Are you talking about weave impressions left from low resin to glass ratio
materials? If you are, the answer is get away from using that nasty old
7628/7629 material facing foil. Go resin rich for no weave impressions and
better innerlaminar bond strength with better resist adherence.
Earl Moon
----- Original Message -----
From: Anne Ledger <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, August 17, 1999 5:45 AM
Subject: [TN] Innerlayer issue
> Good Morning Technetters,
>
> I have a question for board fabbers. Problem: We are experiencing
> weave texture on our innerlayer material. I have spoken to the
> manufacturer who states that weave does shift in the "pour" of the
> material (when the resin is added) and that there is no specification
> that controls the depth requirement of the weave. The topography is
> visual prior to lam/image. The condition is causing our resist to lift
> slightly and allows an etch stain on the double treat foil that so far
> we can not remove. Question: Is this a typical condition of innerlayer
> material (other manufacturers)? Is it double treat foil only? Is there
> a way to remove this type of etch stain? What is the acceptablity of
> stain on inner layer foil? I can't find any reference info in IPC.
>
> Any and all input would be appreciated.
>
> Anne Ledger
> EMDS, Inc.
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|