TECHNET Archives

August 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Charles Barker <[log in to unmask]>
Date:
Thu, 12 Aug 1999 08:40:10 -0500
Content-type:
text/plain; charset=us-ascii
X-To:
Jim Marsico 516-595-5879 <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (89 lines)
Jim
Dow Corning has a product whihc is supposed to remove traces of silicon. I don't
remember the name. Our rep would be glad to fill you in if you don't have a
contact for Dow.

Edd Anthony
Krayden, Inc.
281-238-9080 Ph
281-238-9081 FAX

Good luck
Charlie B.







Jim Marsico 516-595-5879 <[log in to unmask]> on 08/12/99 07:23:00 AM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond to
      Jim Marsico 516-595-5879 <[log in to unmask]>








 To:      [log in to unmask]

 cc:      (bcc: Charles Barker/US/I-O INC)



 Subject: [TN] SILICONE CONTAMINATION








Good Morning Technet:

Can anyone suggest methods of cleaning cast aluminum plates of silicone
residue (from a silicone-based machining oil)?  These plates must be clean
enough to bond to using a structural epoxy.

Thanks...

Jim Marsico
AIL Systems Inc.
(516) 595-5879
[log in to unmask]


##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2