The way to stick low energy surfaces is to make them high energy!
I don't think there is an adhesion promoter chemical for Teflon (as there is
for silicones) so the way to do it would be to belt it with a plasma to
impregnate the surface. Alternatively you can try a controlled char or
powerful oxidizing chemical to do the same thing. These are fairly heroic
for a repair situation so whether this is practical/possible/economic is
what you will have to decide!
May also be worth trying someone like www.belzona.com
They specialise in repair adhesives and processes, usually for metal repairs
and structures but they may be able to come up with something to restore
functionality.
Good luck!
Regards
Mike Fenner
Applications Engineer, European Operations
Indium Corporation
T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Leadfree: www.Pb-Free.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of
[log in to unmask]
Sent: Thursday, January 30, 2003 2:24 AM
To: [log in to unmask]
Subject: [TN] Adhesive for Teflon
'Morning, All
This object of this problem is not a board, but a wave guide with a (PTFE?)
teflon dome bonded to it - or at least to what looks like glass fibre
cladding on the waveguide flange. The guide is pressurised to 28 p.s.i. at
1 atmosphere.
Wall thickness of the dome is approx 10 mils. The flange that it's bonded
to measures about 2.75" x 1.5" x 0.4" thick and there are traces of a
yellow-coloured material, which I take to be the adhesive that bonds the
teflon dome to the flange. I cannot be sure, though.
The problem now is that the dome has separated from the flange along one
side so that it can no longer be pressurised. It's a very expensive
component, and worth repairing if possible. Does any one of you great folks
know of an adhesive and method of application that would be effective in
rebonding the teflon back onto the GF-coated flange? Obviously the adhesive
must stick well to low-energy surfaces, but additonally it must have good
tensile adhesion, since the internal pressure of the dome will tend to
"peel" the rectangular wall away from the flange.
Any help will be greatly appreciated. At present, components that have been
'punctured' like this are just thrown away and replaced with new ones, and
there may be a very good reason for this - like it's not possible to remove
the dome, clean it up and bond it back in place again, but I thought I
would ask anyway.
TIA
Peter
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|