Not sure I worded this question so will ask again a slightly different way as I didn't get any responses.
If one is reflow soldering ENIG boards with a mixture of SnPb & PbF part (in particular PbF BGA's - SAC305) using a 63/37 SnPb solder what would be the preferred peak temp / time above?
Regards,
Iain.
-----Original Message-----
From: Braddock, Iain
Sent: 17 November 2006 08:35
To: [log in to unmask]
Subject: RE: [TN] BGA anomaly
Joyce,
I can't say it is preferable but how does one solder a board using SnPb solder with the odd PbF part whilst trying to ensure the profile will provide sufficient time above Solidus (Werner see I've learned!) to enable a satisfactory soldered joint?
Regards,
********************************************************************
This email and any attachments are confidential to the intended
recipient and may also be privileged. If you are not the intended
recipient please delete it from your system and notify the sender.
You should not copy it or use it for any purpose nor disclose or
distribute its contents to any other person.
********************************************************************
|
|
|