Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Anne Ledger <[log in to unmask]>
Parts/Attachments:
text/plain (94 lines)
Mr. Moon, Mr. Brummer, and all,

It appears that since we did not spec out the construction, our supplier
decided to provide us with the cheapest way, unbeknownst to us.  We are
a small shop without a lot of engineering support.  We typically rely on
our suppliers to steer us in the right direction.  All our lay-ups are
conservative and on the high resin side.  Former purchasing people here
put their trust 100% with the supplier to provide an equally
conservative construction.  It appears that that did not happen.  The
more I know, the more I need to know.  Tough lesson learned.

Thanks for the input.

Anne

> -----Original Message-----
> From: Enter your name here [SMTP:[log in to unmask]]
> Sent: Tuesday, August 17, 1999 7:40 PM
> To:   TechNet E-Mail Forum.; Anne Ledger
> Subject:      Re:      [TN] Innerlayer issue
>
> Are you talking about weave impressions left from low resin to glass
> ratio
> materials? If you are, the answer is get away from using that nasty
> old
> 7628/7629 material facing foil. Go resin rich for no weave impressions
> and
> better innerlaminar bond strength with better resist adherence.
>
> Earl Moon
> ----- Original Message -----
> From: Anne Ledger <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Tuesday, August 17, 1999 5:45 AM
> Subject: [TN] Innerlayer issue
>
>
> > Good Morning Technetters,
> >
> > I have a question for board fabbers.  Problem:  We are experiencing
> > weave texture on our innerlayer material.  I have spoken to the
> > manufacturer who states that weave does shift in the "pour" of the
> > material (when the resin is added) and that there is no
> specification
> > that controls the depth requirement of the weave.  The topography is
> > visual prior to lam/image.  The condition is causing our resist to
> lift
> > slightly and allows an etch stain on the double treat foil that so
> far
> > we can not remove.  Question:  Is this a typical condition of
> innerlayer
> > material (other manufacturers)?  Is it double treat foil only?  Is
> there
> > a way to remove this type of etch stain?  What is the acceptablity
> of
> > stain on inner layer foil?  I can't find any reference info in IPC.
> >
> > Any and all input would be appreciated.
> >
> > Anne Ledger
> > EMDS, Inc.
> >
> > ##############################################################
> > TechNet Mail List provided as a free service by IPC using LISTSERV
> 1.8c
> > ##############################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> > the body:
> > To subscribe:   SUBSCRIBE TECHNET <your full name>
> > To unsubscribe:   SIGNOFF TECHNET
> > ##############################################################
> > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> > information.
> > If you need assistance - contact Gayatri Sardeshpande at
> [log in to unmask] or
> > 847-509-9700 ext.5365
> > ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2