 lines

Re: Cleaning of No-clean Assemblies

<>

Mon, 13 May 2002 07:12:24 -0500

34 lines

Re: Cleaning of No-clean Assemblies

d. terstegge

Mon, 13 May 2002 15:34:39 +0200

82 lines

New Thread

CLEARANCE FRON PWB EDGES

CLEARANCE FRON PWB EDGES

Marsico, James

Tue, 7 May 2002 09:14:52 -0400

36 lines

Re: CLEARANCE FRON PWB EDGES

WEEKES, MICHAEL HS-SNS

Wed, 15 May 2002 10:56:27 -0400

65 lines

New Thread

Coating thickness

Coating thickness

fullname

Fri, 31 May 2002 10:26:43 +0800

36 lines

Re: Coating thickness

David Douthit

Thu, 30 May 2002 21:41:40 -0700

63 lines

Re: Coating thickness

Phil Kinner

Fri, 31 May 2002 09:05:32 +0100

280 lines

Re: Coating thickness

Hinners Hans M Civ WRALC/LUGE

Fri, 31 May 2002 13:36:35 +0100

88 lines

Re: Coating thickness

Lum Wee Mei

Sat, 1 Jun 2002 12:06:06 +0800

106 lines

New Thread

conductive blind via plug

conductive blind via plug

tony steinke

Wed, 29 May 2002 09:33:28 -0700

72 lines

Re: conductive blind via plug

Russell Burdick

Wed, 29 May 2002 07:52:27 -0700

48 lines

Re: conductive blind via plug

Franck, George

Wed, 29 May 2002 13:02:09 -0400

138 lines

Re: conductive blind via plug

tony steinke

Wed, 29 May 2002 13:09:50 -0700

167 lines

Re: conductive blind via plug

Don Vischulis

Wed, 29 May 2002 13:19:38 -0500

198 lines

Re: conductive blind via plug

Alain Savard

Wed, 29 May 2002 15:18:23 -0400

77 lines

Re: conductive blind via plug

Russell Burdick

Wed, 29 May 2002 13:08:36 -0700

111 lines

Re: conductive blind via plug

Earl Moon

Wed, 29 May 2002 15:14:44 -0500

24 lines

Re: conductive blind via plug

<>

Thu, 30 May 2002 08:36:40 +0800

116 lines

New Thread

Conformal Coating

Conformal Coating

Olivia Mc Dermott

Thu, 2 May 2002 15:40:09 +0000

31 lines

Re: Conformal Coating

WEEKES, MICHAEL HS-SNS

Thu, 2 May 2002 12:58:54 -0400

61 lines

Re: Conformal Coating

Chris Almeras

Thu, 2 May 2002 12:28:38 -0500

69 lines

Re: Conformal Coating

Olivia Mc Dermott

Fri, 3 May 2002 07:48:08 +0000

82 lines

Re: Conformal Coating

Graham Collins

Fri, 3 May 2002 08:34:44 -0400

71 lines

Re: Conformal Coating

Chris Almeras

Fri, 3 May 2002 08:42:35 -0500

341 lines

Re: Conformal Coating

<>

Fri, 3 May 2002 07:53:30 -0600

83 lines

Re: Conformal Coating

Graham Collins

Fri, 3 May 2002 10:09:57 -0400

118 lines

Re: Conformal Coating

Bloomquist, Ken

Fri, 3 May 2002 07:21:35 -0700

112 lines

Re: Conformal Coating

Lee Whiteman

Fri, 3 May 2002 11:26:05 -0400

80 lines

Conformal Coating

Dehoyos, Ramon

Tue, 14 May 2002 11:47:54 -0700

28 lines

Re: Conformal Coating

Phil Nutting

Tue, 14 May 2002 16:04:35 -0400

65 lines

Re: Conformal Coating

Hinners Hans M Civ WRALC/LUGE

Tue, 14 May 2002 21:18:33 +0100

74 lines

Re: Conformal Coating

Graham Collins

Wed, 15 May 2002 06:57:35 -0400

75 lines

Re: Conformal Coating

Marsico, James

Wed, 15 May 2002 07:26:51 -0400

69 lines

Re: Conformal Coating

<>

Wed, 15 May 2002 08:28:11 -0500

30 lines

Re: Conformal Coating

<>

Wed, 15 May 2002 15:48:58 EDT

26 lines

Conformal Coating

Misner, Bruce

Fri, 17 May 2002 12:09:48 -0500

29 lines

Re: Conformal Coating

Dieselberg, Ron

Fri, 17 May 2002 10:16:06 -0400

170 lines

Re: Conformal Coating

David Douthit

Fri, 17 May 2002 11:44:37 -0700

59 lines

Re: Conformal Coating

<>

Fri, 17 May 2002 17:46:01 EDT

25 lines

Re: Conformal Coating

Mel Parrish

Fri, 17 May 2002 16:54:37 -0500

80 lines

New Thread

Conformal coating / gluing

Conformal coating / gluing

Tim McQuay

Thu, 23 May 2002 12:44:36 -0500

40 lines

Re: Conformal coating / gluing

Hinners Hans M Civ WRALC/LUGE

Thu, 23 May 2002 20:06:31 +0100

94 lines

Re: Conformal coating / gluing

Connie Korth

Thu, 23 May 2002 15:09:53 -0500

75 lines

Re: Conformal coating / gluing

Tom Parkinson - Quality System Manager

Thu, 23 May 2002 16:25:30 -0400

70 lines

Re: Conformal coating / gluing

<>

Fri, 24 May 2002 07:58:55 +0800

95 lines

Re: Conformal coating / gluing

Graham Naisbitt

Fri, 24 May 2002 11:54:29 +0100

182 lines

Re: Conformal coating / gluing

<>

Tue, 28 May 2002 11:31:52 EDT

39 lines

New Thread

Conformal coating BGAs

Conformal coating BGAs

Linda Woody

Mon, 20 May 2002 10:53:22 -0500

28 lines

Re: Conformal coating BGAs

<>

Tue, 21 May 2002 13:33:32 +0800

94 lines

Re: Conformal coating BGAs

<>

Tue, 21 May 2002 08:05:03 -0500

33 lines

Re: Conformal coating BGAs

Werner Engelmaier

Tue, 21 May 2002 10:51:19 EDT

26 lines

Re: Conformal coating BGAs

Graham Naisbitt

Tue, 21 May 2002 21:40:08 +0100

173 lines

Re: Conformal coating BGAs

Dave Hillman

Tue, 21 May 2002 17:22:50 -0500

84 lines

Re: Conformal coating BGAs

<>

Wed, 22 May 2002 09:22:27 +0800

73 lines

Re: Conformal coating BGAs

Werner Engelmaier

Wed, 22 May 2002 04:16:00 EDT

28 lines

Re: Conformal coating BGAs

Tom Buschor

Wed, 22 May 2002 12:00:36 -0500

36 lines

Re: Conformal coating BGAs

Tegehall Per-Erik

Thu, 23 May 2002 17:29:36 +0200

237 lines

Re: Conformal coating BGAs

Werner Engelmaier

Sat, 25 May 2002 22:55:51 EDT

32 lines

New Thread

Crimp Tools

Crimp Tools

<>

Wed, 1 May 2002 15:18:27 -0600

25 lines

Re: Crimp Tools

Guy Ramsey

Thu, 2 May 2002 07:32:00 -0400

59 lines

New Thread

Crimped connections

Crimped connections

<>

Thu, 16 May 2002 07:45:58 -0400

58 lines

Re: Crimped connections

Charles Caswell

Thu, 16 May 2002 08:58:24 -0500

95 lines

Re: Crimped connections

Sauer, Steven T.

Thu, 16 May 2002 10:22:06 -0400

38 lines

Re: Crimped connections

Mel Parrish

Thu, 16 May 2002 09:45:18 -0500

106 lines

Re: Crimped connections

Dan R. Johnson

Thu, 16 May 2002 08:00:35 -0700

32 lines

Re: Crimped connections

Kathy Kuhlow

Thu, 16 May 2002 09:59:12 -0500

50 lines

Re: Crimped connections

<>

Thu, 16 May 2002 11:10:59 -0400

62 lines

Re: Crimped connections

Phil Nutting

Thu, 16 May 2002 11:48:41 -0400

75 lines

Re: Crimped connections

Dan R. Johnson

Thu, 16 May 2002 10:08:21 -0700

26 lines

Re: Crimped connections

Kasprzak, Bill (sys) USX

Fri, 17 May 2002 07:32:02 -0400

107 lines

Re: Crimped connections

Strickland, Mark

Fri, 17 May 2002 07:09:38 -0500

74 lines

Re: Crimped connections

Phil Nutting

Fri, 17 May 2002 08:54:49 -0400

173 lines

Re: Crimped connections

Seth Goodman

Sun, 19 May 2002 13:57:41 -0500

56 lines

Re: Crimped connections

Kasprzak, Bill (sys) USX

Mon, 20 May 2002 07:01:49 -0400

99 lines

Re: Crimped connections

Seth Goodman

Mon, 20 May 2002 15:34:57 -0500

69 lines

New Thread

Cycle Time for Solder Paste Printing

Cycle Time for Solder Paste Printing

Becerra Alejandro

Tue, 7 May 2002 08:02:47 -0500

103 lines

Re: Cycle Time for Solder Paste Printing

<>

Tue, 7 May 2002 11:05:55 -0700

64 lines

New Thread

D.O.E

D.O.E

Barry Gallegos

Wed, 15 May 2002 13:50:47 -0600

37 lines

Re: D.O.E

Lou Hart

Wed, 15 May 2002 16:38:18 -0400

65 lines

Re: D.O.E

Michael Bell

Thu, 16 May 2002 08:43:45 +1200

74 lines

Re: D.O.E

<>

Wed, 15 May 2002 16:24:43 -0500

35 lines

Re: D.O.E

Crepeau, Phil

Wed, 15 May 2002 14:41:04 -0700

62 lines

Re: D.O.E

Crepeau, Phil

Wed, 15 May 2002 14:42:02 -0700

60 lines

Re: D.O.E

Barry Gallegos

Wed, 15 May 2002 15:43:39 -0600

77 lines

Re: D.O.E

Jindra, Larry

Wed, 15 May 2002 19:08:22 -0700

79 lines

Re: D.O.E

Brian Ellis

Thu, 16 May 2002 10:09:41 +0300

59 lines

Re: D.O.E

Liviu Jurjica-Prundeanu

Thu, 16 May 2002 08:09:40 -0400

102 lines

Re: D.O.E

Tempea, Ioan

Thu, 16 May 2002 08:25:12 -0400

121 lines

Re: D.O.E

Crepeau, Phil

Thu, 16 May 2002 07:07:13 -0700

80 lines

New Thread

D2PAK devices

D2PAK devices

Reid, Lorraine

Thu, 23 May 2002 12:40:44 +0100

40 lines

Re: D2PAK devices

Sauer, Steven T.

Thu, 23 May 2002 10:18:29 -0400

46 lines

Re: D2PAK devices

Guy Ramsey

Thu, 23 May 2002 10:33:00 -0400

53 lines

Re: D2PAK devices

Sauer, Steven T.

Fri, 24 May 2002 08:34:08 -0400

46 lines

New Thread

Danny Harkins/CSI is out of the office.

Danny Harkins/CSI is out of the office.

<>

Tue, 28 May 2002 01:00:45 -0400

25 lines

New Thread

Dielectric constant for cores and prepeg

Dielectric constant for cores and prepeg

Fineline Circuits, Inc.

Fri, 3 May 2002 14:57:37 -0400

61 lines

New Thread

Dielectric Constants For Core and Prepreg

Dielectric Constants For Core and Prepreg

Fineline Circuits, Inc.

Fri, 3 May 2002 13:04:16 -0400

71 lines

Re: Dielectric Constants For Core and Prepreg

Earl Moon

Thu, 2 May 2002 12:12:14 -0500

25 lines

Re: Dielectric Constants For Core and Prepreg

Scott Kramer

Thu, 2 May 2002 10:49:58 -0700

136 lines

Re: Dielectric Constants For Core and Prepreg

Martyn Gaudion

Thu, 2 May 2002 19:52:02 +0100

95 lines

Re: Dielectric Constants For Core and Prepreg

<>

Tue, 28 May 2002 09:46:21 EDT

50 lines

New Thread

Dielectric material vs. Solder mask

Dielectric material vs. Solder mask

Bev Christian

Fri, 17 May 2002 15:39:26 -0400

27 lines

New Thread

DPMO benchmarking

Re: DPMO benchmarking

Jack Crawford

Wed, 29 May 2002 16:28:44 -0500

96 lines

New Thread

dross disposal

dross disposal

Bissonnette, Jean-Francois

Wed, 15 May 2002 10:33:30 -0400

51 lines

Re: dross disposal

Phil Nutting

Wed, 15 May 2002 11:17:20 -0400

89 lines

Re: dross disposal

Charles Caswell

Wed, 15 May 2002 10:46:55 -0500

84 lines

Re: dross disposal

Graham Collins

Wed, 15 May 2002 12:10:16 -0400

91 lines

Re: dross disposal

Bloomquist, Ken

Wed, 15 May 2002 09:45:55 -0700

59 lines

New Thread

Econonic Boom

Econonic Boom

Earl Moon

Fri, 31 May 2002 10:06:44 -0500

66 lines

New Thread

Electrical Isolation in dbm ?

Electrical Isolation in dbm ?

Goh Guan Chye

Thu, 16 May 2002 11:29:03 +0800

32 lines

Re: Electrical Isolation in dbm ?

Seth Goodman

Sat, 18 May 2002 18:11:19 -0500

73 lines

New Thread

Electronics Manufacturers Association Meeting (Seattle)

Electronics Manufacturers Association Meeting (Seattle)

Bloomquist, Ken

Thu, 9 May 2002 06:54:56 -0700

98 lines

New Thread

ESD and equipment isolation

ESD and equipment isolation

Jim Jenkins

Thu, 30 May 2002 13:25:40 -0500

44 lines

Re: ESD and equipment isolation

Earl Moon

Thu, 30 May 2002 14:27:06 -0500

24 lines

Re: ESD and equipment isolation

Kane, Joseph

Thu, 30 May 2002 16:17:53 -0400

100 lines

Re: ESD and equipment isolation

Guy Ramsey

Thu, 30 May 2002 17:22:21 -0400

85 lines

Re: ESD and equipment isolation

Gary Camac

Fri, 31 May 2002 07:44:49 -0500

106 lines

New Thread

Eutectic solder paste on silver plated boards

Eutectic solder paste on silver plated boards

Vandendolder, Ron

Fri, 10 May 2002 08:08:06 -0400

29 lines

Re: Eutectic solder paste on silver plated boards

Werner Engelmaier

Fri, 10 May 2002 20:00:43 EDT

27 lines

New Thread

ExposedCu

ExposedCu

<>

Tue, 7 May 2002 11:53:15 EDT

51 lines

Re: ExposedCu

Bloomquist, Ken

Tue, 7 May 2002 11:35:18 -0700

38 lines

New Thread

Film Capacitors...geeze!

Film Capacitors...geeze!

<>

Thu, 23 May 2002 21:51:58 EDT

38 lines

Re: Film Capacitors...geeze!

Guy Ramsey

Fri, 24 May 2002 07:01:53 -0400

77 lines

Re: Film Capacitors...geeze!

<>

Fri, 24 May 2002 07:04:12 -0500

97 lines

Re: Film Capacitors...geeze!

<>

Fri, 24 May 2002 08:58:50 EDT

106 lines

Re: Film Capacitors...geeze!

Tostevin, Bruce

Fri, 24 May 2002 10:15:00 -0500

83 lines

Re: Film Capacitors...geeze!

<>

Fri, 24 May 2002 11:44:43 EDT

55 lines

New Thread

Fire Up for IPC Annual Meeting 2002

Fire Up for IPC Annual Meeting 2002

John Perry

Thu, 23 May 2002 10:12:13 -0500

66 lines

Re: Fire Up for IPC Annual Meeting 2002

<>

Thu, 23 May 2002 14:19:56 -0500

23 lines

Re: Fire Up for IPC Annual Meeting 2002

Werner Engelmaier

Sat, 25 May 2002 22:55:52 EDT

25 lines

New Thread

First Article Inspection of bare boards

First Article Inspection of bare boards

d. terstegge

Tue, 14 May 2002 10:34:39 +0200

37 lines

Re: First Article Inspection of bare boards

Don Vischulis

Tue, 14 May 2002 07:19:51 -0500

75 lines

Re: First Article Inspection of bare boards

Hogg, Blair K.

Tue, 14 May 2002 09:44:46 -0400

29 lines

Re: First Article Inspection of bare boards

Kathy Kuhlow

Tue, 14 May 2002 08:57:57 -0500

55 lines

New Thread

Flip-flop panels

Re: Flip-flop panels

Eddie Rocha

Wed, 1 May 2002 17:11:39 -0700

32 lines

Re: Flip-flop panels

Tempea, Ioan

Thu, 2 May 2002 08:20:34 -0400

47 lines

New Thread

Flux on top of PCBs from wave

Flux on top of PCBs from wave

David White

Thu, 9 May 2002 10:33:02 -0400

29 lines

Re: Flux on top of PCBs from wave

Charles Caswell

Thu, 9 May 2002 10:43:56 -0500

63 lines

Re: Flux on top of PCBs from wave

Furrow, Robert Gordon (Bob)

Thu, 9 May 2002 11:40:43 -0400

70 lines

Re: Flux on top of PCBs from wave

David Douthit

Thu, 9 May 2002 10:27:11 -0700

74 lines

New Thread

fLUX RESIDUE IN NO CLEAN SOLDER WIRE

fLUX RESIDUE IN NO CLEAN SOLDER WIRE

Karnwal, Pankaj

Fri, 31 May 2002 08:03:54 +0200

44 lines

Re: fLUX RESIDUE IN NO CLEAN SOLDER WIRE

Steve Owen

Fri, 31 May 2002 07:45:19 +0100

83 lines

Re: fLUX RESIDUE IN NO CLEAN SOLDER WIRE

Brian Ellis

Fri, 31 May 2002 11:56:58 +0300

68 lines

New Thread

For Francois in case this didn't get posted to the technet

For Francois in case this didn't get posted to the technet

Earl Moon

Thu, 2 May 2002 10:50:56 -0500

47 lines

Re: For Francois in case this didn't get posted to the technet

Earl Moon

Thu, 2 May 2002 11:20:19 -0500

190 lines

New Thread

FPBGA Area Ratio Question

FPBGA Area Ratio Question

bbarr

Wed, 29 May 2002 11:40:15 -0400

44 lines

Re: FPBGA Area Ratio Question

Becerra Alejandro

Wed, 29 May 2002 12:41:06 -0500

255 lines

Re: FPBGA Area Ratio Question

bbarr

Wed, 29 May 2002 14:40:08 -0400

392 lines

Re: FPBGA Area Ratio Question

Dave Pahlas

Wed, 29 May 2002 17:00:33 -0400

449 lines

Re: FPBGA Area Ratio Question

Becerra Alejandro

Wed, 29 May 2002 16:01:13 -0500

432 lines

Re: FPBGA Area Ratio Question

bbarr

Wed, 29 May 2002 17:44:07 -0400

111 lines

Re: FPBGA Area Ratio Question

Ahne Oosterhof

Wed, 29 May 2002 15:16:38 -0700

96 lines

Re: FPBGA Area Ratio Question

Ahne Oosterhof

Wed, 29 May 2002 15:39:48 -0700

461 lines

New Thread

Gold Reclaim

Gold Reclaim

<>

Tue, 21 May 2002 12:27:46 -0400

33 lines

New Thread

good to be back

good to be back

William Sullivan

Thu, 9 May 2002 07:11:23 -0700

28 lines

New Thread

Guidelines or standards for number of missing unused BGA pads allowed

Guidelines or standards for number of missing unused BGA pads allowed

Francis Sun

Wed, 8 May 2002 12:02:57 -0400

41 lines

Re: Guidelines or standards for number of missing unused BGA pads allowed

Earl Moon

Wed, 8 May 2002 12:41:39 -0500

26 lines

Re: Guidelines or standards for number of missing unused BGA pads allowed

Francis Sun

Wed, 8 May 2002 16:37:30 -0400

66 lines

Re: Guidelines or standards for number of missing unused BGA pads allowed

Guy Ramsey

Thu, 9 May 2002 08:37:19 -0400

109 lines

New Thread

HDI and Sanmina

HDI and Sanmina

Earl Moon

Mon, 6 May 2002 09:58:55 -0500

81 lines

Re: HDI and Sanmina

David Douthit

Mon, 6 May 2002 10:01:26 -0700

106 lines

Re: HDI and Sanmina

Earl Moon

Mon, 6 May 2002 12:30:56 -0500

31 lines

Re: HDI and Sanmina

Jana Carraway

Mon, 6 May 2002 11:06:25 -0700

117 lines

Re: HDI and Sanmina

Earl Moon

Mon, 6 May 2002 13:09:21 -0500

34 lines

Re: HDI and Sanmina

Jana Carraway

Mon, 6 May 2002 11:43:38 -0700

58 lines

Re: HDI and Sanmina

Kathy Kuhlow

Mon, 6 May 2002 14:21:59 -0500

52 lines

Re: HDI and Sanmina

Dwight Mattix

Mon, 6 May 2002 15:55:52 -0700

136 lines

Re: HDI and Sanmina

Dwight Mattix

Mon, 6 May 2002 16:07:08 -0700

48 lines

Re: HDI and Sanmina

Earl Moon

Mon, 6 May 2002 19:07:43 -0500

47 lines

Re: HDI and Sanmina

Seth Goodman

Tue, 7 May 2002 01:14:48 -0500

88 lines

Re: HDI and Sanmina

Earl Moon

Tue, 7 May 2002 06:13:18 -0500

40 lines

New Thread

High lead composition solder paste and rinse water.

High lead composition solder paste and rinse water.

Charlie Pitarys

Wed, 1 May 2002 11:51:48 -0400

90 lines

Re: High lead composition solder paste and rinse water.

Wenger, George M.

Wed, 1 May 2002 13:28:05 -0400

168 lines

Re: High lead composition solder paste and rinse water.

Guy Ramsey

Wed, 1 May 2002 14:40:49 -0400

141 lines

Re: High lead composition solder paste and rinse water.

<>

Wed, 1 May 2002 14:10:55 -0500

29 lines

Re: High lead composition solder paste and rinse water.

Bev Christian

Wed, 1 May 2002 17:13:02 -0400

187 lines

Re: High lead composition solder paste and rinse water.

Charlie Pitarys

Thu, 2 May 2002 08:47:13 -0400

154 lines

Re: High lead composition solder paste and rinse water.

Guy Ramsey

Thu, 2 May 2002 10:07:46 -0400

89 lines

Re: High lead composition solder paste and rinse water.

Hinners Hans M Civ WRALC/LUGE

Thu, 2 May 2002 16:33:07 +0100

218 lines

Re: High lead composition solder paste and rinse water.

Mike Fenner

Thu, 2 May 2002 17:12:03 +0100

181 lines

New Thread

high Tg FR4

high Tg FR4

tony steinke

Tue, 21 May 2002 16:25:34 -0700

76 lines

New Thread

High Voltage tracking on pbc surface

High Voltage tracking on pbc surface

Phil Nutting

Wed, 15 May 2002 17:03:23 -0400

51 lines

Re: High Voltage tracking on pbc surface

Joseph Keary

Wed, 15 May 2002 15:51:05 -0700

81 lines

Re: High Voltage tracking on pbc surface

Brian Ellis

Thu, 16 May 2002 10:05:27 +0300

96 lines

Re: High Voltage tracking on pbc surface

<>

Thu, 16 May 2002 08:02:54 -0500

32 lines

Re: High Voltage tracking on pbc surface

Earl Moon

Thu, 16 May 2002 08:18:56 -0500

30 lines

Re: High Voltage tracking on pbc surface

Brian Ellis

Thu, 16 May 2002 17:37:52 +0300

58 lines

Re: High Voltage tracking on pbc surface

Earl Moon

Thu, 16 May 2002 09:54:28 -0500

26 lines

Re: High Voltage tracking on pbc surface

Brian Ellis

Thu, 16 May 2002 18:11:17 +0300

44 lines

Re: High Voltage tracking on pbc surface

Earl Moon

Thu, 16 May 2002 11:16:47 -0400

62 lines

Re: High Voltage tracking on pbc surface

<>

Thu, 16 May 2002 11:36:57 -0500

31 lines

Re: High Voltage tracking on pbc surface

Dougal Stewart

Thu, 16 May 2002 20:58:54 +0100

77 lines

Re: High Voltage tracking on pbc surface

Rob Legg

Thu, 16 May 2002 21:49:37 -0400

61 lines

New Thread

hole plating peel test

hole plating peel test

Dan R. Johnson

Wed, 1 May 2002 16:36:32 -0700

48 lines

New Thread

Hole routing in PCBs

Hole routing in PCBs

Phil Nutting

Wed, 1 May 2002 12:55:50 -0400

44 lines

Re: Hole routing in PCBs

John Parsons

Wed, 1 May 2002 10:51:43 -0700

104 lines

Re: Hole routing in PCBs

Randy Bock Sr.

Wed, 1 May 2002 14:18:53 -0400

80 lines

Re: Hole routing in PCBs

Robert B. Denbo

Wed, 1 May 2002 13:17:05 -0500

92 lines

Re: Hole routing in PCBs

Roger Stoops

Wed, 1 May 2002 15:50:28 -0400

90 lines

Re: Hole routing in PCBs

Don Vischulis

Wed, 1 May 2002 15:10:42 -0500

124 lines

Re: Hole routing in PCBs

Seth Goodman

Wed, 1 May 2002 17:13:25 -0500

44 lines

New Thread

HTML 3.2

Re: HTML 3.2

<>

Mon, 6 May 2002 13:44:20 EDT

43 lines

New Thread

Interesting addition to an ealier discussion

Interesting addition to an ealier discussion

Kathy Kuhlow

Fri, 3 May 2002 09:26:17 -0500

179 lines

New Thread

IPC-4552 spec for ENIG

IPC-4552 spec for ENIG

Debbie Schepis

Mon, 13 May 2002 08:52:38 -0400

27 lines

Re: IPC-4552 spec for ENIG

George Milad

Mon, 13 May 2002 09:18:31 EDT

45 lines

New Thread

IPC-DC Boston area mtg, 21-May

IPC-DC Boston area mtg, 21-May

Jeff Seeger

Tue, 14 May 2002 16:04:26 -0400

103 lines

New Thread

Keeping RA and OA flux separate

Keeping RA and OA flux separate

Phil Nutting

Tue, 21 May 2002 09:32:55 -0400

31 lines

Re: Keeping RA and OA flux separate

Brian Ellis

Tue, 21 May 2002 18:18:41 +0300

58 lines

Keeping RA and OA flux separate

Phil Nutting

Tue, 21 May 2002 09:32:55 -0400

50 lines

Re: Keeping RA and OA flux separate

Kathy Kuhlow

Tue, 21 May 2002 16:12:10 -0500

51 lines

New Thread

Locating Jay Brusse

Locating Jay Brusse

Phillip Hinton

Tue, 7 May 2002 00:22:11 EDT

42 lines

Re: Locating Jay Brusse

David Douthit

Mon, 6 May 2002 22:12:01 -0700

67 lines

New Thread

Looking for a capacitance meter

Looking for a capacitance meter

Houston, Terri

Tue, 21 May 2002 15:00:27 -0500

33 lines

Re: Looking for a capacitance meter

Dan R. Johnson

Tue, 21 May 2002 16:21:01 -0700

34 lines

Re: Looking for a capacitance meter

Sauer, Steven T.

Wed, 22 May 2002 07:38:17 -0400

34 lines

Re: Looking for a capacitance meter

Hogg, Blair K.

Wed, 22 May 2002 08:53:56 -0400

59 lines

Re: Looking for a capacitance meter

<>

Wed, 22 May 2002 08:27:39 -0500

25 lines

Re: Looking for a capacitance meter

Barmuta, Mike

Wed, 22 May 2002 07:49:13 -0700

70 lines

New Thread

Looking for A Solderability Spec

Looking for A Solderability Spec

Dave Hillman

Fri, 17 May 2002 13:18:08 -0500

28 lines

Re: Looking for A Solderability Spec

David Fish

Fri, 17 May 2002 16:29:01 -0700

62 lines

Re: Looking for A Solderability Spec

WEEKES, MICHAEL HS-SNS

Fri, 17 May 2002 16:29:31 -0400

57 lines

Re: Looking for A Solderability Spec

Guy Ramsey

Fri, 17 May 2002 17:12:12 -0400

62 lines

Re: Looking for A Solderability Spec

<>

Fri, 17 May 2002 16:17:44 -0500

59 lines

Re: Looking for A Solderability Spec

Earl Moon

Sat, 18 May 2002 12:06:24 -0500

27 lines

New Thread

Looking for A Solderability Spec - No technical content contained

Re: Looking for A Solderability Spec - No technical content contained

Dave Hillman

Fri, 17 May 2002 16:31:28 -0500

87 lines

Re: Looking for A Solderability Spec - No technical content contained

Earl Moon

Sat, 18 May 2002 11:52:34 -0500

29 lines

Re: Looking for A Solderability Spec - No technical content contained

Earl Moon

Sat, 18 May 2002 11:54:42 -0500

21 lines

Re: Looking for A Solderability Spec - No technical content contained

<>

Mon, 20 May 2002 15:23:52 EDT

48 lines

Re: Looking for A Solderability Spec - No technical content contained

Dave Hillman

Mon, 20 May 2002 16:43:23 -0500

66 lines

New Thread

Looking for place who offer classes on ICT/DFT in Bay Area

Looking for place who offer classes on ICT/DFT in Bay Area

Ken Patel

Thu, 30 May 2002 15:40:18 -0700

32 lines

New Thread

Looking for recent PCB Reliability model

Looking for recent PCB Reliability model

Jim Lamb

Wed, 15 May 2002 00:13:34 -0700

30 lines

Re: Looking for recent PCB Reliability model

Werner Engelmaier

Thu, 16 May 2002 18:45:31 EDT

32 lines

Re: Looking for recent PCB Reliability model

Guy Ramsey

Wed, 29 May 2002 07:50:24 -0400

62 lines

New Thread

Low Temp BGA Balls

Low Temp BGA Balls

Jindra, Larry

Mon, 6 May 2002 16:24:00 -0700

29 lines

Re: Low Temp BGA Balls

<>

Mon, 6 May 2002 20:28:37 EDT

108 lines

Re: Low Temp BGA Balls

<>

Tue, 7 May 2002 12:15:02 +0800

105 lines

Re: Low Temp BGA Balls

Marsico, James

Tue, 7 May 2002 07:05:56 -0400

74 lines

New Thread

Mark Orlowski/PEMSTAR Inc is out of the office.

Mark Orlowski/PEMSTAR Inc is out of the office.

Mark Orlowski/PEMSTAR Inc

Wed, 15 May 2002 01:01:40 -0500

24 lines

New Thread

Mechanical Strength of Solder Joints

Re: Mechanical Strength of Solder Joints

Werner Engelmaier

Wed, 1 May 2002 19:28:48 EDT

33 lines

New Thread

Metal core PCB's

Metal core PCB's

David Bailey

Fri, 24 May 2002 15:01:35 +1000

121 lines

Re: Metal core PCB's

Joe Fjelstad

Fri, 24 May 2002 09:34:55 EDT

75 lines

Re: Metal core PCB's

<>

Fri, 24 May 2002 12:13:58 EDT

103 lines

Re: Metal core PCB's

Earl Moon

Fri, 24 May 2002 14:06:04 -0500

22 lines

Re: Metal core PCB's

MA Ranganath/SMPLB/SEC/SANMAR

Sat, 25 May 2002 10:36:11 +0530

159 lines

Re: Metal core PCB's

Tom Waznis

Sat, 25 May 2002 04:47:48 -0700

63 lines

New Thread

Mil spec approval

Mil spec approval

Gordon Falconer

Thu, 2 May 2002 20:07:15 -0700

82 lines

Re: Mil spec approval

Earl Moon

Thu, 2 May 2002 14:24:09 -0500

34 lines

Re: Mil spec approval

MA Ranganath/SMPLB/SEC/SANMAR

Thu, 2 May 2002 20:25:10 -0700

138 lines

Re: Mil spec approval

Joseph Spicuzza

Fri, 3 May 2002 13:59:09 -0400

65 lines

Re: Mil spec approval

<>

Fri, 3 May 2002 15:03:07 EDT

21 lines

Re: Mil spec approval

Joseph Spicuzza

Fri, 3 May 2002 15:57:26 -0400

50 lines

New Thread

no clean paste for High frequencies

no clean paste for High frequencies

Zweigart, Siegmund

Fri, 24 May 2002 10:51:20 +0200

25 lines

Re: no clean paste for High frequencies

<>

Fri, 24 May 2002 07:32:53 -0500

36 lines

Re: no clean paste for High frequencies

<>

Tue, 28 May 2002 08:20:42 EDT

32 lines

New Thread

No Clean?

No Clean?

Henry Rekers

Tue, 14 May 2002 08:00:28 -0700

27 lines

New Thread

NTC - The Gregory's are a team now...

NTC - The Gregory's are a team now...

<>

Thu, 30 May 2002 19:14:48 EDT

31 lines

Re: NTC - The Gregory's are a team now...

Gaby Bogdan

Fri, 31 May 2002 08:10:26 +0200

64 lines

Re: NTC - The Gregory's are a team now...

Earl Moon

Fri, 31 May 2002 01:06:17 -0500

38 lines

Re: NTC - The Gregory's are a team now...

Gaby Bogdan

Fri, 31 May 2002 16:27:52 +0200

73 lines

Re: NTC - The Gregory's are a team now...

Earl Moon

Fri, 31 May 2002 08:43:10 -0500

34 lines

Re: NTC - The Gregory's are a team now...

Earl Moon

Fri, 31 May 2002 09:01:36 -0600

108 lines

Re: NTC - The Gregory's are a team now...

Gaby Bogdan

Fri, 31 May 2002 18:28:59 +0200

154 lines

Re: NTC - The Gregory's are a team now...

Earl Moon

Fri, 31 May 2002 11:47:21 -0500

27 lines

Re: NTC - The Gregory's are a team now...

Gaby Bogdan

Fri, 31 May 2002 20:18:52 +0200

52 lines

Re: NTC - The Gregory's are a team now...

Earl Moon

Fri, 31 May 2002 12:34:20 -0500

34 lines

New Thread

OT Cell phone antenna enhances...NTC

OT Cell phone antenna enhances...NTC

Denis Lefebvre

Fri, 31 May 2002 15:38:31 -0700

63 lines

Re: OT Cell phone antenna enhances...NTC

Earl Moon

Fri, 31 May 2002 19:03:49 -0500

26 lines

New Thread

OT- wasn't an experiment..

OT- wasn't an experiment..

<>

Fri, 31 May 2002 22:26:03 EDT

54 lines

Re: OT- wasn't an experiment..

Earl Moon

Fri, 31 May 2002 22:37:02 -0600

100 lines

Re: OT- wasn't an experiment..

Earl Moon

Fri, 31 May 2002 23:36:42 -0500

24 lines

New Thread

Palladium Leads

Palladium Leads

Henry Rekers

Wed, 8 May 2002 17:33:22 -0700

28 lines

Re: Palladium Leads

Sauer, Steven T.

Thu, 9 May 2002 07:32:09 -0400

44 lines

Re: Palladium Leads

Bev Christian

Thu, 9 May 2002 07:59:23 -0400

72 lines

Re: Palladium Leads

<>

Thu, 9 May 2002 08:36:16 EDT

71 lines

Re: Palladium Leads

Earl Moon

Thu, 9 May 2002 09:07:11 -0400

110 lines

Re: Palladium Leads

Peter Barton

Thu, 9 May 2002 14:59:00 +0100

112 lines

Re: Palladium Leads

Guy Ramsey

Thu, 9 May 2002 11:20:25 -0400

152 lines

Re: Palladium Leads

<>

Thu, 9 May 2002 11:26:45 EDT

98 lines

Re: Palladium Leads

Wenger, George M.

Thu, 9 May 2002 13:11:48 -0400

246 lines

Re: Palladium Leads

Mel Parrish

Thu, 9 May 2002 15:46:07 -0500

268 lines

Re: Palladium Leads

Dave Hillman

Fri, 10 May 2002 14:22:47 -0500

276 lines

New Thread

Palladium Leads - Flux Choices

Re: Palladium Leads - Flux Choices

<>

Mon, 13 May 2002 08:36:55 +0800

339 lines

New Thread

Panelization sanity check needed

Panelization sanity check needed

Lambert, Katherine A.

Tue, 7 May 2002 12:43:04 -0700

51 lines

Re: Panelization sanity check needed

Earl Moon

Tue, 7 May 2002 14:55:28 -0500

38 lines

Re: Panelization sanity check needed

Seth Goodman

Wed, 8 May 2002 00:08:20 -0500

52 lines

Re: Panelization sanity check needed

Brian L. Guidi

Wed, 8 May 2002 08:05:15 -0400

113 lines

Re: Panelization sanity check needed

Earl Moon

Wed, 8 May 2002 07:58:13 -0500

24 lines

Re: Panelization sanity check needed

Eddie Rocha

Wed, 8 May 2002 09:43:58 -0700

26 lines

New Thread

Parts List Definition

Parts List Definition

Richard Hamilton

Mon, 6 May 2002 22:14:23 -0700

34 lines

Re: Parts List Definition

<>

Tue, 7 May 2002 16:19:01 +0800

107 lines

Re: Parts List Definition

Dan R. Johnson

Tue, 7 May 2002 08:03:27 -0700

38 lines

Re: Parts List Definition

Kathy Kuhlow

Tue, 7 May 2002 11:24:06 -0500

80 lines

New Thread

pcb design

pcb design

Frank Conti

Mon, 20 May 2002 10:59:30 EDT

56 lines

Re: pcb design

Brooks,Bill

Mon, 20 May 2002 09:28:18 -0700

144 lines

Re: pcb design

Denis Lefebvre

Mon, 20 May 2002 10:01:49 -0700

144 lines

Re: pcb design

William Sullivan

Mon, 20 May 2002 10:29:32 -0700

61 lines

Re: pcb design

Dan R. Johnson

Mon, 20 May 2002 12:06:51 -0700

64 lines

New Thread

PCB MATERIAL with low OUTGASSING Characteristics....

PCB MATERIAL with low OUTGASSING Characteristics....

Race, Albert

Thu, 16 May 2002 13:53:18 -0400

32 lines

New Thread

PCB materials

PCB materials

Torres, Roberto

Wed, 22 May 2002 14:53:12 -0400

55 lines

Re: PCB materials

rgrant

Thu, 23 May 2002 10:37:44 -0600

97 lines

Re: PCB materials

Torres, Roberto

Thu, 23 May 2002 13:01:13 -0400

118 lines

Re: PCB materials

Earl Moon

Thu, 23 May 2002 12:11:11 -0500

30 lines

Re: PCB materials

<>

Tue, 28 May 2002 11:10:32 EDT

42 lines

Re: PCB materials

<>

Tue, 28 May 2002 11:17:12 EDT

45 lines

Re: PCB materials

<>

Tue, 28 May 2002 11:28:28 EDT

43 lines

Re: PCB materials

Earl Moon

Tue, 28 May 2002 11:38:29 -0500

37 lines

Re: PCB materials

Torres, Roberto

Wed, 29 May 2002 13:11:18 -0400

94 lines

New Thread

Plant closures

Plant closures

Scott Westheimer

Sat, 27 Apr 2002 12:27:20 -0400

74 lines

Re: Plant closures

Joe Fjelstad

Mon, 13 May 2002 12:48:56 EDT

45 lines

Re: Plant closures

WEEKES, MICHAEL HS-SNS

Mon, 13 May 2002 14:32:00 -0400

86 lines

New Thread

power traces

power traces

Eddie Rocha

Thu, 23 May 2002 11:47:16 -0700

22 lines

New Thread

Productivity Way Up

Productivity Way Up

Earl Moon

Tue, 7 May 2002 10:36:38 -0500

30 lines

Re: Productivity Way Up

Kathy Kuhlow

Tue, 7 May 2002 11:16:31 -0500

63 lines

Re: Productivity Way Up

Earl Moon

Tue, 7 May 2002 11:40:41 -0500

35 lines

Re: Productivity Way Up

Dan R. Johnson

Tue, 7 May 2002 10:01:40 -0700

28 lines

Re: Productivity Way Up

Earl Moon

Tue, 7 May 2002 12:20:01 -0500

42 lines

Re: Productivity Way Up

Jeff Ferry

Tue, 7 May 2002 14:46:00 -0400

82 lines

Re: Productivity Way Up

Earl Moon

Tue, 7 May 2002 13:59:15 -0500

36 lines

Re: Productivity Way Up

Dan R. Johnson

Tue, 7 May 2002 12:55:09 -0700

38 lines

Re: Productivity Way Up

Earl Moon

Tue, 7 May 2002 15:05:43 -0500

29 lines

Re: Productivity Way Up

jim

Tue, 7 May 2002 16:43:56 -0500

74 lines

Re: Productivity Way Up

Earl Moon

Tue, 7 May 2002 16:43:29 -0500

28 lines

Re: Productivity Way Up

Genny Gibbard

Tue, 7 May 2002 16:20:49 -0600

103 lines

Re: Productivity Way Up

Earl Moon

Tue, 7 May 2002 17:43:29 -0500

35 lines

Re: Productivity Way Up

Jack C. Olson

Wed, 8 May 2002 08:18:08 -0500

33 lines

Re: Productivity Way Up

Earl Moon

Wed, 8 May 2002 09:24:20 -0500

26 lines

Re: Productivity Way Up

Crepeau, Phil

Wed, 8 May 2002 11:47:12 -0700

56 lines

Re: Productivity Way Up

Earl Moon

Wed, 8 May 2002 14:43:25 -0500

40 lines

New Thread

Productivity Way Up - Off topic

Re: Productivity Way Up - Off topic

McVean

Wed, 8 May 2002 18:24:14 +0100

71 lines

Re: Productivity Way Up - Off topic

Earl Moon

Wed, 8 May 2002 12:21:20 -0500

26 lines

Re: Productivity Way Up - Off topic

Earl Moon

Wed, 8 May 2002 13:22:41 -0500

41 lines

New Thread

Proposed lifting of component date code restrictions

Proposed lifting of component date code restrictions

Francois Monette

Wed, 1 May 2002 09:35:06 -0400

110 lines

Re: Proposed lifting of component date code restrictions

Seth Goodman

Wed, 1 May 2002 16:30:13 -0500

60 lines

New Thread

PTH Vertical Fill Requirement IPC610 Rev. C

PTH Vertical Fill Requirement IPC610 Rev. C

<>

Thu, 9 May 2002 11:43:48 -0700

41 lines

Re: PTH Vertical Fill Requirement IPC610 Rev. C

Richard Carruth

Thu, 9 May 2002 16:48:02 -0500

90 lines

Re: PTH Vertical Fill Requirement IPC610 Rev. C

Nancy Trumbull

Fri, 10 May 2002 07:24:05 -0400

94 lines

Re: PTH Vertical Fill Requirement IPC610 Rev. C

Sauer, Steven T.

Fri, 10 May 2002 07:53:53 -0400

53 lines

Re: PTH Vertical Fill Requirement IPC610 Rev. C

David Douthit

Fri, 10 May 2002 05:41:05 -0700

75 lines

Re: PTH Vertical Fill Requirement IPC610 Rev. C

Nancy Trumbull

Fri, 10 May 2002 14:56:07 -0400

89 lines

Re: PTH Vertical Fill Requirement IPC610 Rev. C

Guy Ramsey

Fri, 10 May 2002 15:51:39 -0400

286 lines

Re: PTH Vertical Fill Requirement IPC610 Rev. C

Werner Engelmaier

Fri, 10 May 2002 20:00:45 EDT

36 lines

New Thread

Re column grid arrays

Re column grid arrays

Dave Hillman

Fri, 31 May 2002 15:05:42 -0500

81 lines

Re: Re column grid arrays

Earl Moon

Fri, 31 May 2002 15:33:18 -0500

51 lines

New Thread

Re Hole Fill

Re Hole Fill

<>

Mon, 20 May 2002 21:58:17 EDT

54 lines

Re: Re Hole Fill

Werner Engelmaier

Tue, 21 May 2002 10:51:22 EDT

82 lines

New Thread

ReA610HoleFill

ReA610HoleFill

<>

Sat, 11 May 2002 16:36:24 EDT

42 lines

Re: ReA610HoleFill

Sauer, Steven T.

Mon, 13 May 2002 08:32:58 -0400

49 lines

Re: ReA610HoleFill

Jack Crawford

Mon, 13 May 2002 09:43:20 -0500

190 lines

Re: ReA610HoleFill

Mel Parrish

Mon, 13 May 2002 09:47:17 -0500

104 lines

New Thread

really big boards

really big boards

Guy Ramsey

Fri, 17 May 2002 07:14:29 -0400

84 lines

Re: really big boards

Marsico, James

Fri, 17 May 2002 08:46:59 -0400

48 lines

Re: really big boards

Guy Ramsey

Fri, 17 May 2002 10:30:52 -0400

78 lines

Re: really big boards

Eric Dawson

Fri, 17 May 2002 15:39:53 +0100

74 lines

Re: really big boards

Hinners Hans M Civ WRALC/LUGE

Fri, 17 May 2002 16:08:14 +0100

118 lines

Re: really big boards

Barmuta, Mike

Fri, 17 May 2002 09:40:11 -0700

74 lines

Re: really big boards

Brummer Chuck

Fri, 17 May 2002 09:40:04 -0700

142 lines

Re: really big boards

Guy Ramsey

Fri, 17 May 2002 15:13:11 -0400

189 lines

Re: really big boards

Dwight Mattix

Fri, 17 May 2002 12:11:25 -0700

80 lines

Re: really big boards

Alain Savard

Fri, 17 May 2002 15:21:51 -0400

83 lines

Re: really big boards

Geoff Layhe

Mon, 20 May 2002 09:12:38 +0100

190 lines

Re: really big boards

Mair, Christian

Wed, 22 May 2002 11:37:11 +0200

92 lines

Re: really big boards

Dougal Stewart

Wed, 22 May 2002 16:36:33 +0100

140 lines

Re: really big boards

Atkinson, Neil

Fri, 24 May 2002 07:43:44 +0100

543 lines

Re: really big boards

Roland Jaquet

Fri, 24 May 2002 21:55:44 +0200

371 lines

New Thread

really big boards - all humor, no tech value

Re: really big boards - all humor, no tech value

Dave Hillman

Fri, 17 May 2002 13:07:04 -0500

120 lines

Re: really big boards - all humor, no tech value

Guy Ramsey

Fri, 17 May 2002 17:04:11 -0400

156 lines

Re: really big boards - all humor, no tech value

Ed Popielarski

Sat, 18 May 2002 08:01:17 -0700

138 lines

Re: really big boards - all humor, no tech value

Randy Bock Sr.

Sat, 18 May 2002 11:58:06 -0400

180 lines

New Thread

Recommended solder paste for a 6 layer double-sided board with CSP & BGA packages

Recommended solder paste for a 6 layer double-sided board with CSP & BGA packages

Francis Sun

Mon, 13 May 2002 10:12:36 -0400

34 lines

New Thread

Reflow Oven Recommendations

Reflow Oven Recommendations

Mcmaster, Michael

Thu, 30 May 2002 16:37:11 -0700

70 lines

Re: Reflow Oven Recommendations

Phil Kinner

Fri, 31 May 2002 09:08:15 +0100

174 lines

New Thread

Repair/Mod pads

Repair/Mod pads

<>

Tue, 21 May 2002 20:26:00 +0800

39 lines

Re: Repair/Mod pads

Linda Langley

Tue, 21 May 2002 09:02:37 -0400

73 lines

Re: Repair/Mod pads

Guy Ramsey

Tue, 21 May 2002 10:43:43 -0400

74 lines

Re: Repair/Mod pads

Jeff Ferry

Tue, 21 May 2002 10:49:24 -0400

90 lines

Re: Repair/Mod pads

Neda Thrash

Tue, 21 May 2002 10:15:20 -0500

71 lines

New Thread

RePalladium Leads

RePalladium Leads

<>

Thu, 9 May 2002 09:41:15 EDT

31 lines

Re: RePalladium Leads

Alex Krstic

Thu, 9 May 2002 13:06:00 -0600

64 lines

New Thread

Restoring solderability

Restoring solderability

Paul Truit

Wed, 15 May 2002 13:41:25 -0400

41 lines

Re: Restoring solderability

Guy Ramsey

Wed, 15 May 2002 15:33:30 -0400

81 lines

Re: Restoring solderability

David Fish

Wed, 15 May 2002 15:32:40 -0700

72 lines

Re: Restoring solderability

Bloomquist, Ken

Wed, 15 May 2002 13:58:22 -0700

69 lines

Re: Restoring solderability

Guy Ramsey

Thu, 16 May 2002 07:29:06 -0400

255 lines

Re: Restoring solderability

Dave Hillman

Thu, 16 May 2002 10:13:55 -0500

100 lines

New Thread

resume post

resume post

William Sullivan

Thu, 23 May 2002 07:22:38 -0700

1012 lines

New Thread

Rod Smith/Endicott/IBM is out of the office.

Rod Smith/Endicott/IBM is out of the office.

Rod Smith

Fri, 31 May 2002 11:11:40 -0400

24 lines

New Thread

safety committee

safety committee

<>

Thu, 2 May 2002 13:11:23 -0500

33 lines

Re: safety committee

Earl Moon

Thu, 2 May 2002 14:55:13 -0400

66 lines

Re: safety committee

Dan R. Johnson

Thu, 2 May 2002 13:14:47 -0700

26 lines

Re: safety committee

Hinners Hans M Civ WRALC/LUGE

Fri, 3 May 2002 21:48:32 +0100

79 lines

New Thread

Sanmina HDI

Re: Sanmina HDI

Jana Carraway

Mon, 6 May 2002 15:50:27 -0700

73 lines

New Thread

Sanminaized

Sanminaized

Earl Moon

Mon, 6 May 2002 14:00:42 -0500

83 lines

New Thread

Shear stress on laser vias

Shear stress on laser vias

Franck, George

Thu, 2 May 2002 10:47:33 -0400

40 lines

New Thread

Side fillet requirements

Side fillet requirements

Frank Kimmey

Mon, 20 May 2002 15:16:53 -0700

35 lines

Re: Side fillet requirements

<>

Tue, 21 May 2002 13:41:17 +0800

83 lines

Re: Side fillet requirements

Mel Parrish

Tue, 21 May 2002 07:36:56 -0500

132 lines

Re: Side fillet requirements

Guy Ramsey

Tue, 21 May 2002 08:57:56 -0400

54 lines

Re: Side fillet requirements

Frank Kimmey

Tue, 21 May 2002 08:25:32 -0700

106 lines

Re: Side fillet requirements

Greg Scott

Tue, 21 May 2002 09:55:57 -0700

143 lines

Re: Side fillet requirements

David Ricketts

Tue, 21 May 2002 11:22:20 -0700

72 lines

Re: Side fillet requirements

Sauer, Steven T.

Wed, 22 May 2002 08:19:57 -0400

48 lines

Re: Side fillet requirements

Mel Parrish

Wed, 22 May 2002 11:00:55 -0500

90 lines

New Thread

Solder after reflow on Gold Immersion finish

Solder after reflow on Gold Immersion finish

Brooks,Bill

Thu, 9 May 2002 12:09:54 -0700

100 lines

Re: Solder after reflow on Gold Immersion finish

Dave Hillman

Fri, 10 May 2002 14:33:21 -0500

159 lines

Re: Solder after reflow on Gold Immersion finish

David Fish

Sun, 12 May 2002 09:17:30 -0700

211 lines

New Thread

Solder Defect Rates

Re: Solder Defect Rates

Hogg, Blair K.

Wed, 29 May 2002 15:43:09 -0400

65 lines

New Thread

Solder-UBM Separation

Solder-UBM Separation

<>

Thu, 16 May 2002 10:39:09 +0800

41 lines

Re: Solder-UBM Separation

<>

Thu, 16 May 2002 12:36:37 +0800

107 lines

Re: Solder-UBM Separation

Mike Fenner

Fri, 17 May 2002 09:08:57 +0100

91 lines

New Thread

soldermask ring v. full coat for BGA design

soldermask ring v. full coat for BGA design

Ochenas, Tom

Thu, 30 May 2002 16:57:49 -0700

180 lines

Re: soldermask ring v. full coat for BGA design

<>

Thu, 30 May 2002 20:57:48 EDT

55 lines

Re: soldermask ring v. full coat for BGA design

Ochenas, Tom

Fri, 31 May 2002 11:00:05 -0700

131 lines

Re: soldermask ring v. full coat for BGA design

Eddie Rocha

Fri, 31 May 2002 13:27:54 -0700

31 lines

Re: soldermask ring v. full coat for BGA design

Earl Moon

Fri, 31 May 2002 15:37:10 -0500

26 lines

New Thread

Some Advice on PCB tols required

Some Advice on PCB tols required

Eric Christison

Thu, 2 May 2002 13:18:41 +0100

48 lines

Re: Some Advice on PCB tols required

Guy Ramsey

Thu, 2 May 2002 14:02:21 -0400

92 lines

New Thread

Surrogate Post - Multiple Choice Question

Surrogate Post - Multiple Choice Question

Houston, Terri

Fri, 3 May 2002 12:27:26 -0600

37 lines

New Thread

SV: [TN] Recommended solder paste for a 6 layer double-sided board with CSP & BGA packages

SV: [TN] Recommended solder paste for a 6 layer double-sided board with CSP & BGA packages

Björn Kullman

Tue, 14 May 2002 08:31:25 +0200

93 lines

New Thread

SV: [TN] Vapor phase

SV: [TN] Vapor phase

Björn Kullman

Mon, 27 May 2002 08:57:25 +0200

82 lines

Re: SV: [TN] Vapor phase

Brian Ellis

Mon, 27 May 2002 12:10:38 +0300

101 lines

Re: SV: [TN] Vapor phase

Graham Naisbitt

Mon, 27 May 2002 10:36:46 +0100

182 lines

Re: SV: [TN] Vapor phase

Mike Fenner

Mon, 27 May 2002 14:20:14 +0100

119 lines

Re: SV: [TN] Vapor phase

Graham Naisbitt

Mon, 27 May 2002 17:05:14 +0100

191 lines

Re: SV: [TN] Vapor phase

Mike Fenner

Tue, 28 May 2002 16:59:39 +0100

111 lines

New Thread

Tape & Reel Size for 0402 Components

Tape & Reel Size for 0402 Components

Becerra Alejandro

Thu, 16 May 2002 13:00:35 -0500

77 lines

Re: Tape & Reel Size for 0402 Components

Krug, Dick

Thu, 16 May 2002 17:00:18 -0400

85 lines

New Thread

TechNet Cops are NOT on vacation

TechNet Cops are NOT on vacation

Jack Crawford

Fri, 31 May 2002 16:44:13 -0500

70 lines

New Thread

TechNet Digest - 12 May 2002 to 13 May 2002 (#2002-109)

Re: TechNet Digest - 12 May 2002 to 13 May 2002 (#2002-109)

Brock Hunter

Tue, 14 May 2002 02:25:06 -0400

36 lines

Re: TechNet Digest - 12 May 2002 to 13 May 2002 (#2002-109)

Jim Wertin

Tue, 14 May 2002 11:14:47 -0700

834 lines

New Thread

testing via holes

testing via holes

Kris Keating

Fri, 17 May 2002 10:07:34 -0400

25 lines

Re: testing via holes

Dwight Mattix

Fri, 17 May 2002 12:06:13 -0700

50 lines

Re: testing via holes

Werner Engelmaier

Sun, 19 May 2002 20:42:25 EDT

38 lines

Re: testing via holes

Eric Dawson

Mon, 20 May 2002 08:19:37 +0100

33 lines

New Thread

Texas Designer's Learning Symposium - May 20 - 25, 2002

Texas Designer's Learning Symposium - May 20 - 25, 2002

Barbara Burcham

Wed, 8 May 2002 13:26:08 -0500

74 lines

New Thread

The Best Opportunity in Texas!!!

The Best Opportunity in Texas!!!

Stephannie Caliendo

Thu, 16 May 2002 20:08:07 -0500

69 lines

New Thread

Thickness of finish

Thickness of finish

Bev Christian

Wed, 1 May 2002 17:15:04 -0400

56 lines

New Thread

Tinning SMD diodes

Tinning SMD diodes

Robert Meston

Tue, 7 May 2002 07:37:11 -0500

37 lines

Re: Tinning SMD diodes

Marsico, James

Tue, 7 May 2002 10:41:12 -0400

84 lines

Re: Tinning SMD diodes

Wenger, George M.

Tue, 7 May 2002 12:35:34 -0400

132 lines

New Thread

TM650

TM650

tony steinke

Thu, 23 May 2002 16:43:36 -0700

66 lines

Re: TM650

Brian McCrory

Thu, 23 May 2002 16:32:38 -0700

85 lines

New Thread

Trough hole soldering

Trough hole soldering

Marki Sasportas

Sun, 19 May 2002 16:59:52 +0200

26 lines

Re: Trough hole soldering

Rob Legg

Mon, 20 May 2002 00:38:14 -0400

55 lines

New Thread

TypeUR conformal coatings

TypeUR conformal coatings

Linda Woody

Wed, 22 May 2002 14:24:06 -0500

31 lines

Re: TypeUR conformal coatings

Chris Almeras

Wed, 22 May 2002 15:18:07 -0500

74 lines

Re: TypeUR conformal coatings

Phil Kinner

Thu, 23 May 2002 15:20:41 +0100

232 lines

New Thread

V-groove 031 thick PCB

V-groove 031 thick PCB

<>

Mon, 6 May 2002 10:08:19 -0700

34 lines

New Thread

Vacuum ???

Vacuum ???

Rudy Sedlak

Wed, 1 May 2002 08:52:35 EDT

58 lines

New Thread

vacuum seal and MSD

vacuum seal and MSD

Earl Moon

Wed, 1 May 2002 18:29:23 -0500

38 lines

Re: vacuum seal and MSD

<>

Wed, 1 May 2002 20:39:32 EDT

39 lines

Vacuum Seal and MSD

Francois Monette

Thu, 2 May 2002 09:50:22 -0400

113 lines

Re: Vacuum Seal and MSD

Earl Moon

Thu, 2 May 2002 10:46:45 -0400

172 lines

New Thread

Vacuum Sealing

Vacuum Sealing

bbarr

Wed, 1 May 2002 11:05:46 -0400

40 lines

Re: Vacuum Sealing

Creswick, Steven

Wed, 1 May 2002 14:26:01 -0400

92 lines

New Thread

Vacuum sealing equipment

Vacuum sealing equipment

Francois Monette

Thu, 2 May 2002 10:27:39 -0400

71 lines

Re: Vacuum sealing equipment

Earl Moon

Thu, 2 May 2002 11:36:06 -0400

112 lines

Re: Vacuum sealing equipment

Earl Moon

Thu, 2 May 2002 11:44:23 -0400

104 lines

New Thread

Vacuum sealing equipment...

Re: Vacuum sealing equipment...

Brian Ellis

Wed, 1 May 2002 10:18:32 +0300

70 lines

Re: Vacuum sealing equipment...

Charles Caswell

Wed, 1 May 2002 07:09:14 -0500

85 lines

Re: Vacuum sealing equipment...

Charles Caswell

Wed, 1 May 2002 07:10:43 -0500

119 lines

Re: Vacuum sealing equipment...

<>

Wed, 1 May 2002 08:39:44 EDT

66 lines

Re: Vacuum sealing equipment...

James TerVeen

Wed, 1 May 2002 09:42:46 -0400

68 lines

Vacuum sealing equipment...

Francois Monette

Wed, 1 May 2002 09:53:21 -0400

73 lines

Re: Vacuum sealing equipment...

Earl Moon

Wed, 1 May 2002 09:02:53 -0500

28 lines

Re: Vacuum sealing equipment...

Tempea, Ioan

Wed, 1 May 2002 10:50:34 -0400

135 lines

Re: Vacuum sealing equipment...

Dan R. Johnson

Wed, 1 May 2002 08:03:23 -0700

29 lines

Re: Vacuum sealing equipment...

D.Terstegge

Thu, 2 May 2002 18:37:00 +0200

257 lines

Re: Vacuum sealing equipment...

Earl Moon

Thu, 2 May 2002 11:47:18 -0500

28 lines

New Thread

Vapor phase

Vapor phase

Stefano Riccardi

Fri, 24 May 2002 09:31:50 +0200

70 lines

Re: Vapor phase

Brian Ellis

Fri, 24 May 2002 14:56:50 +0300

48 lines

Re: Vapor phase

Mike Fenner

Fri, 24 May 2002 17:50:25 +0100

91 lines

Re: Vapor phase

rgrant

Fri, 24 May 2002 11:55:26 -0600

89 lines

Re: Vapor phase

Brian Ellis

Sat, 25 May 2002 09:06:27 +0300

48 lines

Re: Vapor phase

Stefano Riccardi

Mon, 27 May 2002 08:31:58 +0200

148 lines

Re: Vapor phase

Brian Ellis

Mon, 27 May 2002 12:12:07 +0300

28 lines

Re: Vapor phase

rgrant

Tue, 28 May 2002 12:52:56 -0600

177 lines

Re: Vapor phase

Earl Moon

Tue, 28 May 2002 14:22:10 -0500

22 lines

Re: Vapor phase

<>

Tue, 28 May 2002 16:06:12 EDT

51 lines

Re: Vapor phase

Earl Moon

Tue, 28 May 2002 15:05:35 -0500

30 lines

Re: Vapor phase

Graham Naisbitt

Tue, 28 May 2002 22:50:41 +0100

99 lines

Re: Vapor phase

Earl Moon

Tue, 28 May 2002 18:07:02 -0500

33 lines

Re: Vapor phase

<>

Wed, 29 May 2002 10:29:29 -0400

25 lines

New Thread

Via Capacitance

Via Capacitance

<>

Mon, 20 May 2002 11:57:38 +0200

32 lines

Re: Via Capacitance

Seth Goodman

Mon, 20 May 2002 17:43:02 -0500

83 lines

New Thread

Via Plug

Re: Via Plug

Dwight Mattix

Thu, 2 May 2002 10:55:02 -0700

97 lines

New Thread

Vias-in-pads

Vias-in-pads

Denis Lefebvre

Tue, 7 May 2002 12:15:40 -0700

94 lines

Re: Vias-in-pads

Earl Moon

Tue, 7 May 2002 14:25:34 -0500

36 lines

Re: Vias-in-pads

ryan

Wed, 24 Apr 2002 19:52:21 -0400

350 lines

Re: Vias-in-pads

Bob Perkins

Fri, 10 May 2002 08:27:12 -0700

340 lines

New Thread

VIRUS WARNNING !!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!

VIRUS WARNNING !!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!

Bill Dworak

Mon, 6 May 2002 00:06:36 -0700

134 lines

Re: VIRUS WARNNING !!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!

Randy Bock Sr.

Mon, 6 May 2002 07:36:03 -0400

105 lines

New Thread

Voids in BGA/CSP Balls

Voids in BGA/CSP Balls

Zweigart, Siegmund

Wed, 29 May 2002 17:43:13 +0200

28 lines

New Thread

Voids in fine-pitch BGAs after reflow

Voids in fine-pitch BGAs after reflow

Håkan Törnqvist (EMW)

Thu, 16 May 2002 11:10:18 +0200

36 lines

Re: Voids in fine-pitch BGAs after reflow

Guy Ramsey

Fri, 17 May 2002 07:42:39 -0400

167 lines

Re: Voids in fine-pitch BGAs after reflow

Werner Engelmaier

Fri, 17 May 2002 19:33:14 EDT

41 lines

New Thread

Voids on 0.75 mm micro-BGA

Voids on 0.75 mm micro-BGA

<>

Wed, 8 May 2002 10:14:39 -0700

40 lines

Re: Voids on 0.75 mm micro-BGA

Earl Moon

Wed, 8 May 2002 12:47:23 -0500

29 lines

New Thread

Wave solder re-runs/re-work

Wave solder re-runs/re-work

David White

Thu, 2 May 2002 11:14:20 -0400

29 lines

Re: Wave solder re-runs/re-work

Earl Moon

Thu, 2 May 2002 12:16:13 -0500

28 lines

Re: Wave solder re-runs/re-work

<>

Fri, 3 May 2002 08:05:25 +0800

107 lines

Re: Wave solder re-runs/re-work

David Douthit

Thu, 2 May 2002 22:08:04 -0700

118 lines

Re: Wave solder re-runs/re-work

<>

Fri, 3 May 2002 23:58:21 EDT

24 lines

New Thread

Wave solder re-runs/re-work exposed copper

Re: Wave solder re-runs/re-work exposed copper

Guy Ramsey

Fri, 3 May 2002 07:10:54 -0400

157 lines

Re: Wave solder re-runs/re-work exposed copper

Kathy Kuhlow

Fri, 3 May 2002 09:09:48 -0500

87 lines

Re: Wave solder re-runs/re-work exposed copper

Mel Parrish

Fri, 3 May 2002 11:29:33 -0500

203 lines

Re: Wave solder re-runs/re-work exposed copper

<>

Mon, 6 May 2002 13:39:17 +0800

206 lines

Re: Wave solder re-runs/re-work exposed copper

Guy Ramsey

Mon, 6 May 2002 08:51:07 -0400

196 lines

New Thread

[TN} Vacuum Sealing...

[TN} Vacuum Sealing...

<>

Wed, 1 May 2002 22:52:44 EDT

27 lines

Re: [TN} Vacuum Sealing...

Earl Moon

Thu, 2 May 2002 06:36:12 -0400

76 lines

Advanced Options


Options

Log In

Log In

Get Password

Get Password


Search Archives

Search Archives


Subscribe or Unsubscribe

Subscribe or Unsubscribe


Archives

May 2019
April 2019
March 2019
February 2019
January 2019
December 2018
November 2018
October 2018
September 2018
August 2018
July 2018
June 2018
May 2018
April 2018
March 2018
February 2018
January 2018
December 2017
November 2017
October 2017
September 2017
August 2017
July 2017
June 2017
May 2017
April 2017
March 2017
February 2017
January 2017
December 2016
November 2016
October 2016
September 2016
August 2016
July 2016
June 2016
May 2016
April 2016
March 2016
February 2016
January 2016
December 2015
November 2015
October 2015
September 2015
August 2015
July 2015
June 2015
May 2015
April 2015
March 2015
February 2015
January 2015
December 2014
November 2014
October 2014
September 2014
August 2014
July 2014
June 2014
May 2014
April 2014
March 2014
February 2014
January 2014
December 2013
November 2013
October 2013
September 2013
August 2013
July 2013
June 2013
May 2013
April 2013
March 2013
February 2013
January 2013
December 2012
November 2012
October 2012
September 2012
August 2012
July 2012
June 2012
May 2012
April 2012
March 2012
February 2012
January 2012
December 2011
November 2011
October 2011
September 2011
August 2011
July 2011
June 2011
May 2011
April 2011
March 2011
February 2011
January 2011
December 2010
November 2010
October 2010
September 2010
August 2010
July 2010
June 2010
May 2010
April 2010
March 2010
February 2010
January 2010
December 2009
November 2009
October 2009
September 2009
August 2009
July 2009
June 2009
May 2009
April 2009
March 2009
February 2009
January 2009
December 2008
November 2008
October 2008
September 2008
August 2008
July 2008
June 2008
May 2008
April 2008
March 2008
February 2008
January 2008
December 2007
November 2007
October 2007
September 2007
August 2007
July 2007
June 2007
May 2007
April 2007
March 2007
February 2007
January 2007
December 2006
November 2006
October 2006
September 2006
August 2006
July 2006
June 2006
May 2006
April 2006
March 2006
February 2006
January 2006
December 2005
November 2005
October 2005
September 2005
August 2005
July 2005
June 2005
May 2005
April 2005
March 2005
February 2005
January 2005
December 2004
November 2004
October 2004
September 2004
August 2004
July 2004
June 2004
May 2004
April 2004
March 2004
February 2004
January 2004
December 2003
November 2003
October 2003
September 2003
August 2003
July 2003
June 2003
May 2003
April 2003
March 2003
February 2003
January 2003
December 2002
November 2002
October 2002
September 2002
August 2002
July 2002
June 2002
May 2002
April 2002
March 2002
February 2002
January 2002
December 2001
November 2001
October 2001
September 2001
August 2001
July 2001
June 2001
May 2001
April 2001
March 2001
February 2001
January 2001
December 2000
November 2000
October 2000
September 2000
August 2000
July 2000
June 2000
May 2000
April 2000
March 2000
February 2000
January 2000
December 1999
November 1999
October 1999
September 1999
August 1999
July 1999
June 1999
May 1999
April 1999
March 1999
February 1999
January 1999
December 1998
November 1998
October 1998
September 1998
August 1998
July 1998
June 1998
May 1998
April 1998
March 1998
February 1998
January 1998
December 1997
November 1997
October 1997
September 1997
August 1997
July 1997
June 1997
May 1997
April 1997
March 1997
February 1997
January 1997
1996
1995

ATOM RSS1 RSS2



LISTSERV.IPC.ORG

Secured by F-Secure Anti-Virus CataList Email List Search Powered by the LISTSERV Email List Manager