You're right Tony ,
one of those .
We run NiAu for ages , analysing pot annually , only a trace in it .
That is whole boards , not just con's .
As far as the dross gold "mop" , not quite , gold stays .
It would sure pleased recyclers otherwise .
Checked that one , you bet .
See you Paul Klasek ; ResMed
>----------
>From: Tony Bugeja[SMTP:[log in to unmask]]
>Sent: Tuesday, 10 February 1998 23:32
>To: [log in to unmask]
>Subject: [TN] Leaching of Gold into a solder pot?
>
>-- [ From: Tony Bugeja * EMC.Ver #2.5.02 ] --
>
>Is it a big problem running gold connectors in your wave solder? Will it
>contaminate your pot? Or is this just a myth?
>
>Doesn't alot of the gold just end up being dross?
>--
>Tony Bugeja, P.Eng. E-Mail: [log in to unmask]
>Process Engineer Phone: (204) 631-7241
>C-Mac Electronics Fax: (204) 631-7294
>1455 Mountain Ave
>Wpg., Mb. R2X 2Y9
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
>information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>847-509-9700 ext.311
>################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|