Ian:
The short answer is do not do it. There are plenty of
responses on this matter in the archives. Specifically SAC BGA balls do
not solder reliably well using 63/37 SnPb solder, should reball. LF
terminations (Pure Sn) will solder fine except, must ensure whisker
mitigation methods are put in place.
Regards,
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Braddock, Iain
Sent: Monday, November 20, 2006 6:48 AM
To: [log in to unmask]
Subject: Re: [TN] BGA anomaly
Not sure I worded this question so will ask again a slightly different
way as I didn't get any responses.
If one is reflow soldering ENIG boards with a mixture of SnPb & PbF part
(in particular PbF BGA's - SAC305) using a 63/37 SnPb solder what would
be the preferred peak temp / time above?
Regards,
Iain.
-----Original Message-----
From: Braddock, Iain
Sent: 17 November 2006 08:35
To: [log in to unmask]
Subject: RE: [TN] BGA anomaly
Joyce,
I can't say it is preferable but how does one solder a board using SnPb
solder with the odd PbF part whilst trying to ensure the profile will
provide sufficient time above Solidus (Werner see I've learned!) to
enable a satisfactory soldered joint?
Regards,
********************************************************************
This email and any attachments are confidential to the intended
recipient and may also be privileged. If you are not the intended
recipient please delete it from your system and notify the sender.
You should not copy it or use it for any purpose nor disclose or
distribute its contents to any other person.
********************************************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|