TECHNET Archives

March 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 19 Mar 2008 17:02:53 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Wenger, George M." <[log in to unmask]>
Subject:
From:
"Wenger, George M." <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (78 lines)
 

Maybe I missed something.  I would expect
Werner,



 



Maybe I missed something.  I would expect that if one looked at the BGA

ball side of a fracture you would see something completely different

from the 35-50%Ni, 20%Sn, and a couple of percent Pb that they

indicated.  I think that some of the fractures might have occurred at

the solder ball  / BGA package interface and that they were looking at

the package side of those fractures rather than the ball side of a

fracture at the PCBA.



 



Regards,



George



George M. Wenger



Andrew Wireless Solutions



Senior Principal FMA / Reliability Engineer



40 Technology Drive, Warren, NJ 07059



(908) 546-4531 [Office]  (732) 309-8964 [Cell]



[log in to unmask]



 



________________________________



From: [log in to unmask] [mailto:[log in to unmask]] 

Sent: Wednesday, March 19, 2008 4:50 PM

To: Wenger, George M.; [log in to unmask]

Subject: Re: [TN] Case of the popping BGAs



 



Hi George,

The ball-side fracture surfaces were measured and described.







Werner







**************

Create a Home Theater Like the Pros. Watch the video on AOL Home.

(http://home.aol.com/diy/home-improvement-eric-stromer?video=15?ncid=aol

hom00030000000001)



------------------------------------------------------------------------------------------------

This message is for the designated recipient only and may

contain privileged, proprietary, or otherwise private information.  

If you have received it in error, please notify the sender

immediately and delete the original.  Any unauthorized use of

this email is prohibited.

------------------------------------------------------------------------------------------------

[mf2]



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2