It's a good point, a 10C drop in oven temp can virtually double time to full
cure. The quality of cure can also be affected by the longer time/lower
peak, thus you could be getting a lower Tg. One way of doing this without
"changing anything" would be to increase the oven load by increasing the
number of boards cured.
Regards
Mike Fenner
Applications Engineer, European Operations
Indium Corporation
T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Leadfree: www.Pb-Free.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Braddock, Iain
Sent: Monday, January 27, 2003 8:20 AM
To: [log in to unmask]
Subject: Re: [TN] This is a new one on me
Like Carrie I have seen this in the past, turned out to be the oven
calibration, the cure temp used was at the lower end of the manufacturers
recommendation. With the oven performing under temp the cure 'appeared' to
hold components but some fell off during wavesolder.
Iain.
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: 22 January 2003 17:13
To: [log in to unmask]
Cc: [log in to unmask]
Subject: Re: [TN] This is a new one on me
*** WARNING ***
This mail has originated outside your organization,
either from an external partner or the Global Internet.
Keep this in mind if you answer this message.
I've seen this before and it turned out to be an improper cure profile.
Unfortunately, it sounds like you've been running the process for a while.
So, the question lies in what variables are most likely to change.
Do you have a new oven? New adhesive? What's the lot number on the
adhesive?
Do you have a new operator? Did ANYTHING change in the process? Did
ANYTHING
change with the raw materials (components, adhesive -- storage, purchasing?)
Good luck.
Please let us all know what you find so we can add it to our archives of
"Wow...never heard of that happening!"
-Carrie
-----Original Message-----
From: Bill Page [mailto:[log in to unmask]]
Sent: Wednesday, January 22, 2003 10:09 AM
To: [log in to unmask]
Subject: [TN] This is a new one on me
Hey folks,
I've been in this business for over 20 years, and thought I had seen it all,
but this is a new one. We're having problems with our glue/wave solder
process. Parts are falling off the board.
"That's not new," you say?
"Check your handling, stupid," you say?
"Check your glue cure process, stupid," you say?
Yep.
Shear tests indicate that our glue process is working.
We're using a product that is very widely used in the industry, following
the manufacturer's recommended cure profile.
And yet, parts fall off -- as they go through the wave solder machine.
Adhesive stays put. Has a flat surface where the part used to be.
Pads are beautifully soldered...just no parts there.
And we have verified that the parts are present before the wave.
Across chip suppliers and part numbers, across solder mask types, across PWB
vendors.
Is it just me?
Is the business finally catching up with me?
Should I give up and become a high school band director?
Your suggestions are welcome!
Bill Page
Kenosha, WI
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
********************************************************************
This email and any attachments are confidential to the intended
recipient and may also be privileged. If you are not the intended
recipient please delete it from your system and notify the sender.
You should not copy it or use it for any purpose nor disclose or
distribute its contents to any other person.
********************************************************************
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|