TECHNET Archives

March 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Igoshev, Vladimir" <[log in to unmask]>
Date:
Fri, 21 Mar 2008 12:38:35 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Wenger, George M." <[log in to unmask]>
Subject:
From:
"Wenger, George M." <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (105 lines)
That is exactly my point; none of the terms being used
Vladimir,



That is exactly my point; none of the terms being used for ENIG failures

such as "Black Pad", "Black Line Nickel", "Weak Nickel", "something

else", "Mud Cracking", "Dark Gray Pad", etc. are scientific definitions.







Regards,

 

George

George M. Wenger

Andrew Wireless Solutions

Senior Principle FMA / Reliability Engineer

40 Technology Drive, Warren, NJ 07059

(908) 546-4531 (office) (732) 309-8964 (cell)

[log in to unmask]

 



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Igoshev, Vladimir

Sent: Friday, March 21, 2008 12:28 PM

To: [log in to unmask]

Subject: Re: [TN] Case of the popping BGAs



Hi Werner,



From all failures I've seen on ENIG including BP, Brittle Fracture and

something else (which does exist on ENIG but does not belong to either

of the two), I would say that they look pretty much the same as far as a

shade of black is concerned.



I agree with Dave. Introducing such "scientific" definitions :-) as grey

pad and so on, won't help :-)



Regards,





Vladimir



----- Original Message -----

From: TechNet <[log in to unmask]>

To: [log in to unmask] <[log in to unmask]>

Sent: Fri Mar 21 12:06:12 2008

Subject: Re: [TN] Case of the popping BGAs



Hi Dave,

Shades of black, maybe.

Of course, not all 'Black Pad' failures have a black appearance, that is

why some peoble come up with things like 'Gray Pads' and 'ENIG Brittle

Fractures' 

in apparent contrast to 'Black Pad'.

That is why George Wenger asked his question.







Werner







**************

Create a Home Theater Like the Pros. Watch the video on AOL 

Home.

      

(http://home.aol.com/diy/home-improvement-eric-stromer?video=15?ncid=aol

hom00030000000001)



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------



------------------------------------------------------------------------------------------------

This message is for the designated recipient only and may

contain privileged, proprietary, or otherwise private information.  

If you have received it in error, please notify the sender

immediately and delete the original.  Any unauthorized use of

this email is prohibited.

------------------------------------------------------------------------------------------------

[mf2]



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2