I have used a Dow Corning OS-XXX product to strip silicone coating from
tooling. They had an azeotropic mix with alcohol that evaporated in seconds.
5 minutes later, I could coat the tooling in acrylic (I tried it to qualify
the cleaner, not used in production) with no problems.
Try using one of these fluids.
You may also see if the supplier can use an organic machining oil.
Aric Parr
Sr. Process Engineer
Eaton Corporation
1400 S. Livernois
PO Box 5020
Rochester Hills, MI 48308-5020
248 608 7780
[log in to unmask]
---------- Original Text ----------
From: C=US/A=INTERNET/DDA=ID/TechNet(a)IPC.ORG, on 8/12/99 7:51 AM:
Good Morning Technet:
Can anyone suggest methods of cleaning cast aluminum plates of silicone
residue (from a silicone-based machining oil)? These plates must be clean
enough to bond to using a structural epoxy.
Thanks...
Jim Marsico
AIL Systems Inc.
(516) 595-5879
[log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|