Take care for the stresses that occur during the mini PCBs separation, the
ceramic components should be far enough from the V Groove line.

Best  Regards

Reuven  ROKAH




                      Jeffrey Bush
                      <Jeffrey.Bush@VTCI         To:      [log in to unmask]
                      RCUITS.COM>                cc:
                      Sent by: TechNet           Subject: Re: [TN] Subject: V-Groove Keep Out Area
                      <[log in to unmask]>


                      15/06/2004 23:50
                      Please respond to
                      "TechNet E-Mail
                      Forum."; Please
                      respond to Jeffrey
                      Bush





Jump score will allow also a combination of routing - along the
sensitive area - and v-groove for webs to keep the unit in the pallet.
The keep-put area is ~ .300"+ as the blades have a transition as they
jump in and out.  Using a v-score web over tabs with perforation holes
is a good pallet design that is easy to work with.



Jeffrey Bush
Director, Quality Assurance and Technical Support

                          76 Technology Drive - POB 1890
                             Brattleboro, Vermont 05302-1890
                                Tel. 802.257.4571.21 Fax. 802.257.0011
                                    [log in to unmask]
                              http://www.vtcircuits.com



-----Original Message-----
From: Croslin, Robert [mailto:[log in to unmask]]
Sent: Tuesday, June 15, 2004 3:51 PM
To: [log in to unmask]
Subject: Re: [TN] Subject: V-Groove Keep Out Area


Daan, can you explain jump scoring.  I've never heard the term before

Thanks,

Bob Croslin
Nielsen Media Research


-----Original Message-----
From: Daan Terstegge [mailto:[log in to unmask]]
Sent: Monday, June 14, 2004 10:05 AM
To: [log in to unmask]
Subject: Re: [TN] Subject: V-Groove Keep Out Area


Hi Bob,

Have you tried jump-scoring?  With this technique you can have thinner
webs, while keeping the stiffness of the panel.

Daan Terstegge
Thales Communications
Unclassified mail
Personal Website: http://www.smtinfo.net

>>> [log in to unmask] 06/10/04 09:20pm >>>
I have been given a v-groove score keep out area dimension of 1mm from
the edge of the groove to the component body; except the dimension
becomes 5mm for ceramic components. 5mm seems like a very large value.
Does anybody have experience with this? Is it really necessary to keep
ceramic components that far from a v-groove score?

Thanks.

Bob

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2