<List>Re: [TN] ENIG roughness (2 messages)
Acid Traps (11 messages)
After RoHS aftermath meeting (4 messages)
Altera BGA, lead-free or not? (26 messages)
Anti crack paste (4 messages)
Arlon Thermount discontinued (4 messages)
Attaching a Test Board to an Existing Footprint (10 messages)
BGA and conformal coating (24 messages)
BGA anomaly (27 messages)
BGA Reballing Service in Penang? (1 message)
Bizzare Phenomena... (18 messages)
Brittle Fracture (5 messages)
CALL FOR PARTICIPATION - IPC/JEDEC Global Conference, 4/17-18/07 in Boston, MA (2 messages)
CEI/IEC 68-2-60: 1995 equivalents?? (1 message)
Chemistry in Vias (3 messages)
China "Complying with RoHS" Friday, November 17, 2006|TÜV Product Service Ltd (1 message)
China RoHS - are you up to speed? (1 message)
Cleaning media for no clean paste (8 messages)
Cleaning No Clean Assemblies (2 messages)
cloth with wires (5 messages)
conformal coatings as under fills (1 message)
conformal coatings as underfills (1 message)
Copper Dissolution (10 messages)
Delam from separating boards (8 messages)
Delamination pics (IS410) (12 messages)
Die Bonder Recommendation (2 messages)
Dissolution Rate of Tin (2 messages)
Duofoil-MLB release plate (1 message)
Electrolytic Ni/Au issue (2 messages)
ENIG Risks (1 message)
ENIG roughness (7 messages)
EU not busting for RoHS violations yet (3 messages)
Flip Chip Assembly (1 message)
For The Ladies (1 message)
Friday quote - NTC (3 messages)
Gold Embrittlement (42 messages)
Happy Thanksgiving (2 messages)
Hard Gold Electro-Damage (1 message)
Henry Rekers is out of the office. (1 message)
IPC China RoHS Webcast you can'ts miss! (1 message)
IPC Workshops: Design for Manufacture & Compliant Electronics for EU Applications - Fredericksburg, VA (1 message)
IPC's Design for Excellence - Staying Current with Technology (2 messages)
IPC's Design for Excellence webcast series and Exploring the Challenges workshop (1 message)
IPC's Design for Manufacture/Compliant Electronics for EU Applications - December 4-6, 2006 in Fredericksburg, VA (1 message)
IPC/JEDEC Conference in Boston you won't want to miss! (1 message)
IPC/JEDEC International Conference on LF Components & Assemblies in Boston, MA (1 message)
IPC/JEDEC International Conference on LF Electronic Components & Assemblies "RoHS & Beyond" in Boston, MA (1 message)
IPC/JEDEC International Conference on LF Electronic Components & Assemblies - December 5-7, 2006, in Boston (1 message)
IPC4101B/126 7 129 (4 messages)
Japan Reaches out (1 message)
Lead Spacing (1 message)
Looking for fab shop 4-6 oz copper capability (4 messages)
Manufacturing with Electroplated Gold PCB in LF applications (3 messages)
masking question (2 messages)
More delam (24 messages)
More Separation in BGA joints (6 messages)
Move Up, Keep Up & Catch Up with the latest IPC workshops in January 2007 (1 message)
Need urgent feedback --- Routing of track on component side (1 message)
New round of stakeholder consultation for RoHS exemption requests (8 messages)
NTC - George's Friday Clip... (2 messages)
NTC-APEXPO Promo (1 message)
NTC-Have a Happy Thanksgiving (3 messages)
NTC:is there a audiofil out there? (8 messages)
Official release of the new exemptions (6 messages)
One solder Ball Not Connected on a No Connect Pad After Rework (10 messages)
pallatech mls (5 messages)
Perchlorate Test Lab? (1 message)
Power Via Capping (8 messages)
Pricing on RoHS lab analysis (1 message)
PWB mannufacturer Audit (5 messages)
PWB/PCB raw card stamping (2 messages)
Question about J-STD-001 cleanliness designator C-22 (6 messages)
Question for Mr Yoda (1 message)
Request for Weave Exposure / Texture Photographs (1 message)
Request from another forum (1 message)
Rework Requires Approval & Vehement Tech (6 messages)
RoHS and Aerospace (6 messages)
Rohus version (3 messages)
routing of track on component side in between the pads (3 messages)
Separation in BGA joints (30 messages)
Service Request 10567441: BGA (2 messages)
Silver Plating (3 messages)
solder projections (3 messages)
Solder Voids in Hole barrel after W/S (3 messages)
Soldering Anomaly (9 messages)
Stacking chip capacitors (5 messages)
Stencils (5 messages)
Strong demand to keep tin prices high - article link (2 messages)
Terry L Huddleston/ElecTec/Teledyne is out of the office. (1 message)
Tin - Lead Solder / Gold connector interface (2 messages)
TMA recommendation (9 messages)
Ultimate PCB assembly books (3 messages)
Ultimate PCB assembly books (and more) (7 messages)
UV flourescent pens for rework identification. (7 messages)
Warning to expert witnesses in Houston (29 messages)
What to do with a 9 pin .5mm BGA? (4 messages)
who brought the cat? (1 message)
Yet Another Warp & Twist Question (1 message)
[Fwd: Re: [TN] Warning to expert witnesses in Houston] (4 messages)
[LF] black pad (2 messages)
[LF] China RoHS news (1 message)
[LF] EU Not Busting for RoHS Violations Yet (1 message)
[LF] Gold Embrittlement (7 messages)
[LF] Why EU Not Busting for RoHS Violations Yet (10 messages)
[MDPP] China Labeling (1 message)
[TN] China "Complying with RoHS" Friday, November 17, 2006|TÜV Product Service Ltd (1 message)
[TN] BGA anomaly (18 messages)
[TN] FW: [MDPP] China Labeling (1 message)
[TN] FW: [MDPP] China Labeling NTC (1 message)
[TN] Solder Voids in Hole barrel  after W/S (1 message)

LISTSERV Archives

LISTSERV Archives

TECHNET Home

TECHNET Home

Subject Sorted by Subject, Chronologically

From

Date

Size

New Thread

<List>Re: [TN] ENIG roughness

Re: Re: [TN] ENIG roughness

Gary Warner

Thu, 30 Nov 2006 12:03:17 -0700

57 lines

Re: Re: [TN] ENIG roughness

Vladimir Igoshev

Thu, 30 Nov 2006 16:57:10 -0500

90 lines

New Thread

Acid Traps

Acid Traps

John Foster

Tue, 21 Nov 2006 08:53:02 -0800

37 lines

Re: Acid Traps

Frank Kimmey

Tue, 21 Nov 2006 09:10:16 -0800

85 lines

Re: Acid Traps

Deac Descoteaux

Tue, 21 Nov 2006 12:22:14 -0500

160 lines

Re: Acid Traps

Frank Kimmey

Tue, 21 Nov 2006 09:35:17 -0800

188 lines

Re: Acid Traps

Wayne Thayer

Tue, 21 Nov 2006 13:34:11 -0500

244 lines

Re: Acid Traps

Dan Skweres

Tue, 21 Nov 2006 13:57:38 -0600

271 lines

Re: Acid Traps

John Foster

Tue, 21 Nov 2006 16:14:46 -0800

295 lines

Re: Acid Traps

Edward Szpruch

Wed, 22 Nov 2006 07:49:24 +0200

70 lines

Re: Acid Traps

Wayne Thayer

Wed, 22 Nov 2006 07:50:33 -0500

101 lines

Re: Acid Traps

ZLATKO BIJEDIC

Thu, 23 Nov 2006 16:28:47 -0800

47 lines

Re: Acid Traps

Whittaker, Dewey (EHCOE)

Tue, 28 Nov 2006 07:20:04 -0700

185 lines

New Thread

After RoHS aftermath meeting

After RoHS aftermath meeting

John Burke

Fri, 3 Nov 2006 17:03:37 -0800

57 lines

Re: After RoHS aftermath meeting

Joe Fjelstad

Fri, 3 Nov 2006 23:18:46 EST

26 lines

Re: After RoHS aftermath meeting

Joe Fjelstad

Fri, 3 Nov 2006 23:18:46 EST

46 lines

Re: After RoHS aftermath meeting

Joe Fjelstad

Fri, 3 Nov 2006 23:18:46 EST

47 lines

New Thread

Altera BGA, lead-free or not?

Altera BGA, lead-free or not?

Steve Gregory

Tue, 7 Nov 2006 08:19:15 -0600

36 lines

Re: Altera BGA, lead-free or not?

Kerry McMullen

Tue, 7 Nov 2006 09:28:30 -0500

87 lines

Re: Altera BGA, lead-free or not?

Wenger, George M.

Tue, 7 Nov 2006 09:32:41 -0500

59 lines

Re: Altera BGA, lead-free or not?

Steve Gregory

Tue, 7 Nov 2006 08:56:51 -0600

109 lines

Re: Altera BGA, lead-free or not?

Genny Gibbard

Tue, 7 Nov 2006 09:14:17 -0600

141 lines

Re: Altera BGA, lead-free or not?

Peter Wong

Tue, 7 Nov 2006 09:27:11 -0800

71 lines

Re: Altera BGA, lead-free or not?

Whittaker, Dewey (EHCOE)

Tue, 7 Nov 2006 10:49:08 -0700

98 lines

Re: Altera BGA, lead-free or not?

Thad Schultz

Tue, 7 Nov 2006 10:58:42 -0700

75 lines

Re: Altera BGA, lead-free or not?

Stadem, Richard D.

Tue, 7 Nov 2006 12:09:25 -0600

92 lines

Re: Altera BGA, lead-free or not?

John Burke

Tue, 7 Nov 2006 10:11:26 -0800

123 lines

Re: Altera BGA, lead-free or not?

Stadem, Richard D.

Tue, 7 Nov 2006 12:13:06 -0600

133 lines

Re: Altera BGA, lead-free or not?

Stadem, Richard D.

Tue, 7 Nov 2006 12:13:55 -0600

145 lines

Re: Altera BGA, lead-free or not?

Dehoyos, Ramon

Tue, 7 Nov 2006 13:24:07 -0500

157 lines

Re: Altera BGA, lead-free or not?

Steve Gregory

Tue, 7 Nov 2006 12:25:31 -0600

131 lines

Re: Altera BGA, lead-free or not?

Dehoyos, Ramon

Tue, 7 Nov 2006 13:32:32 -0500

158 lines

Re: Altera BGA, lead-free or not?

Steve Gregory

Tue, 7 Nov 2006 13:15:03 -0600

198 lines

Re: Altera BGA, lead-free or not?

Stadem, Richard D.

Tue, 7 Nov 2006 13:40:21 -0600

222 lines

Re: Altera BGA, lead-free or not?

Genny Gibbard

Tue, 7 Nov 2006 13:46:34 -0600

245 lines

Re: Altera BGA, lead-free or not?

Stadem, Richard D.

Tue, 7 Nov 2006 13:50:34 -0600

268 lines

Re: Altera BGA, lead-free or not?

Hfjord

Tue, 7 Nov 2006 22:31:13 +0100

148 lines

Re: Altera BGA, lead-free or not?

Stadem, Richard D.

Tue, 7 Nov 2006 15:48:57 -0600

179 lines

Re: Altera BGA, lead-free or not?

Whittaker, Dewey (EHCOE)

Tue, 7 Nov 2006 14:49:24 -0700

188 lines

Re: Altera BGA, lead-free or not?

Hfjord

Tue, 7 Nov 2006 22:56:35 +0100

200 lines

Re: Altera BGA, lead-free or not?

Genny Gibbard

Tue, 7 Nov 2006 16:35:47 -0600

302 lines

Re: Altera BGA, lead-free or not?

John Burke

Tue, 7 Nov 2006 16:59:33 -0800

160 lines

Re: Altera BGA, lead-free or not?

- Bogert

Sat, 11 Nov 2006 14:39:50 -0500

76 lines

New Thread

Anti crack paste

Anti crack paste

Braddock, Iain

Wed, 29 Nov 2006 14:29:23 -0000

42 lines

Re: Anti crack paste

Kevin Glidden

Wed, 29 Nov 2006 09:35:59 -0500

71 lines

Re: Anti crack paste

Braddock, Iain

Wed, 29 Nov 2006 14:46:19 -0000

110 lines

Re: Anti crack paste

Fox, Ian

Wed, 29 Nov 2006 18:24:57 -0000

138 lines

New Thread

Arlon Thermount discontinued

Arlon Thermount discontinued

Kevin Glidden

Tue, 14 Nov 2006 09:17:06 -0500

34 lines

Re: Arlon Thermount discontinued

Steve Gregory

Tue, 14 Nov 2006 08:48:46 -0600

62 lines

Re: Arlon Thermount discontinued

Kevin Glidden

Tue, 14 Nov 2006 10:04:27 -0500

33 lines

Re: Arlon Thermount discontinued

Fox, Ian

Tue, 14 Nov 2006 15:08:31 -0000

98 lines

New Thread

Attaching a Test Board to an Existing Footprint

Attaching a Test Board to an Existing Footprint

Jack Olson

Mon, 20 Nov 2006 13:13:11 -0600

36 lines

Re: Attaching a Test Board to an Existing Footprint

Bloomquist, Ken

Mon, 20 Nov 2006 11:17:08 -0800

47 lines

Re: Attaching a Test Board to an Existing Footprint

Steve Smith

Mon, 20 Nov 2006 14:17:45 -0500

65 lines

Re: Attaching a Test Board to an Existing Footprint

Stadem, Richard D.

Mon, 20 Nov 2006 13:22:39 -0600

63 lines

Re: Attaching a Test Board to an Existing Footprint

Kerry McMullen

Mon, 20 Nov 2006 14:26:17 -0500

96 lines

Re: Attaching a Test Board to an Existing Footprint

Olav Folland

Mon, 20 Nov 2006 11:25:24 -0800

63 lines

Re: Attaching a Test Board to an Existing Footprint

Wayne Thayer

Mon, 20 Nov 2006 14:27:22 -0500

73 lines

Re: Attaching a Test Board to an Existing Footprint

Haynes, Kim

Mon, 20 Nov 2006 14:05:24 -0600

65 lines

Re: Attaching a Test Board to an Existing Footprint

Stadem, Richard D.

Mon, 20 Nov 2006 15:37:18 -0600

106 lines

Re: Attaching a Test Board to an Existing Footprint

Jack Olson

Tue, 21 Nov 2006 17:12:15 -0600

58 lines

New Thread

BGA and conformal coating

BGA and conformal coating

Vered BS

Mon, 20 Nov 2006 10:40:17 -0600

23 lines

Re: BGA and conformal coating

Macko, Joe @ IEC

Mon, 20 Nov 2006 10:47:27 -0800

58 lines

Re: BGA and conformal coating

Wayne Thayer

Mon, 20 Nov 2006 14:09:52 -0500

91 lines

Re: BGA and conformal coating

David D. Hillman

Mon, 20 Nov 2006 13:20:28 -0600

113 lines

Re: BGA and conformal coating

Crepeau, Phil (Space Technology)

Mon, 20 Nov 2006 11:21:52 -0800

54 lines

Re: BGA and conformal coating

Dehoyos, Ramon

Mon, 20 Nov 2006 14:26:33 -0500

57 lines

Re: BGA and conformal coating

Wayne Thayer

Mon, 20 Nov 2006 14:30:57 -0500

83 lines

Re: BGA and conformal coating

Dehoyos, Ramon

Mon, 20 Nov 2006 14:37:41 -0500

104 lines

Re: BGA and conformal coating

Werner Engelmaier

Mon, 20 Nov 2006 15:02:30 EST

25 lines

Re: BGA and conformal coating

Macko, Joe @ IEC

Mon, 20 Nov 2006 13:11:56 -0800

111 lines

Re: BGA and conformal coating

- Bogert

Mon, 20 Nov 2006 16:52:17 -0500

166 lines

Re: BGA and conformal coating

David D. Hillman

Mon, 20 Nov 2006 17:27:24 -0600

217 lines

Re: BGA and conformal coating

Crepeau, Phil (Space Technology)

Mon, 20 Nov 2006 15:43:03 -0800

258 lines

Re: BGA and conformal coating

Graham Collins

Tue, 21 Nov 2006 06:08:01 -0500

303 lines

Re: BGA and conformal coating

Graham Naisbitt

Tue, 21 Nov 2006 17:31:37 +0000

89 lines

Re: BGA and conformal coating

Dehoyos, Ramon

Wed, 22 Nov 2006 09:21:44 -0500

112 lines

Re: BGA and conformal coating

Graham Naisbitt

Wed, 22 Nov 2006 15:52:30 +0000

159 lines

Re: BGA and conformal coating

Dehoyos, Ramon

Wed, 22 Nov 2006 12:26:57 -0500

110 lines

Re: BGA and conformal coating

- Bogert

Thu, 23 Nov 2006 14:27:50 -0500

333 lines

Re: BGA and conformal coating

Graham Collins

Thu, 23 Nov 2006 15:27:55 -0500

367 lines

Re: BGA and conformal coating

Stadem, Richard D.

Mon, 27 Nov 2006 07:13:37 -0600

439 lines

Re: BGA and conformal coating

Graham Collins

Mon, 27 Nov 2006 08:52:12 -0500

501 lines

Re: BGA and conformal coating

Stadem, Richard D.

Mon, 27 Nov 2006 08:25:00 -0600

511 lines

Re: BGA and conformal coating

Whittaker, Dewey (EHCOE)

Tue, 28 Nov 2006 07:32:05 -0700

116 lines

New Thread

BGA anomaly

BGA anomaly

Braddock, Iain

Thu, 16 Nov 2006 11:17:38 -0000

64 lines

Re: BGA anomaly

[log in to unmask]

Thu, 16 Nov 2006 12:33:18 +0100

101 lines

Re: BGA anomaly

Werner Engelmaier

Thu, 16 Nov 2006 09:51:16 EST

30 lines

Re: BGA anomaly

Werner Engelmaier

Thu, 16 Nov 2006 09:53:58 EST

29 lines

Re: BGA anomaly

Joyce Koo

Thu, 16 Nov 2006 10:34:22 -0500

60 lines

Re: BGA anomaly

Braddock, Iain

Fri, 17 Nov 2006 08:25:59 -0000

134 lines

Re: BGA anomaly

Braddock, Iain

Fri, 17 Nov 2006 08:28:53 -0000

34 lines

Re: BGA anomaly

Braddock, Iain

Fri, 17 Nov 2006 08:34:57 -0000

70 lines

Re: BGA anomaly

Werner Engelmaier

Fri, 17 Nov 2006 07:28:52 EST

31 lines

Re: BGA anomaly

Tempea, Ioan

Fri, 17 Nov 2006 08:49:24 -0500

76 lines

Re: BGA anomaly

Dehoyos, Ramon

Fri, 17 Nov 2006 09:08:05 -0500

82 lines

Re: BGA anomaly

Ahne Oosterhof

Fri, 17 Nov 2006 07:19:45 -0800

90 lines

Re: BGA anomaly

Werner Engelmaier

Fri, 17 Nov 2006 15:08:14 EST

25 lines

Re: BGA anomaly

Werner Engelmaier

Fri, 17 Nov 2006 15:11:52 EST

35 lines

Re: BGA anomaly

Tempea, Ioan

Fri, 17 Nov 2006 15:52:08 -0500

59 lines

Re: BGA anomaly

Matt Kehoe

Fri, 17 Nov 2006 14:03:05 -0700

18 lines

Re: BGA anomaly

Braddock, Iain

Mon, 20 Nov 2006 11:36:11 -0000

68 lines

Re: BGA anomaly

Braddock, Iain

Mon, 20 Nov 2006 11:47:47 -0000

33 lines

Re: BGA anomaly

Dehoyos, Ramon

Mon, 20 Nov 2006 08:02:16 -0500

72 lines

Re: BGA anomaly

Werner Engelmaier

Mon, 20 Nov 2006 10:03:46 EST

31 lines

Re: BGA anomaly

Werner Engelmaier

Mon, 20 Nov 2006 10:06:24 EST

26 lines

Re: BGA anomaly

Braddock, Iain

Mon, 20 Nov 2006 15:51:37 -0000

62 lines

Re: BGA anomaly

Braddock, Iain

Mon, 20 Nov 2006 15:56:04 -0000

54 lines

Re: BGA anomaly

Stadem, Richard D.

Mon, 20 Nov 2006 11:36:40 -0600

54 lines

Re: BGA anomaly

Dehoyos, Ramon

Mon, 20 Nov 2006 13:50:21 -0500

82 lines

Re: BGA anomaly

Wenger, George M.

Mon, 20 Nov 2006 14:27:25 -0500

91 lines

Re: BGA anomaly

- Bogert

Mon, 20 Nov 2006 16:49:19 -0500

72 lines

New Thread

BGA Reballing Service in Penang?

BGA Reballing Service in Penang?

Michael Forrester

Wed, 22 Nov 2006 14:27:59 -0500

28 lines

New Thread

Bizzare Phenomena...

Re: Bizzare Phenomena...

Ed Popielarski

Wed, 1 Nov 2006 07:55:19 -0800

179 lines

Re: Bizzare Phenomena...

Ahne Oosterhof

Wed, 1 Nov 2006 12:57:22 -0800

70 lines

Re: Bizzare Phenomena...

- Bogert

Wed, 1 Nov 2006 18:34:59 -0500

107 lines

Re: Bizzare Phenomena...

Steve Gregory

Thu, 2 Nov 2006 06:46:16 -0600

135 lines

Re: Bizzare Phenomena...

Steve Gregory

Thu, 2 Nov 2006 09:41:13 -0600

194 lines

Re: Bizzare Phenomena...

Ian Hanna

Thu, 2 Nov 2006 10:54:15 -0500

219 lines

Re: Bizzare Phenomena...

Steve Gregory

Thu, 2 Nov 2006 10:10:07 -0600

247 lines

Re: Bizzare Phenomena...

Hfjord

Thu, 2 Nov 2006 17:19:36 +0100

221 lines

Re: Bizzare Phenomena...

Roger Mack

Thu, 2 Nov 2006 10:31:42 -0600

235 lines

Re: Bizzare Phenomena...

Steve Gregory

Thu, 2 Nov 2006 10:34:09 -0600

240 lines

Re: Bizzare Phenomena...

Steve Gregory

Thu, 2 Nov 2006 10:50:56 -0600

273 lines

Re: Bizzare Phenomena...

Hfjord

Thu, 2 Nov 2006 17:52:57 +0100

254 lines

Re: Bizzare Phenomena...

Steve Gregory

Thu, 2 Nov 2006 11:02:36 -0600

280 lines

Re: Bizzare Phenomena...

Hfjord

Thu, 2 Nov 2006 18:21:41 +0100

298 lines

Re: Bizzare Phenomena...

Werner Engelmaier

Thu, 2 Nov 2006 16:32:49 EST

35 lines

Re: Bizzare Phenomena...

Werner Engelmaier

Thu, 2 Nov 2006 16:46:56 EST

27 lines

Re: Bizzare Phenomena...

Bloomquist, Ken

Thu, 2 Nov 2006 13:52:08 -0800

47 lines

Re: Bizzare Phenomena...

Hfjord

Thu, 2 Nov 2006 17:52:57 +0100

274 lines

New Thread

Brittle Fracture

Re: Brittle Fracture

Werner Engelmaier

Tue, 28 Nov 2006 15:00:46 EST

29 lines

Re: Brittle Fracture

Gabriela Bogdan

Tue, 28 Nov 2006 23:06:09 +0300

56 lines

Re: Brittle Fracture

Vladimir Igoshev

Tue, 28 Nov 2006 15:13:30 -0500

66 lines

Re: Brittle Fracture

Victor G. Hernandez

Tue, 28 Nov 2006 14:20:52 -0600

93 lines

Re: Brittle Fracture

Vladimir Igoshev

Tue, 28 Nov 2006 15:23:46 -0500

96 lines

New Thread

CALL FOR PARTICIPATION - IPC/JEDEC Global Conference, 4/17-18/07 in Boston, MA

CALL FOR PARTICIPATION - IPC/JEDEC Global Conference, 4/17-18/07 in Boston, MA

Tina Nerad

Thu, 30 Nov 2006 15:31:10 -0600

56 lines

Re: CALL FOR PARTICIPATION - IPC/JEDEC Global Conference, 4/17-18/07 in Boston, MA

John Burke

Thu, 30 Nov 2006 15:53:00 -0800

86 lines

New Thread

CEI/IEC 68-2-60: 1995 equivalents??

CEI/IEC 68-2-60: 1995 equivalents??

Mike Fenner

Thu, 23 Nov 2006 16:01:02 -0000

39 lines

New Thread

Chemistry in Vias

Chemistry in Vias

James Verrette

Mon, 6 Nov 2006 17:06:29 -0500

54 lines

Re: Chemistry in Vias

Stephen Pierce

Mon, 6 Nov 2006 15:22:56 -0800

61 lines

Re: Chemistry in Vias

Wayne Thayer

Mon, 6 Nov 2006 18:44:39 -0500

122 lines

New Thread

China "Complying with RoHS" Friday, November 17, 2006|TÜV Product Service Ltd

China "Complying with RoHS" Friday, November 17, 2006|TÜV Product Service Ltd

Joe Fjelstad

Fri, 17 Nov 2006 12:44:57 EST

32 lines

New Thread

China RoHS - are you up to speed?

China RoHS - are you up to speed?

Tina Nerad

Mon, 6 Nov 2006 10:30:43 -0600

48 lines

New Thread

Cleaning media for no clean paste

Cleaning media for no clean paste

Dan Mauro

Mon, 6 Nov 2006 10:55:45 -0500

37 lines

Re: Cleaning media for no clean paste

Steve Gregory

Mon, 6 Nov 2006 10:05:55 -0600

68 lines

Re: Cleaning media for no clean paste

Brian Ellis

Mon, 6 Nov 2006 18:19:57 +0200

63 lines

Re: Cleaning media for no clean paste

Douglas O. Pauls

Mon, 6 Nov 2006 10:26:14 -0600

124 lines

Re: Cleaning media for no clean paste

Richard Kraszewski

Mon, 6 Nov 2006 11:12:15 -0600

81 lines

Re: Cleaning media for no clean paste

R Sedlak

Mon, 6 Nov 2006 15:00:26 -0800

152 lines

Re: Cleaning media for no clean paste

- Bogert

Mon, 6 Nov 2006 18:13:34 -0500

188 lines

Re: Cleaning media for no clean paste

Douglas O. Pauls

Tue, 7 Nov 2006 07:41:28 -0600

200 lines

New Thread

Cleaning No Clean Assemblies

Cleaning No Clean Assemblies

Steven Hoffner

Fri, 17 Nov 2006 18:14:49 -0800

43 lines

Re: Cleaning No Clean Assemblies

Brian Ellis

Sat, 18 Nov 2006 10:27:41 +0200

69 lines

New Thread

cloth with wires

cloth with wires

Syed Ahmad

Thu, 2 Nov 2006 16:38:40 -0600

34 lines

Re: cloth with wires

stephengregory5849

Thu, 2 Nov 2006 17:00:15 -0600

67 lines

Re: cloth with wires

Kane, Joseph E (US SSA)

Thu, 2 Nov 2006 18:00:54 -0500

65 lines

Re: cloth with wires

Gene Felder

Thu, 2 Nov 2006 15:35:08 -0800

98 lines

Re: cloth with wires

Miguel Vallejo

Thu, 2 Nov 2006 18:44:14 -0800

59 lines

New Thread

conformal coatings as under fills

conformal coatings as under fills

Edward Mines

Fri, 24 Nov 2006 08:45:50 -0800

38 lines

New Thread

conformal coatings as underfills

conformal coatings as underfills

Edward Mines

Tue, 21 Nov 2006 09:14:34 -0800

50 lines

New Thread

Copper Dissolution

Copper Dissolution

Irving Lee

Thu, 2 Nov 2006 22:44:59 +0800

31 lines

Re: Copper Dissolution

Tempea, Ioan

Thu, 2 Nov 2006 10:01:28 -0500

72 lines

Re: Copper Dissolution

Irving Lee

Thu, 2 Nov 2006 23:12:42 +0800

104 lines

Re: Copper Dissolution

Tempea, Ioan

Thu, 2 Nov 2006 10:21:03 -0500

120 lines

Re: Copper Dissolution

Irving Lee

Thu, 2 Nov 2006 23:54:04 +0800

139 lines

Re: Copper Dissolution

Corey A Peterson

Thu, 2 Nov 2006 09:55:00 -0600

70 lines

Re: Copper Dissolution

Irving Lee

Fri, 3 Nov 2006 00:06:43 +0800

92 lines

Re: Copper Dissolution

Corey A Peterson

Thu, 2 Nov 2006 12:11:46 -0600

65 lines

Re: Copper Dissolution

Werner Engelmaier

Thu, 2 Nov 2006 16:22:45 EST

25 lines

Re: Copper Dissolution

Corey A Peterson

Thu, 2 Nov 2006 12:11:46 -0600

73 lines

New Thread

Delam from separating boards

Delam from separating boards

pearl petras

Mon, 6 Nov 2006 12:37:02 -0500

35 lines

Re: Delam from separating boards

Steve Gregory

Mon, 6 Nov 2006 12:34:11 -0600

95 lines

Re: Delam from separating boards

Stadem, Richard D.

Mon, 6 Nov 2006 12:55:00 -0600

119 lines

Re: Delam from separating boards

Steve Gregory

Mon, 6 Nov 2006 13:06:32 -0600

142 lines

Re: Delam from separating boards

Dehoyos, Ramon

Mon, 6 Nov 2006 14:38:42 -0500

170 lines

Re: Delam from separating boards

pearl petras

Mon, 6 Nov 2006 15:47:59 -0500

88 lines

Re: Delam from separating boards

Steve Gregory

Mon, 6 Nov 2006 15:30:38 -0600

157 lines

Re: Delam from separating boards

pearl petras

Mon, 6 Nov 2006 16:56:27 -0500

33 lines

New Thread

Delamination pics (IS410)

Re: FW: Delamination pics (IS410)

stephen gregory

Wed, 29 Nov 2006 09:11:38 -0800

56 lines

Re: FW: Delamination pics (IS410)

Geoff Layhe of Lamar Group

Wed, 29 Nov 2006 17:22:48 -0000

104 lines

Re: FW: Delamination pics (IS410)

Ian Hanna

Wed, 29 Nov 2006 12:23:08 -0500

94 lines

Re: FW: Delamination pics (IS410)

Chuck Brummer

Wed, 29 Nov 2006 10:29:11 -0800

124 lines

Re: FW: Delamination pics (IS410)

JaMi Smith

Wed, 29 Nov 2006 11:03:59 -0800

96 lines

Re: FW: Delamination pics (IS410)

Ian Hanna

Wed, 29 Nov 2006 14:15:09 -0500

139 lines

Re: Delamination pics (IS410)

Werner Engelmaier

Wed, 29 Nov 2006 14:34:06 EST

28 lines

Re: FW: Delamination pics (IS410)

stephengregory5849

Wed, 29 Nov 2006 13:55:50 -0600

188 lines

Re: Delamination pics (IS410)

Werner Engelmaier

Wed, 29 Nov 2006 15:13:59 EST

40 lines

Re: Delamination pics (IS410)

Chuck Brummer

Wed, 29 Nov 2006 12:24:26 -0800

93 lines

Re: FW: Delamination pics (IS410)

Dwight Mattix

Wed, 29 Nov 2006 12:50:35 -0800

265 lines

Re: FW: Delamination pics (IS410)

Jeffrey Bush

Wed, 29 Nov 2006 15:39:21 -0500

93 lines

New Thread

Die Bonder Recommendation

Die Bonder Recommendation

Syed Ahmad

Thu, 30 Nov 2006 16:08:26 -0600

30 lines

Re: Die Bonder Recommendation

Joyce Koo

Thu, 30 Nov 2006 17:29:16 -0500

57 lines

New Thread

Dissolution Rate of Tin

Dissolution Rate of Tin

David D. Hillman

Wed, 15 Nov 2006 08:10:25 -0600

29 lines

Re: Dissolution Rate of Tin

ZLATKO BIJEDIC

Sun, 19 Nov 2006 06:35:17 -0800

45 lines

New Thread

Duofoil-MLB release plate

Duofoil-MLB release plate

Pradeep

Tue, 21 Nov 2006 09:52:32 +0530

38 lines

New Thread

Electrolytic Ni/Au issue

Electrolytic Ni/Au issue

Lin Leo

Mon, 20 Nov 2006 02:13:40 +0800

40 lines

Re: Electrolytic Ni/Au issue

Brian Ellis

Mon, 20 Nov 2006 11:02:05 +0200

77 lines

New Thread

ENIG Risks

ENIG Risks

Robert Lazzara

Thu, 30 Nov 2006 15:47:20 -0600

49 lines

New Thread

ENIG roughness

ENIG roughness

Vladimir Igoshev

Wed, 29 Nov 2006 15:25:11 -0500

35 lines

Re: ENIG roughness

Werner Engelmaier

Wed, 29 Nov 2006 15:55:38 EST

26 lines

Re: ENIG roughness

Vladimir Igoshev

Wed, 29 Nov 2006 15:58:26 -0500

48 lines

Re: ENIG roughness

George Milad

Wed, 29 Nov 2006 18:58:51 EST

45 lines

Re: ENIG roughness

John Burke

Wed, 29 Nov 2006 16:25:03 -0800

81 lines

Re: ENIG roughness

Dennis Fritz

Wed, 29 Nov 2006 21:53:44 EST

31 lines

Re: ENIG roughness

Anil Kher

Thu, 30 Nov 2006 12:11:11 +0530

63 lines

New Thread

EU not busting for RoHS violations yet

EU not busting for RoHS violations yet

John Burke

Thu, 2 Nov 2006 09:55:38 -0800

38 lines

EU not busting for RoHS violations yet

John Burke

Thu, 2 Nov 2006 09:55:38 -0800

57 lines

Re: EU Not Busting for RoHS Violations Yet

Stadem, Richard D.

Thu, 16 Nov 2006 07:34:00 -0600

65 lines

New Thread

Flip Chip Assembly

Flip Chip Assembly

Steve Kelly

Thu, 9 Nov 2006 15:41:10 -0500

41 lines

New Thread

For The Ladies

FW: For The Ladies

Whittaker, Dewey (EHCOE)

Thu, 16 Nov 2006 07:41:49 -0700

152 lines

New Thread

Friday quote - NTC

Friday quote - NTC

Joe Fjelstad

Fri, 10 Nov 2006 13:42:16 EST

24 lines

Re: Friday quote - NTC

Whittaker, Dewey (EHCOE)

Mon, 13 Nov 2006 07:19:28 -0700

53 lines

Re: Friday quote - NTC

Brian Ellis

Mon, 13 Nov 2006 20:05:37 +0200

42 lines

New Thread

Gold Embrittlement

Gold Embrittlement

Kane, Amol (349)

Thu, 2 Nov 2006 12:42:09 -0500

46 lines

Re: Gold Embrittlement

Joyce Koo

Thu, 2 Nov 2006 12:49:35 -0500

72 lines

Re: Gold Embrittlement

Richard Kraszewski

Thu, 2 Nov 2006 12:00:20 -0600

113 lines

Re: Gold Embrittlement

Graham Collins

Thu, 2 Nov 2006 13:03:04 -0500

94 lines

Re: Gold Embrittlement

Dehoyos, Ramon

Thu, 2 Nov 2006 13:40:10 -0500

139 lines

Re: Gold Embrittlement

Kane, Joseph E (US SSA)

Thu, 2 Nov 2006 13:38:53 -0500

128 lines

Re: Gold Embrittlement

Kane, Joseph E (US SSA)

Thu, 2 Nov 2006 13:38:53 -0500

148 lines

Re: Gold Embrittlement

Graham Collins

Thu, 2 Nov 2006 13:03:04 -0500

115 lines

Re: Gold Embrittlement

Joyce Koo

Thu, 2 Nov 2006 12:49:35 -0500

91 lines

Re: Gold Embrittlement

Werner Engelmaier

Thu, 2 Nov 2006 17:06:11 EST

32 lines

Re: Gold Embrittlement

Wayne Thayer

Thu, 2 Nov 2006 17:23:12 -0500

63 lines

Re: Gold Embrittlement

Werner Engelmaier

Thu, 2 Nov 2006 17:30:15 EST

24 lines

Re: Gold Embrittlement

Whittaker, Dewey (EHCOE)

Fri, 3 Nov 2006 06:49:11 -0700

70 lines

Re: Gold Embrittlement

Kane, Amol (349)

Fri, 3 Nov 2006 09:45:55 -0500

124 lines

Re: Gold Embrittlement

Joyce Koo

Fri, 3 Nov 2006 10:02:21 -0500

151 lines

Re: Gold Embrittlement

Werner Engelmaier

Fri, 3 Nov 2006 14:20:43 EST

29 lines

Re: Gold Embrittlement

Werner Engelmaier

Fri, 3 Nov 2006 14:47:21 EST

24 lines

Re: Gold Embrittlement

Joyce Koo

Fri, 3 Nov 2006 10:02:21 -0500

170 lines

Re: Gold Embrittlement

Ingemar Hernefjord (KC/EMW)

Mon, 6 Nov 2006 09:59:50 +0100

70 lines

Re: Gold Embrittlement

Dehoyos, Ramon

Mon, 6 Nov 2006 08:13:44 -0500

101 lines

Re: Gold Embrittlement

Guy Ramsey

Mon, 6 Nov 2006 08:31:25 -0500

123 lines

Re: Gold Embrittlement

Steve Gregory

Mon, 6 Nov 2006 07:34:56 -0600

122 lines

Re: Gold Embrittlement

Wenger, George M.

Mon, 6 Nov 2006 08:52:37 -0500

168 lines

Re: Gold Embrittlement

Steve Gregory

Mon, 6 Nov 2006 09:45:52 -0600

182 lines

Re: Gold Embrittlement

Joe Fjelstad

Mon, 6 Nov 2006 11:49:31 EST

36 lines

Re: Gold Embrittlement

Ian Hanna

Mon, 6 Nov 2006 12:06:47 -0500

63 lines

Re: Gold Embrittlement

Stadem, Richard D.

Mon, 6 Nov 2006 11:04:07 -0600

73 lines

Re: Gold Embrittlement

Colin McVean

Mon, 6 Nov 2006 17:17:36 -0000

116 lines

Re: Gold Embrittlement

Dehoyos, Ramon

Mon, 6 Nov 2006 12:54:09 -0500

146 lines

Re: Gold Embrittlement

John Burke

Mon, 6 Nov 2006 11:33:24 -0800

91 lines

Re: Gold Embrittlement

JaMi Smith

Tue, 7 Nov 2006 12:27:15 -0800

170 lines

Re: Gold Embrittlement

Werner Engelmaier

Tue, 7 Nov 2006 15:44:33 EST

32 lines

Re: Gold Embrittlement

JaMi Smith

Tue, 7 Nov 2006 13:30:31 -0800

96 lines

Re: Gold Embrittlement

Whittaker, Dewey (EHCOE)

Tue, 7 Nov 2006 15:11:34 -0700

143 lines

Re: Gold Embrittlement

Hfjord

Tue, 7 Nov 2006 23:39:02 +0100

248 lines

Re: Gold Embrittlement

JaMi Smith

Tue, 7 Nov 2006 15:44:50 -0800

325 lines

Re: Gold Embrittlement

Werner Engelmaier

Tue, 7 Nov 2006 19:40:34 EST

75 lines

Re: Gold Embrittlement

Stadem, Richard D.

Wed, 8 Nov 2006 07:35:57 -0600

373 lines

Re: Gold Embrittlement

Jack Olson

Thu, 9 Nov 2006 11:32:49 -0600

64 lines

Re: Gold Embrittlement

Stadem, Richard D.

Thu, 9 Nov 2006 11:45:24 -0600

88 lines

Re: Gold Embrittlement

JaMi Smith

Thu, 9 Nov 2006 12:23:10 -0800

392 lines

Re: Gold Embrittlement

Jack Olson

Thu, 9 Nov 2006 20:17:47 -0600

68 lines

New Thread

Happy Thanksgiving

Happy Thanksgiving

Phillip Bavaro

Wed, 22 Nov 2006 12:52:55 -0800

28 lines

Re: Happy Thanksgiving

Alcorn, Brent

Wed, 22 Nov 2006 16:04:48 -0500

53 lines

New Thread

Hard Gold Electro-Damage

Hard Gold Electro-Damage

Jack Olson

Mon, 13 Nov 2006 15:12:03 -0600

39 lines

New Thread

Henry Rekers is out of the office.

Henry Rekers is out of the office.

No Name

Sun, 12 Nov 2006 04:00:30 -0800

23 lines

New Thread

IPC China RoHS Webcast you can'ts miss!

IPC China RoHS Webcast you can'ts miss!

Tina Nerad

Wed, 1 Nov 2006 10:14:33 -0600

49 lines

New Thread

IPC Workshops: Design for Manufacture & Compliant Electronics for EU Applications - Fredericksburg, VA

IPC Workshops: Design for Manufacture & Compliant Electronics for EU Applications - Fredericksburg, VA

Tina Nerad

Mon, 13 Nov 2006 09:57:12 -0600

65 lines

New Thread

IPC's Design for Excellence - Staying Current with Technology

IPC's Design for Excellence - Staying Current with Technology

Tina Nerad

Fri, 3 Nov 2006 15:24:51 -0600

60 lines

IPC's Design for Excellence - Staying Current with Technology

Tina Nerad

Tue, 28 Nov 2006 08:53:58 -0600

53 lines

New Thread

IPC's Design for Excellence webcast series and Exploring the Challenges workshop

IPC's Design for Excellence webcast series and Exploring the Challenges workshop

Tina Nerad

Fri, 10 Nov 2006 10:43:36 -0600

64 lines

New Thread

IPC's Design for Manufacture/Compliant Electronics for EU Applications - December 4-6, 2006 in Fredericksburg, VA

IPC's Design for Manufacture/Compliant Electronics for EU Applications - December 4-6, 2006 in Fredericksburg, VA

Tina Nerad

Mon, 20 Nov 2006 11:42:39 -0600

84 lines

New Thread

IPC/JEDEC Conference in Boston you won't want to miss!

IPC/JEDEC Conference in Boston you won't want to miss!

Tina Nerad

Thu, 2 Nov 2006 09:35:31 -0600

37 lines

New Thread

IPC/JEDEC International Conference on LF Components & Assemblies in Boston, MA

IPC/JEDEC International Conference on LF Components & Assemblies in Boston, MA

Tina Nerad

Wed, 29 Nov 2006 09:36:35 -0600

59 lines

New Thread

IPC/JEDEC International Conference on LF Electronic Components & Assemblies "RoHS & Beyond" in Boston, MA

IPC/JEDEC International Conference on LF Electronic Components & Assemblies "RoHS & Beyond" in Boston, MA

Tina Nerad

Tue, 21 Nov 2006 11:24:09 -0600

64 lines

New Thread

IPC/JEDEC International Conference on LF Electronic Components & Assemblies - December 5-7, 2006, in Boston

IPC/JEDEC International Conference on LF Electronic Components & Assemblies - December 5-7, 2006, in Boston

Tina Nerad

Tue, 14 Nov 2006 11:25:09 -0600

43 lines

New Thread

IPC4101B/126 7 129

IPC4101B/126 7 129

Geoff Layhe of Lamar Group

Thu, 30 Nov 2006 13:49:13 -0000

40 lines

Re: IPC4101B/126 7 129

Donald Kyle

Thu, 30 Nov 2006 08:29:31 -0600

83 lines

Re: IPC4101B/126 7 129

Whittaker, Dewey (EHCOE)

Thu, 30 Nov 2006 07:41:16 -0700

117 lines

Re: IPC4101B/126 7 129

valerie St. Cyr

Thu, 30 Nov 2006 09:58:43 -0500

157 lines

New Thread

Japan Reaches out

Japan Reaches out

John Burke

Thu, 2 Nov 2006 15:58:43 -0800

39 lines

New Thread

Lead Spacing

Lead Spacing

Kane, Joseph E (US SSA)

Wed, 15 Nov 2006 12:20:24 -0500

42 lines

New Thread

Looking for fab shop 4-6 oz copper capability

Looking for fab shop 4-6 oz copper capability

Dee Stover

Fri, 3 Nov 2006 09:39:15 -0700

33 lines

Re: Looking for fab shop 4-6 oz copper capability

Sauer, Steve (Xetron)

Fri, 3 Nov 2006 11:54:49 -0500

60 lines

Re: Looking for fab shop 4-6 oz copper capability

Sauer, Steve (Xetron)

Fri, 3 Nov 2006 11:54:49 -0500

80 lines

Re: Looking for fab shop 4-6 oz copper capability

Sauer, Steve (Xetron)

Fri, 3 Nov 2006 11:54:49 -0500

79 lines

New Thread

Manufacturing with Electroplated Gold PCB in LF applications

Manufacturing with Electroplated Gold PCB in LF applications

Rajesh Dhoum

Fri, 3 Nov 2006 12:56:35 -0500

38 lines

Re: Manufacturing with Electroplated Gold PCB in LF applications

Werner Engelmaier

Fri, 3 Nov 2006 15:06:17 EST

27 lines

Manufacturing with Electroplated Gold PCB in LF applications

Rajesh Dhoum

Fri, 3 Nov 2006 12:56:35 -0500

59 lines

New Thread

masking question

masking question

Gloria Brown

Thu, 9 Nov 2006 13:34:19 -0600

53 lines

Re: masking question

Barmuta, Michael

Thu, 9 Nov 2006 13:25:23 -0800

121 lines

New Thread

More delam

More delam

pearl petras

Mon, 27 Nov 2006 11:02:33 -0500

42 lines

Re: More delam

stephengregory5849

Mon, 27 Nov 2006 11:23:49 -0600

84 lines

Re: More delam

stephengregory5849

Tue, 28 Nov 2006 09:56:05 -0600

97 lines

Re: More delam

pearl petras

Tue, 28 Nov 2006 11:11:43 -0500

92 lines

Re: More delam

Ian Hanna

Tue, 28 Nov 2006 11:36:22 -0500

133 lines

Re: More delam

Susan Mansilla

Tue, 28 Nov 2006 11:46:18 EST

28 lines

Re: More delam

pearl petras

Tue, 28 Nov 2006 11:58:59 -0500

33 lines

Re: More delam

Ian Hanna

Tue, 28 Nov 2006 12:07:57 -0500

72 lines

Re: More delam

<>

Tue, 28 Nov 2006 12:13:47 EST

81 lines

Re: More delam

pearl petras

Tue, 28 Nov 2006 12:17:17 -0500

35 lines

Re: More delam

Jeffrey Bush

Tue, 28 Nov 2006 12:03:58 -0500

70 lines

Re: More delam

Dan Skweres

Tue, 28 Nov 2006 15:30:36 -0600

122 lines

Re: More delam

Gloria Brown

Tue, 28 Nov 2006 15:43:53 -0600

180 lines

Re: More delam

Gloria Brown

Tue, 28 Nov 2006 16:11:25 -0600

173 lines

Re: More delam

Dan Skweres

Tue, 28 Nov 2006 16:25:34 -0600

168 lines

Re: More delam

Genny Gibbard

Tue, 28 Nov 2006 16:28:19 -0600

188 lines

Re: More delam

Alistair Murray

Wed, 29 Nov 2006 14:39:25 -0000

89 lines

Re: More delam

stephen gregory

Wed, 29 Nov 2006 10:43:41 -0800

33 lines

Re: More delam

pearl petras

Thu, 30 Nov 2006 10:07:45 -0500

72 lines

Re: More delam

Ian Hanna

Thu, 30 Nov 2006 10:16:29 -0500

118 lines

Re: More delam

Randy Bock Sr.

Thu, 30 Nov 2006 10:18:40 -0500

142 lines

Re: More delam

Susan Mansilla

Thu, 30 Nov 2006 10:28:02 EST

44 lines

Re: More delam

Jeffrey Bush

Thu, 30 Nov 2006 10:23:35 -0500

122 lines

Re: More delam

Dehoyos, Ramon

Thu, 30 Nov 2006 15:23:09 -0500

79 lines

New Thread

More Separation in BGA joints

Re: More Separation in BGA joints

Werner Engelmaier

Wed, 15 Nov 2006 15:21:57 EST

24 lines

Re: More Separation in BGA joints

Vladimir Igoshev

Wed, 15 Nov 2006 15:35:26 -0500

34 lines

Re: More Separation in BGA joints

Werner Engelmaier

Wed, 15 Nov 2006 15:37:15 EST

26 lines

Re: More Separation in BGA joints

Vladimir Igoshev

Wed, 15 Nov 2006 15:48:08 -0500

22 lines

Re: More Separation in BGA joints

Stadem, Richard D.

Wed, 15 Nov 2006 15:15:34 -0600

58 lines

Re: More Separation in BGA joints

Vladimir Igoshev

Wed, 15 Nov 2006 19:00:15 -0500

64 lines

New Thread

Move Up, Keep Up & Catch Up with the latest IPC workshops in January 2007

Move Up, Keep Up & Catch Up with the latest IPC workshops in January 2007

Tina Nerad

Wed, 22 Nov 2006 08:16:09 -0600

99 lines

New Thread

Need urgent feedback --- Routing of track on component side

Need urgent feedback --- Routing of track on component side

pras chop

Wed, 22 Nov 2006 06:01:47 +0000

55 lines

New Thread

New round of stakeholder consultation for RoHS exemption requests

New round of stakeholder consultation for RoHS exemption requests

John Burke

Thu, 9 Nov 2006 08:46:26 -0800

157 lines

Re: New round of stakeholder consultation for RoHS exemption requests

Bloomquist, Ken

Thu, 9 Nov 2006 10:19:42 -0800

33 lines

Re: New round of stakeholder consultation for RoHS exemption requests

Ian Hanna

Thu, 9 Nov 2006 13:35:16 -0500

59 lines

Re: New round of stakeholder consultation for RoHS exemption requests

Whittaker, Dewey (EHCOE)

Thu, 9 Nov 2006 11:43:39 -0700

88 lines

Re: New round of stakeholder consultation for RoHS exemption requests

John Burke

Thu, 9 Nov 2006 10:46:38 -0800

114 lines

Re: New round of stakeholder consultation for RoHS exemption requests

Ian Hanna

Thu, 9 Nov 2006 13:54:50 -0500

147 lines

Re: New round of stakeholder consultation for RoHS exemption requests

Whittaker, Dewey (EHCOE)

Thu, 9 Nov 2006 12:43:30 -0700

151 lines

Re: New round of stakeholder consultation for RoHS exemption requests

Joe Fjelstad

Thu, 9 Nov 2006 16:49:30 EST

47 lines

New Thread

NTC - George's Friday Clip...

NTC - George's Friday Clip...

Steve Gregory

Fri, 10 Nov 2006 07:00:25 -0600

200 lines

Re: NTC - George's Friday Clip...

Bill Kasprzak

Fri, 10 Nov 2006 08:32:26 -0500

245 lines

New Thread

NTC-APEXPO Promo

NTC-APEXPO Promo

Keach Sasamori

Tue, 21 Nov 2006 14:01:40 -0600

67 lines

New Thread

NTC-Have a Happy Thanksgiving

NTC-Have a Happy Thanksgiving

Stadem, Richard D.

Wed, 22 Nov 2006 09:33:02 -0600

35 lines

Re: NTC-Have a Happy Thanksgiving

Joe Fjelstad

Wed, 22 Nov 2006 12:25:05 EST

50 lines

Re: NTC-Have a Happy Thanksgiving

Bloomquist, Ken

Wed, 22 Nov 2006 09:35:50 -0800

70 lines

New Thread

NTC:is there a audiofil out there?

NTC:is there a audiofil out there?

Inge

Thu, 2 Nov 2006 23:26:05 +0100

36 lines

Re: NTC:is there a audiofil out there?

<>

Mon, 6 Nov 2006 08:57:45 -0500

74 lines

Re: NTC:is there a audiofil out there?

Stadem, Richard D.

Mon, 6 Nov 2006 08:42:54 -0600

95 lines

Re: NTC:is there a audiofil out there?

Matthias Mansfeld

Mon, 6 Nov 2006 16:05:10 +0100

42 lines

Re: NTC:is there a audiofil out there?

Hfjord

Mon, 6 Nov 2006 20:45:29 +0100

124 lines

Re: NTC:is there a audiofil out there?

Hfjord

Mon, 6 Nov 2006 20:56:44 +0100

73 lines

Re: NTC:is there a audiofil out there?

Hfjord

Mon, 6 Nov 2006 20:59:53 +0100

88 lines

Re: NTC:is there a audiofil out there?

Steve Gregory

Mon, 6 Nov 2006 14:48:50 -0600

136 lines

New Thread

Official release of the new exemptions

Official release of the new exemptions

John Burke

Wed, 1 Nov 2006 00:35:25 -0800

74 lines

Re: Official release of the new exemptions

Dehoyos, Ramon

Wed, 1 Nov 2006 09:54:46 -0500

109 lines

Re: Official release of the new exemptions

John Burke

Wed, 1 Nov 2006 06:56:59 -0800

95 lines

Re: Official release of the new exemptions

Joyce Koo

Wed, 1 Nov 2006 10:36:00 -0500

123 lines

Re: Official release of the new exemptions

Miguel Vallejo

Wed, 1 Nov 2006 07:53:16 -0800

105 lines

Re: Official release of the new exemptions

Tempea, Ioan

Wed, 1 Nov 2006 11:22:49 -0500

150 lines

New Thread

One solder Ball Not Connected on a No Connect Pad After Rework

One solder Ball Not Connected on a No Connect Pad After Rework

bob wettermann

Fri, 17 Nov 2006 07:10:58 -0800

37 lines

Re: One solder Ball Not Connected on a No Connect Pad After Rework

Stadem, Richard D.

Fri, 17 Nov 2006 09:17:04 -0600

75 lines

Re: One solder Ball Not Connected on a No Connect Pad After Rework

Gabriela Bogdan

Fri, 17 Nov 2006 18:55:49 +0300

74 lines

Re: One solder Ball Not Connected on a No Connect Pad After Rework

Vladimir Igoshev

Fri, 17 Nov 2006 11:06:28 -0500

123 lines

Re: One solder Ball Not Connected on a No Connect Pad After Rework

Gabriela Bogdan

Fri, 17 Nov 2006 19:39:07 +0300

150 lines

Re: One solder Ball Not Connected on a No Connect Pad After Rework

Vladimir Igoshev

Fri, 17 Nov 2006 11:57:01 -0500

113 lines

Re: One solder Ball Not Connected on a No Connect Pad After Rework

bob wettermann

Fri, 17 Nov 2006 09:37:06 -0800

103 lines

Re: One solder Ball Not Connected on a No Connect Pad After Rework

Vladimir Igoshev

Fri, 17 Nov 2006 12:50:56 -0500

94 lines

Re: One solder Ball Not Connected on a No Connect Pad After Rework

Wayne Thayer

Fri, 17 Nov 2006 13:26:03 -0500

172 lines

Re: One solder Ball Not Connected on a No Connect Pad After Rework

Guy Ramsey

Fri, 17 Nov 2006 15:29:20 -0500

95 lines

New Thread

pallatech mls

pallatech mls

Joyce Koo

Mon, 13 Nov 2006 11:53:18 -0500

28 lines

Re: pallatech mls

Creswick, Steven

Mon, 13 Nov 2006 15:28:19 -0500

56 lines

Re: pallatech mls

Gary Ferrari

Mon, 13 Nov 2006 15:35:09 -0500

71 lines

Re: pallatech mls

R Sedlak

Mon, 13 Nov 2006 13:02:27 -0800

74 lines

Re: pallatech mls

Joyce Koo

Mon, 13 Nov 2006 16:53:29 -0500

111 lines

New Thread

Perchlorate Test Lab?

Perchlorate Test Lab?

Richard Kraszewski

Fri, 3 Nov 2006 08:07:01 -0600

35 lines

New Thread

Power Via Capping

Power Via Capping

Kerry McMullen

Fri, 10 Nov 2006 16:10:44 -0500

47 lines

Re: Power Via Capping

Graham Collins

Fri, 10 Nov 2006 19:48:52 -0500

86 lines

Re: Power Via Capping

ZLATKO BIJEDIC

Sat, 11 Nov 2006 05:20:55 -0800

50 lines

Re: Power Via Capping

Stadem, Richard D.

Sat, 11 Nov 2006 07:48:19 -0600

82 lines

Re: Power Via Capping

Gallegos, Luis A.

Mon, 13 Nov 2006 07:20:51 -0600

136 lines

Re: Power Via Capping

Dehoyos, Ramon

Mon, 13 Nov 2006 10:45:19 -0500

149 lines

Re: Power Via Capping

Joyce Koo

Mon, 13 Nov 2006 11:50:26 -0500

172 lines

Re: Power Via Capping

Kerry McMullen

Mon, 13 Nov 2006 13:08:59 -0500

123 lines

New Thread

Pricing on RoHS lab analysis

Pricing on RoHS lab analysis

John Burke

Mon, 27 Nov 2006 12:27:03 -0800

67 lines

New Thread

PWB mannufacturer Audit

PWB mannufacturer Audit

Dominic Boudreau

Thu, 30 Nov 2006 13:38:43 -0500

36 lines

Re: PWB mannufacturer Audit

Victor G. Hernandez

Thu, 30 Nov 2006 12:53:49 -0600

64 lines

Re: PWB mannufacturer Audit

Werner Engelmaier

Thu, 30 Nov 2006 13:58:40 EST

44 lines

Re: PWB mannufacturer Audit

Jeffrey Bush

Thu, 30 Nov 2006 14:37:18 -0500

67 lines

Re: PWB mannufacturer Audit

Stadem, Richard D.

Thu, 30 Nov 2006 14:59:04 -0600

70 lines

New Thread

PWB/PCB raw card stamping

PWB/PCB raw card stamping

Victor G. Hernandez

Mon, 27 Nov 2006 11:13:56 -0600

34 lines

Re: PWB/PCB raw card stamping

Wayne Thayer

Mon, 27 Nov 2006 13:05:18 -0500

77 lines

New Thread

Question about J-STD-001 cleanliness designator C-22

Question about J-STD-001 cleanliness designator C-22

Joel Alexander

Thu, 30 Nov 2006 11:46:47 -0500

35 lines

Re: Question about J-STD-001 cleanliness designator C-22

Joyce Koo

Thu, 30 Nov 2006 12:55:57 -0500

66 lines

Re: Question about J-STD-001 cleanliness designator C-22

Kevin Glidden

Thu, 30 Nov 2006 13:23:24 -0500

68 lines

Re: Question about J-STD-001 cleanliness designator C-22

Bloomquist, Ken

Thu, 30 Nov 2006 12:44:32 -0800

33 lines

Re: Question about J-STD-001 cleanliness designator C-22

Kevin Glidden

Thu, 30 Nov 2006 15:55:30 -0500

68 lines

Re: Question about J-STD-001 cleanliness designator C-22

Bloomquist, Ken

Thu, 30 Nov 2006 13:58:16 -0800

70 lines

New Thread

Question for Mr Yoda

Re: Question for Mr Yoda

Ed Popielarski

Wed, 1 Nov 2006 07:55:19 -0800

147 lines

New Thread

Request for Weave Exposure / Texture Photographs

Request for Weave Exposure / Texture Photographs

Wee Mei

Tue, 28 Nov 2006 16:04:20 +0800

28 lines

New Thread

Request from another forum

Request from another forum

John Burke

Tue, 21 Nov 2006 09:37:45 -0800

68 lines

New Thread

Rework Requires Approval & Vehement Tech

Rework Requires Approval & Vehement Tech

Kevin Glidden

Wed, 22 Nov 2006 13:48:05 -0500

39 lines

Re: Rework Requires Approval & Vehement Tech

Crepeau, Phil (Space Technology)

Wed, 22 Nov 2006 11:50:42 -0800

68 lines

Re: Rework Requires Approval & Vehement Tech

Crepeau, Phil (Space Technology)

Wed, 22 Nov 2006 11:52:44 -0800

68 lines

Re: Rework Requires Approval & Vehement Tech

Kane, Joseph E (US SSA)

Wed, 22 Nov 2006 15:04:29 -0500

87 lines

Re: Rework Requires Approval & Vehement Tech

Crepeau, Phil (Space Technology)

Wed, 22 Nov 2006 12:34:39 -0800

107 lines

Re: Rework Requires Approval & Vehement Tech

- Bogert

Thu, 23 Nov 2006 14:14:47 -0500

97 lines

New Thread

RoHS and Aerospace

RoHS and Aerospace

Bloomquist, Ken

Tue, 21 Nov 2006 06:09:39 -0800

33 lines

Re: RoHS and Aerospace

Stadem, Richard D.

Tue, 21 Nov 2006 08:48:24 -0600

56 lines

Re: RoHS and Aerospace

Edwin Louis

Tue, 21 Nov 2006 10:24:08 -0500

74 lines

Re: RoHS and Aerospace

Kevin Glidden

Tue, 21 Nov 2006 11:24:24 -0500

63 lines

Re: RoHS and Aerospace

Crepeau, Phil (Space Technology)

Tue, 21 Nov 2006 09:03:14 -0800

86 lines

Re: RoHS and Aerospace

Fox, Ian

Tue, 21 Nov 2006 18:28:14 -0000

63 lines

New Thread

Rohus version

Rohus version

Bill Dworak

Tue, 21 Nov 2006 08:31:17 -0800

47 lines

Re: Rohus version

Geoff Layhe of Lamar Group

Tue, 21 Nov 2006 17:10:32 -0000

85 lines

Re: Rohus version

John Burke

Tue, 21 Nov 2006 09:56:59 -0800

119 lines

New Thread

routing of track on component side in between the pads

routing of track on component side in between the pads

pras chop

Tue, 21 Nov 2006 05:56:11 +0000

39 lines

Re: routing of track on component side in between the pads

Wayne Thayer

Tue, 21 Nov 2006 08:08:36 -0500

82 lines

Re: routing of track on component side in between the pads

pras chop

Thu, 23 Nov 2006 13:26:00 +0000

116 lines

New Thread

Separation in BGA joints

Separation in BGA joints

Tempea, Ioan

Wed, 15 Nov 2006 09:56:31 -0500

42 lines

Re: Separation in BGA joints

Tempea, Ioan

Wed, 15 Nov 2006 10:57:38 -0500

85 lines

Re: Separation in BGA joints

Victor G. Hernandez

Wed, 15 Nov 2006 10:09:36 -0600

117 lines

Re: Separation in BGA joints

Tempea, Ioan

Wed, 15 Nov 2006 11:36:12 -0500

137 lines

Re: Separation in BGA joints

Paul Edwards

Wed, 15 Nov 2006 09:07:34 -0800

95 lines

Re: Separation in BGA joints

Werner Engelmaier

Wed, 15 Nov 2006 13:47:57 EST

28 lines

Re: Separation in BGA joints

Werner Engelmaier

Wed, 15 Nov 2006 14:02:42 EST

42 lines

Re: Separation in BGA joints

Victor G. Hernandez

Wed, 15 Nov 2006 13:17:31 -0600

282 lines

Re: Separation in BGA joints

Vladimir Igoshev

Wed, 15 Nov 2006 14:11:45 -0500

84 lines

Re: Separation in BGA joints

Werner Engelmaier

Wed, 15 Nov 2006 15:20:53 EST

27 lines

Re: Separation in BGA joints

Vladimir Igoshev

Wed, 15 Nov 2006 15:31:04 -0500

19 lines

Re: Separation in BGA joints

Reuven Rokah

Wed, 15 Nov 2006 22:36:24 +0200

55 lines

Re: Separation in BGA joints

<>

Wed, 15 Nov 2006 16:03:10 -0500

64 lines

Re: Separation in BGA joints

P. Langeveld

Wed, 15 Nov 2006 22:17:23 +0100

64 lines

Re: Separation in BGA joints

Victor G. Hernandez

Thu, 16 Nov 2006 06:40:58 -0600

56 lines

Re: Separation in BGA joints

Steve Gregory

Thu, 16 Nov 2006 06:44:36 -0600

79 lines

Separation in BGA joints

Tempea, Ioan

Thu, 16 Nov 2006 09:12:18 -0500

50 lines

Re: Separation in BGA joints

Werner Engelmaier

Thu, 16 Nov 2006 09:57:29 EST

26 lines

Re: Separation in BGA joints

Victor G. Hernandez

Thu, 16 Nov 2006 10:00:32 -0600

85 lines

Re: Separation in BGA joints

Gabriela Bogdan

Thu, 16 Nov 2006 19:04:03 +0300

56 lines

Re: Separation in BGA joints

Steve Gregory

Thu, 16 Nov 2006 10:12:34 -0600

110 lines

Re: Separation in BGA joints

Wenger, George M.

Thu, 16 Nov 2006 11:18:03 -0500

74 lines

Re: Separation in BGA joints

Werner Engelmaier

Thu, 16 Nov 2006 11:29:22 EST

100 lines

Re: Separation in BGA joints

Vladimir Igoshev

Thu, 16 Nov 2006 11:29:16 -0500

141 lines

Re: Separation in BGA joints

Vladimir Igoshev

Thu, 16 Nov 2006 11:45:00 -0500

153 lines

Re: Separation in BGA joints

P. Langeveld

Thu, 16 Nov 2006 17:51:58 +0100

122 lines

Re: Separation in BGA joints

Tempea, Ioan

Thu, 16 Nov 2006 12:09:57 -0500

99 lines

Re: Separation in BGA joints

Gabriela Bogdan

Thu, 16 Nov 2006 22:08:36 +0300

130 lines

Re: Separation in BGA joints

Werner Engelmaier

Thu, 16 Nov 2006 14:51:57 EST

32 lines

Re: Separation in BGA joints

Gabriela Bogdan

Thu, 16 Nov 2006 22:56:19 +0300

65 lines

New Thread

Service Request 10567441: BGA

FW: Service Request 10567441: BGA

Dehoyos, Ramon

Fri, 10 Nov 2006 11:10:00 -0500

166 lines

Re: FW: Service Request 10567441: BGA

Steve Gregory

Fri, 10 Nov 2006 11:22:28 -0600

200 lines

New Thread

Silver Plating

Silver Plating

Dehoyos, Ramon

Wed, 22 Nov 2006 09:07:32 -0500

59 lines

Re: Silver Plating

Dennis Fritz

Wed, 22 Nov 2006 12:37:14 -0500

89 lines

Re: Silver Plating

Dehoyos, Ramon

Wed, 22 Nov 2006 12:56:46 -0500

122 lines

New Thread

solder projections

solder projections

Gloria Brown

Tue, 14 Nov 2006 14:06:54 -0600

45 lines

Re: solder projections

Dehoyos, Ramon

Tue, 14 Nov 2006 15:29:29 -0500

71 lines

Re: solder projections

P. Langeveld

Tue, 14 Nov 2006 23:04:08 +0100

70 lines

New Thread

Solder Voids in Hole barrel after W/S

Solder Voids in Hole barrel after W/S

Irving Lee

Fri, 1 Dec 2006 00:31:23 +0800

33 lines

Re: Solder Voids in Hole barrel after W/S

Miguel Vallejo

Thu, 30 Nov 2006 08:30:06 -0800

58 lines

Re: Solder Voids in Hole barrel after W/S

Miguel Vallejo

Thu, 30 Nov 2006 09:08:00 -0800

62 lines

New Thread

Soldering Anomaly

Soldering Anomaly

Diamond, Pat

Mon, 27 Nov 2006 08:12:38 -0000

64 lines

Re: Soldering Anomaly

stephengregory5849

Mon, 27 Nov 2006 11:23:23 -0600

111 lines

Re: Soldering Anomaly

Wayne Thayer

Mon, 27 Nov 2006 12:56:36 -0500

164 lines

Re: Soldering Anomaly

John Burke

Mon, 27 Nov 2006 10:54:59 -0800

142 lines

Re: Soldering Anomaly

Stadem, Richard D.

Mon, 27 Nov 2006 13:25:46 -0600

138 lines

Re: Soldering Anomaly

Roger Mack

Mon, 27 Nov 2006 14:24:38 -0600

165 lines

Re: Soldering Anomaly

Werner Engelmaier

Mon, 27 Nov 2006 17:13:01 EST

26 lines

Re: Soldering Anomaly

Diamond, Pat

Tue, 28 Nov 2006 08:09:58 -0000

194 lines

Re: Soldering Anomaly

Dehoyos, Ramon

Tue, 28 Nov 2006 09:26:44 -0500

231 lines

New Thread

Stacking chip capacitors

Stacking chip capacitors

Kevin Glidden

Fri, 3 Nov 2006 11:16:40 -0500

31 lines

Re: Stacking chip capacitors

Dehoyos, Ramon

Fri, 3 Nov 2006 12:52:43 -0500

94 lines

Stacking chip capacitors

Kevin Glidden

Fri, 3 Nov 2006 11:16:40 -0500

52 lines

Stacking chip capacitors

Kevin Glidden

Fri, 3 Nov 2006 11:16:40 -0500

51 lines

Re: Stacking chip capacitors

Hfjord

Tue, 7 Nov 2006 22:50:42 +0100

66 lines

New Thread

Stencils

Stencils

Tom Parkinson

Thu, 30 Nov 2006 12:22:47 -0500

34 lines

Re: Stencils

Kathy Jenczewski

Thu, 30 Nov 2006 12:38:42 -0500

62 lines

Re: Stencils

Miguel Vallejo

Thu, 30 Nov 2006 09:35:13 -0800

59 lines

Re: Stencils

Stadem, Richard D.

Thu, 30 Nov 2006 13:44:23 -0600

106 lines

Re: Stencils

Bloomquist, Ken

Thu, 30 Nov 2006 11:58:14 -0800

55 lines

New Thread

Strong demand to keep tin prices high - article link

Strong demand to keep tin prices high - article link

John Burke

Mon, 13 Nov 2006 09:05:22 -0800

41 lines

Re: Strong demand to keep tin prices high - article link

James Verrette

Tue, 14 Nov 2006 09:40:31 -0500

63 lines

New Thread

Terry L Huddleston/ElecTec/Teledyne is out of the office.

Terry L Huddleston/ElecTec/Teledyne is out of the office.

Terry Huddleston

Wed, 8 Nov 2006 11:17:27 -0800

13 lines

New Thread

Tin - Lead Solder / Gold connector interface

Tin - Lead Solder / Gold connector interface

Kevin Glidden

Mon, 20 Nov 2006 10:34:24 -0500

35 lines

Re: Tin - Lead Solder / Gold connector interface

Ahne Oosterhof

Mon, 20 Nov 2006 14:44:32 -0800

68 lines

New Thread

TMA recommendation

TMA recommendation

valerie St. Cyr

Thu, 16 Nov 2006 14:56:52 -0500

38 lines

Re: TMA recommendation

Werner Engelmaier

Thu, 16 Nov 2006 15:16:33 EST

51 lines

Re: TMA recommendation

Richard Kraszewski

Thu, 16 Nov 2006 14:28:17 -0600

87 lines

Re: TMA recommendation

Gerald Gagnon

Thu, 16 Nov 2006 16:27:35 -0500

94 lines

Re: TMA recommendation

Joyce Koo

Thu, 16 Nov 2006 16:37:04 -0500

76 lines

Re: TMA recommendation

valerie St. Cyr

Thu, 16 Nov 2006 17:39:06 -0500

48 lines

Re: TMA recommendation

valerie St. Cyr

Thu, 16 Nov 2006 17:51:03 -0500

138 lines

Re: TMA recommendation

valerie St. Cyr

Fri, 17 Nov 2006 10:59:59 -0500

49 lines

Re: TMA recommendation

Dennis Fritz

Fri, 17 Nov 2006 14:53:55 EST

52 lines

New Thread

Ultimate PCB assembly books

Ultimate PCB assembly books

Tempea, Ioan

Mon, 27 Nov 2006 15:15:01 -0500

36 lines

Re: Ultimate PCB assembly books

Christopher Nash

Mon, 27 Nov 2006 15:29:40 -0500

68 lines

Re: Ultimate PCB assembly books

Brian Ellis

Tue, 28 Nov 2006 10:30:42 +0200

57 lines

New Thread

Ultimate PCB assembly books (and more)

Re: Ultimate PCB assembly books (and more)

Gabriela Bogdan

Tue, 28 Nov 2006 21:51:41 +0300

115 lines

Re: Ultimate PCB assembly books (and more)

Vladimir Igoshev

Tue, 28 Nov 2006 14:13:33 -0500

186 lines

Re: Ultimate PCB assembly books (and more)

Werner Engelmaier

Tue, 28 Nov 2006 14:20:34 EST

28 lines

Re: Ultimate PCB assembly books (and more)

Vladimir Igoshev

Tue, 28 Nov 2006 14:30:08 -0500

84 lines

Re: Ultimate PCB assembly books (and more)

Victor G. Hernandez

Tue, 28 Nov 2006 14:09:55 -0600

212 lines

Re: Ultimate PCB assembly books (and more)

Victor G. Hernandez

Tue, 28 Nov 2006 14:14:14 -0600

117 lines

Re: Ultimate PCB assembly books (and more)

Vladimir Igoshev

Tue, 28 Nov 2006 15:30:09 -0500

127 lines

New Thread

UV flourescent pens for rework identification.

UV flourescent pens for rework identification.

Jenny Drake

Wed, 1 Nov 2006 13:36:48 -0000

32 lines

Re: UV flourescent pens for rework identification.

Dehoyos, Ramon

Wed, 1 Nov 2006 15:21:42 -0500

63 lines

Re: UV flourescent pens for rework identification.

Kevin Glidden

Wed, 1 Nov 2006 16:03:38 -0500

91 lines

Re: UV flourescent pens for rework identification.

Jenny Drake

Thu, 2 Nov 2006 08:36:55 -0000

126 lines

Re: UV flourescent pens for rework identification.

Brian Ellis

Thu, 2 Nov 2006 11:01:09 +0200

173 lines

Re: UV flourescent pens for rework identification.

Kevin Glidden

Thu, 2 Nov 2006 08:22:19 -0500

251 lines

FW: UV flourescent pens for rework identification.

Jenny Drake

Fri, 3 Nov 2006 08:25:04 -0000

265 lines

New Thread

Warning to expert witnesses in Houston

Warning to expert witnesses in Houston

Werner Engelmaier

Tue, 7 Nov 2006 11:46:35 EST

25 lines

Re: Warning to expert witnesses in Houston

Eric CHRISTISON

Tue, 7 Nov 2006 16:58:47 +0000

58 lines

Re: Warning to expert witnesses in Houston

Joe Fjelstad

Tue, 7 Nov 2006 12:15:35 EST

29 lines

Re: Warning to expert witnesses in Houston

Stadem, Richard D.

Tue, 7 Nov 2006 11:21:27 -0600

55 lines

Re: Warning to expert witnesses in Houston

Mike Buetow

Tue, 7 Nov 2006 12:23:28 -0500

84 lines

Re: Warning to expert witnesses in Houston

John Burke

Tue, 7 Nov 2006 09:35:41 -0800

56 lines

Re: Warning to expert witnesses in Houston

John Burke

Tue, 7 Nov 2006 09:36:15 -0800

77 lines

Re: Warning to expert witnesses in Houston

Whittaker, Dewey (EHCOE)

Tue, 7 Nov 2006 10:44:46 -0700

58 lines

Re: Warning to expert witnesses in Houston

Olav Folland

Tue, 7 Nov 2006 10:27:06 -0800

76 lines

Re: Warning to expert witnesses in Houston

Neil Maloney

Tue, 7 Nov 2006 12:55:42 -0600

104 lines

Re: Warning to expert witnesses in Houston

Werner Engelmaier

Tue, 7 Nov 2006 14:56:11 EST

25 lines

Re: Warning to expert witnesses in Houston

Steve Gregory

Tue, 7 Nov 2006 14:00:00 -0600

50 lines

Re: Warning to expert witnesses in Houston

Joe Fjelstad

Tue, 7 Nov 2006 15:23:34 EST

29 lines

Re: Warning to expert witnesses in Houston

Werner Engelmaier

Tue, 7 Nov 2006 15:31:34 EST

27 lines

Re: Warning to expert witnesses in Houston

Joe Russeau

Tue, 7 Nov 2006 15:31:34 -0500

61 lines

Re: Warning to expert witnesses in Houston

Werner Engelmaier

Tue, 7 Nov 2006 15:39:00 EST

26 lines

Re: Warning to expert witnesses in Houston

Jerry Dengler

Tue, 7 Nov 2006 15:42:14 -0500

58 lines

Re: Warning to expert witnesses in Houston

Croslin, Robert

Tue, 7 Nov 2006 15:54:17 -0500

56 lines

Re: Warning to expert witnesses in Houston

John Burke

Tue, 7 Nov 2006 13:00:11 -0800

75 lines

Re: Warning to expert witnesses in Houston

Neil Maloney

Tue, 7 Nov 2006 15:25:58 -0600

56 lines

Re: Warning to expert witnesses in Houston

Dale Ritzen

Tue, 7 Nov 2006 15:42:38 -0600

85 lines

Re: Warning to expert witnesses in Houston

Whittaker, Dewey (EHCOE)

Tue, 7 Nov 2006 15:02:53 -0700

210 lines

Re: Warning to expert witnesses in Houston

Wayne Thayer

Tue, 7 Nov 2006 17:37:38 -0500

243 lines

Re: Warning to expert witnesses in Houston

Jeffrey Bush

Tue, 7 Nov 2006 17:02:48 -0500

62 lines

Re: Warning to expert witnesses in Houston

Brian Ellis

Wed, 8 Nov 2006 13:57:53 +0200

53 lines

Re: Warning to expert witnesses in Houston

Tom Stearns

Wed, 8 Nov 2006 07:10:49 -0500

26 lines

Re: Warning to expert witnesses in Houston

JaMi Smith

Thu, 9 Nov 2006 14:46:53 -0800

68 lines

Re: Warning to expert witnesses in Houston

Werner Engelmaier

Thu, 9 Nov 2006 18:44:16 EST

23 lines

Re: Warning to expert witnesses in Houston

Joe Fjelstad

Thu, 9 Nov 2006 19:20:38 EST

28 lines

New Thread

What to do with a 9 pin .5mm BGA?

What to do with a 9 pin .5mm BGA?

Barbara Burcham

Fri, 3 Nov 2006 09:40:47 -0600

40 lines

Re: What to do with a 9 pin .5mm BGA?

Kevin Glidden

Fri, 3 Nov 2006 11:33:43 -0500

80 lines

What to do with a 9 pin .5mm BGA?

Barbara Burcham

Fri, 3 Nov 2006 09:40:47 -0600

60 lines

Re: What to do with a 9 pin .5mm BGA?

Kevin Glidden

Fri, 3 Nov 2006 11:33:43 -0500

100 lines

New Thread

who brought the cat?

Re: who brought the cat?

Hfjord

Tue, 7 Nov 2006 23:09:44 +0100

27 lines

New Thread

Yet Another Warp & Twist Question

Yet Another Warp & Twist Question

Smith, Richard

Tue, 14 Nov 2006 07:32:10 -0500

36 lines

New Thread

[Fwd: Re: [TN] Warning to expert witnesses in Houston]

[Fwd: Re: [TN] Warning to expert witnesses in Houston]

Olav Folland

Tue, 7 Nov 2006 11:01:27 -0800

129 lines

Re: [Fwd: Re: [TN] Warning to expert witnesses in Houston]

Whittaker, Dewey (EHCOE)

Tue, 7 Nov 2006 12:16:48 -0700

173 lines

Re: [Fwd: Re: [TN] Warning to expert witnesses in Houston]

Steve Gregory

Tue, 7 Nov 2006 13:37:53 -0600

205 lines

Re: [Fwd: Re: [TN] Warning to expert witnesses in Houston]

Stadem, Richard D.

Tue, 7 Nov 2006 13:47:23 -0600

204 lines

New Thread

[LF] black pad

Re: [LF] black pad

Gabriela Bogdan

Wed, 29 Nov 2006 21:17:32 +0300

125 lines

Re: [LF] black pad

Vladimir Igoshev

Wed, 29 Nov 2006 14:12:09 -0500

180 lines

New Thread

[LF] China RoHS news

FW: [LF] China RoHS news

John Burke

Mon, 13 Nov 2006 09:42:42 -0800

48 lines

New Thread

[LF] EU Not Busting for RoHS Violations Yet

Re: [LF] EU Not Busting for RoHS Violations Yet

Stadem, Richard D.

Thu, 9 Nov 2006 10:13:56 -0600

189 lines

New Thread

[LF] Gold Embrittlement

Re: [LF] Gold Embrittlement

Kane, Amol (349)

Thu, 2 Nov 2006 15:12:05 -0500

200 lines

Re: [LF] Gold Embrittlement

Joyce Koo

Thu, 2 Nov 2006 15:21:15 -0500

227 lines

Re: [LF] Gold Embrittlement

Steve Gregory

Thu, 2 Nov 2006 14:34:29 -0600

244 lines

Re: [LF] Gold Embrittlement

Steve Gregory

Thu, 2 Nov 2006 14:35:47 -0600

237 lines

Re: [LF] Gold Embrittlement

Kane, Amol (349)

Thu, 2 Nov 2006 16:32:31 -0500

280 lines

Re: [LF] Gold Embrittlement

Joyce Koo

Thu, 2 Nov 2006 16:50:51 -0500

264 lines

Re: [LF] Gold Embrittlement

David D. Hillman

Fri, 3 Nov 2006 08:18:41 -0600

260 lines

New Thread

[LF] Why EU Not Busting for RoHS Violations Yet

Re: [LF] Why EU Not Busting for RoHS Violations Yet

Stadem, Richard D.

Tue, 14 Nov 2006 15:25:59 -0600

165 lines

Re: [LF] Why EU Not Busting for RoHS Violations Yet

Eric CHRISTISON

Wed, 15 Nov 2006 09:46:45 +0000

234 lines

Re: [LF] Why EU Not Busting for RoHS Violations Yet

Dehoyos, Ramon

Wed, 15 Nov 2006 08:15:14 -0500

293 lines

Re: [LF] Why EU Not Busting for RoHS Violations Yet

Stadem, Richard D.

Wed, 15 Nov 2006 07:53:22 -0600

319 lines

Re: [LF] Why EU Not Busting for RoHS Violations Yet

Reuven Rokah

Wed, 15 Nov 2006 16:03:04 +0200

351 lines

Re: [LF] Why EU Not Busting for RoHS Violations Yet

Joe Fjelstad

Wed, 15 Nov 2006 10:10:01 EST

31 lines

Re: [LF] Why EU Not Busting for RoHS Violations Yet

Stadem, Richard D.

Wed, 15 Nov 2006 11:09:29 -0600

56 lines

Re: [LF] Why EU Not Busting for RoHS Violations Yet

Eric CHRISTISON

Wed, 15 Nov 2006 17:23:15 +0000

232 lines

Re: [LF] Why EU Not Busting for RoHS Violations Yet

Stadem, Richard D.

Wed, 15 Nov 2006 12:46:46 -0600

352 lines

Re: [LF] Why EU Not Busting for RoHS Violations Yet

Werner Engelmaier

Wed, 15 Nov 2006 14:11:49 EST

32 lines

New Thread

[MDPP] China Labeling

FW: [MDPP] China Labeling

John Burke

Thu, 16 Nov 2006 22:01:22 -0800

106 lines

New Thread

[TN] China "Complying with RoHS" Friday, November 17, 2006|TÜV Product Service Ltd

RE: [TN] China "Complying with RoHS" Friday, November 17, 2006|TÜV Product Service Ltd

John Burke

Fri, 17 Nov 2006 10:13:16 -0800

76 lines

New Thread

[TN] BGA anomaly

FW: [TN] BGA anomaly

Dehoyos, Ramon

Mon, 20 Nov 2006 14:35:18 -0500

143 lines

Re: FW: [TN] BGA anomaly

Werner Engelmaier

Mon, 20 Nov 2006 15:00:19 EST

31 lines

Re: FW: [TN] BGA anomaly

Dehoyos, Ramon

Wed, 22 Nov 2006 12:19:06 -0500

61 lines

Re: FW: [TN] BGA anomaly

Werner Engelmaier

Wed, 22 Nov 2006 12:38:40 EST

26 lines

Re: FW: [TN] BGA anomaly

Braddock, Iain

Fri, 24 Nov 2006 12:42:53 -0000

79 lines

Re: FW: [TN] BGA anomaly

Wenger, George M.

Fri, 24 Nov 2006 10:49:00 -0500

97 lines

Re: FW: [TN] BGA anomaly

Joe Fjelstad

Fri, 24 Nov 2006 11:06:22 EST

57 lines

Re: FW: [TN] BGA anomaly

Braddock, Iain

Mon, 27 Nov 2006 09:57:11 -0000

171 lines

Re: FW: [TN] BGA anomaly

Dehoyos, Ramon

Mon, 27 Nov 2006 08:47:25 -0500

201 lines

Re: FW: [TN] BGA anomaly

Wenger, George M.

Mon, 27 Nov 2006 09:00:01 -0500

161 lines

Re: FW: [TN] BGA anomaly

Dehoyos, Ramon

Mon, 27 Nov 2006 12:09:07 -0500

287 lines

Re: FW: [TN] BGA anomaly

Wenger, George M.

Mon, 27 Nov 2006 13:06:44 -0500

200 lines

Re: FW: [TN] BGA anomaly

bob wettermann

Mon, 27 Nov 2006 13:18:58 -0800

281 lines

Re: FW: [TN] BGA anomaly

Wenger, George M.

Mon, 27 Nov 2006 21:19:23 -0500

216 lines

Re: FW: [TN] BGA anomaly

Stadem, Richard D.

Tue, 28 Nov 2006 07:06:31 -0600

385 lines

Re: FW: [TN] BGA anomaly

Wenger, George M.

Tue, 28 Nov 2006 08:32:07 -0500

254 lines

Re: FW: [TN] BGA anomaly

Tempea, Ioan

Tue, 28 Nov 2006 09:04:20 -0500

58 lines

Re: FW: [TN] BGA anomaly

Wenger, George M.

Tue, 28 Nov 2006 09:32:20 -0500

68 lines

New Thread

[TN] FW: [MDPP] China Labeling

FW: [TN] FW: [MDPP] China Labeling

Whittaker, Dewey (EHCOE)

Fri, 17 Nov 2006 11:29:34 -0700

145 lines

New Thread

[TN] FW: [MDPP] China Labeling NTC

Re: FW: [TN] FW: [MDPP] China Labeling NTC

Joe Fjelstad

Fri, 17 Nov 2006 13:46:38 EST

163 lines

New Thread

[TN] Solder Voids in Hole barrel  after W/S

Re: [TN] Solder Voids in Hole barrel  after W/S

Werner Engelmaier

Thu, 30 Nov 2006 12:00:04 EST

34 lines

Advanced Options


Options

Log In

Log In

Get Password

Get Password


Search Archives

Search Archives


Subscribe or Unsubscribe

Subscribe or Unsubscribe


Archives

January 2019
December 2018
November 2018
October 2018
September 2018
August 2018
July 2018
June 2018
May 2018
April 2018
March 2018
February 2018
January 2018
December 2017
November 2017
October 2017
September 2017
August 2017
July 2017
June 2017
May 2017
April 2017
March 2017
February 2017
January 2017
December 2016
November 2016
October 2016
September 2016
August 2016
July 2016
June 2016
May 2016
April 2016
March 2016
February 2016
January 2016
December 2015
November 2015
October 2015
September 2015
August 2015
July 2015
June 2015
May 2015
April 2015
March 2015
February 2015
January 2015
December 2014
November 2014
October 2014
September 2014
August 2014
July 2014
June 2014
May 2014
April 2014
March 2014
February 2014
January 2014
December 2013
November 2013
October 2013
September 2013
August 2013
July 2013
June 2013
May 2013
April 2013
March 2013
February 2013
January 2013
December 2012
November 2012
October 2012
September 2012
August 2012
July 2012
June 2012
May 2012
April 2012
March 2012
February 2012
January 2012
December 2011
November 2011
October 2011
September 2011
August 2011
July 2011
June 2011
May 2011
April 2011
March 2011
February 2011
January 2011
December 2010
November 2010
October 2010
September 2010
August 2010
July 2010
June 2010
May 2010
April 2010
March 2010
February 2010
January 2010
December 2009
November 2009
October 2009
September 2009
August 2009
July 2009
June 2009
May 2009
April 2009
March 2009
February 2009
January 2009
December 2008
November 2008
October 2008
September 2008
August 2008
July 2008
June 2008
May 2008
April 2008
March 2008
February 2008
January 2008
December 2007
November 2007
October 2007
September 2007
August 2007
July 2007
June 2007
May 2007
April 2007
March 2007
February 2007
January 2007
December 2006
November 2006
October 2006
September 2006
August 2006
July 2006
June 2006
May 2006
April 2006
March 2006
February 2006
January 2006
December 2005
November 2005
October 2005
September 2005
August 2005
July 2005
June 2005
May 2005
April 2005
March 2005
February 2005
January 2005
December 2004
November 2004
October 2004
September 2004
August 2004
July 2004
June 2004
May 2004
April 2004
March 2004
February 2004
January 2004
December 2003
November 2003
October 2003
September 2003
August 2003
July 2003
June 2003
May 2003
April 2003
March 2003
February 2003
January 2003
December 2002
November 2002
October 2002
September 2002
August 2002
July 2002
June 2002
May 2002
April 2002
March 2002
February 2002
January 2002
December 2001
November 2001
October 2001
September 2001
August 2001
July 2001
June 2001
May 2001
April 2001
March 2001
February 2001
January 2001
December 2000
November 2000
October 2000
September 2000
August 2000
July 2000
June 2000
May 2000
April 2000
March 2000
February 2000
January 2000
December 1999
November 1999
October 1999
September 1999
August 1999
July 1999
June 1999
May 1999
April 1999
March 1999
February 1999
January 1999
December 1998
November 1998
October 1998
September 1998
August 1998
July 1998
June 1998
May 1998
April 1998
March 1998
February 1998
January 1998
December 1997
November 1997
October 1997
September 1997
August 1997
July 1997
June 1997
May 1997
April 1997
March 1997
February 1997
January 1997
1996
1995

ATOM RSS1 RSS2



LISTSERV.IPC.ORG

CataList Email List Search Powered by the LISTSERV Email List Manager