TECHNET Archives

February 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Paul Klasek <[log in to unmask]>
Date:
Wed, 11 Feb 1998 08:45:23 +1100
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Paul Klasek <[log in to unmask]>
Parts/Attachments:
text/plain (59 lines)
You're right Tony ,

one of those .
We run NiAu for ages , analysing pot annually , only a trace in it .
That is whole boards , not just con's .

As far as the dross gold "mop" , not quite , gold stays .
It would sure pleased recyclers otherwise .
Checked that one , you bet .

See you                  Paul Klasek ; ResMed

>----------
>From:  Tony Bugeja[SMTP:[log in to unmask]]
>Sent:  Tuesday, 10 February 1998 23:32
>To:    [log in to unmask]
>Subject:       [TN] Leaching of Gold into a solder pot?
>
>-- [ From: Tony Bugeja * EMC.Ver #2.5.02 ] --
>
>Is it a big problem running gold connectors in your wave solder?  Will it
>contaminate your pot? Or is this just a myth?
>
>Doesn't alot of the gold just end up being dross?
>--
>Tony Bugeja, P.Eng.         E-Mail: [log in to unmask]
>Process Engineer            Phone:  (204) 631-7241
>C-Mac Electronics           Fax:    (204) 631-7294
>1455 Mountain Ave
>Wpg., Mb. R2X 2Y9
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
>information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>847-509-9700 ext.311
>################################################################
>
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2