TECHNET Archives

March 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 31 Mar 2008 09:31:42 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, David Tremmel <[log in to unmask]>
Subject:
From:
David Tremmel <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Comments:
RFC822 error: <W> MESSAGE-ID field duplicated. Last occurrence was retained.
Parts/Attachments:
text/plain (43 lines)
Hello,

 

I am interested in reballing/rebumping BGAs and replacing the SAC305 solder
spheres with 62/2/36 but would like to know if there is any reliability data
or at least a white paper or study published on the subject.

 

If there are no papers or studies available, would anyone venture an opinion
on how will the extra silver (compared to 63/37) effect the solder joint?
Will the extra silver help lessen cyclic creep-fatigue?

 

 

Thank you in advance for your responses. 

 

 

Thank you,

 

David Tremmel

Value Recovery


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2