Hi Ramon
If you want to use a spray gun, by it's nature it is going to atomize the coating material, otherwise it wouldn't be a spray. There are non atomized options - curtain coaters, and Asymtek's swirl coat process, but as far as I know those aren't useable in a hand application technique.
As for a gun that sprays pure coating (unthinned), it will depend on what the coating is - what the viscosity is - but should not be a problem. We use Binks spray guns, originally the standard guns but in recent years the HVLP spray guns, and with both you can change the nozzle to accommodate different viscosity materials.
As for clogs and the number of parts, the HVLP gun has a few more parts than the older ones, but I think it's a worthwhile tradeoff since they waste less material.
regards
Graham Collins
Process Engineer,
Northrop Grumman
Atlantic Facility of Litton Systems Canada
(902) 873-2000 ext 6215
>>> [log in to unmask] 05/14/02 03:47PM >>>
My question is about conformal coating. We want to manualy
conformal coat boards using a spray gun. Does anybody have knowledge of a
gun that sprays pure coating without any atomization of the coating and that
internally have very few parts, in case it clogs, and needs to be
cleaned.
Regards,
Ramon
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|