One way is to use a 0.019" ( 19 mils ) drammel tool. It cuts
cleanly and very fast. After cutting a groove 1/4 of the thickness deep
on both side or so, it break off fairly easy. Practice on a scrap board
to develop skills and process.
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Monday, November 06, 2006 2:07 PM
To: [log in to unmask]
Subject: Re: [TN] Delam from separating boards
...and that's exactly where these guidelines come from.
-Steve-
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Monday, November 06, 2006 12:55 PM
To: [log in to unmask]
Subject: Re: [TN] Delam from separating boards
There are also good repair methods for delaminations within IPC
7711/7721.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Monday, November 06, 2006 12:34 PM
To: [log in to unmask]
Subject: Re: [TN] Delam from separating boards
Hi Pearl!
Just how bad is the delamination? What is the end use of these boards?
If the delam goes into traces, that may be problematic, but not the end
of the world. If it's just base board material, that can usually be
repaired fairly easily. It's just a matter of getting some good two-part
epoxy (I use Loctite 0151), and patching everything together.
Here's a link for some good guidelines for base board repair:
http://www.circuitrework.com/guides/3-0.shtml
I feel your pain when it comes to re-scoring boards that haven't been
scored deep enough and have been already built. I've been there and done
that and even got a tee-shirt. It ain't no fun, but I don't have to tell
you that. Sometimes you have to do what you gotta do.
I found that when you have to go back and make the score deeper with an
exacto knife, patience is key. You have to understand that it's going to
take some time. You need to go over the existing score, scores and
scores of times (pun intended). It's better to go over the score with
your knife many times lightly, rather than trying to make deep cuts,
because it's then when your knife comes out of the score line and goes
into nearby traces. You also need to go over the score from both sides
of the board, not just one side.
Good luck!
-Steve Gregory-
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of pearl petras
Sent: Monday, November 06, 2006 11:37 AM
To: [log in to unmask]
Subject: [TN] Delam from separating boards
We had some v-scored boards, with components so close to the edge that
we could not use a depanelizer to separate them. (I know, I know, root
cause - no DFM)
On top of that, the V-score done was basically just a lightly etched
line.
Some enterprising people used some exacto blades to try to score them
further, and then just applied brute strength...
I have been told that most delam is non-repairable. Is that so? We
have an extremely high percentage of a build that will need to be
written off, if so.
If not, any thoughts on where to go for tips and tricks on how to
repair?
How do you determine what is repairable and what is not?
Switching away from RoHS to other headaches for a bit...
Thanks in advance.
---------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
The best gets better. See why everyone is raving about the All-new
Yahoo! Mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|