Hi Amol - one other resource that is available for use is located at this
web link:
http://circuitsassembly.com/cms/content/view/3630/95/
The folks at Lockheed Martin (thanks to Tom Glifford and Melissa Lau) have
posted a "gold embrittlement" calculator which is very useful to get a
first order approximation on having a gold embrittlement problem. The
JSTD-001 Handbook also has a good bit of information on the topic. Good
Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
"Kane, Amol
(349)"
<akane@HARVARDGRP To
.COM> [log in to unmask]
Sent by: TechNet cc
<[log in to unmask]>
Subject
Re: [TN] [LF] Gold Embrittlement
11/02/2006 02:12
PM
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
"Kane, Amol
(349)"
<akane@HARVARDGRP
.COM>
Thank you very much to all who answered promptly!...... I think we are okay
based on the thickness spec and the acceptable % vol of Au in the joint.
Regards,
Amol
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Kane, Joseph E (US
SSA)
Sent: Thursday, November 02, 2006 1:31 PM
To: [log in to unmask]
Subject: Re: [LF] Gold Embrittlement
You might not need to do a volumetric calculation, because J-STD-001
has done some of the homework for you. You're not required to remove
gold from through-hole leads if it's less than 2.5 microns thick (in
Rev.
D, Para. 3.9.3). If you can't get information from the supplier, XRF
can
tell you the thickness.
-Joe
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Lester Subrattee
Sent: Thursday, November 02, 2006 1:18 PM
To: [log in to unmask]
Subject: Re: [LF] Gold Embrittlement
The typical number going around industry, as far as percentage of
acceptable
gold in a joint, is about 3 percent.
From your data you can approximate how much gold is in the joint and
thus
determine your safety margin.
However, there are two mechanisms at work regarding the "amount" of gold
in
the joint.
If a good nickel/tin intermetallic joint is formed and you have too much
gold in the joint (let's say beyond the 3 percent) there could be
gold/tin
planar intermetallics within the bulk joint which could result in
shearing
along the intermetallic during impact.
So you keep the gold percentage below 3 to be safe.
Your work is not done.
The other mechanism at work is at the interface where the gold dissolves
into the liquid solder. If the soldering process does not allow for
sufficient dissolution of gold into the bulk solder you could end up
with a
gold rich layer in at the interface. This could result in the brittle
interfacial fractures.
If you address these two, I think you're OK.
Hope it helps,
LS
-----Original Message-----
From: Kane, Amol (349) [mailto:[log in to unmask]]
Sent: Thursday, November 02, 2006 12:42 PM
To: [log in to unmask]
Subject: Gold Embrittlement
Dear Technetters,
One of the connectors that we use in an exempt application just went
lead f=
ree. The surface finish on the connector is gold over nickel. One end of
th=
e connector is soldered to the board by tin lead solder, while the other
en=
d goes into a PTH and is hand soldered, again using tin-lead solder. How
ca=
n I be sure that gold embrittlement will not be an issue for this joint?
Is=
there a minimum % of gold that needs to be present in the solder joint
for=
this to become an issue?
If I know the gold plating thickness, pin dimensions, and the PTH
dimension=
s, can I figure out how much gold % would be in the joint, and hence
object=
ively conclude one way or the other? What other information do I need?
Regards,
Amol
CONFIDENTIALITY NOTICE:=20
This e-mail, and any attachments, is for the sole use of the intended=20
recipient(s) and may contain information that is confidential and=20
protected from disclosure under the law. Any unauthorized review,
use,=20
disclosure, or distribution is prohibited. If you are not the
intended=20
recipient, please contact the sender by reply e-mail, and
delete/destroy=20
all copies of the original message and attachments.=20
Thank you.
------------------------------------------------------------------------
----
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=3D4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
------------------------------------------------------------------------
----
---
THIS EMAIL AND ANY ATTACHED FILES ARE CONFIDENTIAL AND MAY BE LEGALLY
PRIVILEGED. If you are not the addressee, any disclosure, reproduction,
copying, distribution or other dissemination or use of this
communication is
strictly prohibited. If you have received this transmission in error,
please
notify the sender immediately and delete this email. It is the policy of
ACR
Electronics, Inc. that no legally binding statements, representations or
commitments (collectively statements) may be made by email. Any such
statements must be confirmed either by facsimile transmission or by
postal
mail before they will have legal effect. The sender of this email is not
authorised to commit the company in any way and the addressee is hereby
notified of that fact.
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
-------------------------------------------------------------------------------Leadfee
Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-------------------------------------------------------------------------------
CONFIDENTIALITY NOTICE:
This e-mail, and any attachments, is for the sole use of the intended
recipient(s) and may contain information that is confidential and
protected from disclosure under the law. Any unauthorized review, use,
disclosure, or distribution is prohibited. If you are not the intended
recipient, please contact the sender by reply e-mail, and delete/destroy
all copies of the original message and attachments.
Thank you.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|