Beware the ides of nickel. If exposed, as Kovar or Invar, solderability is
the traditional issue.
Earl Moon
----- Original Message -----
From: Severson, Scott M. <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, August 17, 1999 8:50 AM
Subject: [TN] Cu/Ni Alloy?
> Hi All,
>
> We have some SMT LED's that were exhibiting solderability problems and
> investigation with the SEM/EDS revealed that the base metal is composed of
a
> copper alloy that contains about 10% nickel. Does anybody have any
> experience with this material? Do they require higher reflow temperatures
> similar to Alloy 42?
>
> Any information would be appreciated.
>
> Thanks
> Scott
>
>
****************************************************************************
> *************************
> Scott M. Severson
> QA/FA Lab Manager "Space and
Time
> are not
> conditions in which we live,
> Benchmark Electronics Inc. but modes in which we
> think."
> 4155 Theurer Blvd.
> Winona, MN 55987
> ---Albert Einstein
> (507)452-8932
>
****************************************************************************
> *************************
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|