Inge:
15 micrometers thickness is almost 600 mils. About 6 times
the "safe" thickness allowed by J-std-001. Have you seen gold
embrittlement with less than 100 mils, or anyone else? It would be
interesting to know. Comment, there is a lot of waste of gold by
electroplating instead of using Immersion.
Regards,
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ingemar Hernefjord
(KC/EMW)
Sent: Monday, November 06, 2006 4:00 AM
To: [log in to unmask]
Subject: Re: [TN] Gold Embrittlement
Agree,
We degold all microwave SMT small outline transistors ("helicopters"),
because we had catastrophic gold embrittlement problems. The solder
joints were so brittle, that the leads lifted from the pad in the temp
cycle tests. We measured as much as 15 micrometers of gold! The
semiconductor manufacturer meant, that it is a problem to have control
on the gold process on such small parts. What nonsense! Anyway, we are
today suspiscious with many gold plated parts and do degolding rather
than getting embrittlement.
I'll send some pictures to Steve, so you can see what can happen.
Horror!
Inge
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: den 2 november 2006 23:06
To: [log in to unmask]
Subject: Re: [TN] Gold Embrittlement
Hi Amol,
I you have imersion Au, Au-embrittlement is not a problem because there
is not enough Au. Be careful, however, if your PCBs come from China; I
have seen much thicker Au-layers than are possible with iAu.
Calculating the wt% of Au in a soldert joint is an exercise in futility,
because you have to make the assumption--frequently not warranted--that
the SnAu-IMCs are uniformally distributed.
In cases where you suspect thicker Au [and for the matter Ag; which is
equally as bad as Au in causing SJ-embrittlement] deposits, the safest
course of action is to wash the Au (Ag) off by tipping.
Werner
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|