You're right Tony , one of those . We run NiAu for ages , analysing pot annually , only a trace in it . That is whole boards , not just con's . As far as the dross gold "mop" , not quite , gold stays . It would sure pleased recyclers otherwise . Checked that one , you bet . See you Paul Klasek ; ResMed >---------- >From: Tony Bugeja[SMTP:[log in to unmask]] >Sent: Tuesday, 10 February 1998 23:32 >To: [log in to unmask] >Subject: [TN] Leaching of Gold into a solder pot? > >-- [ From: Tony Bugeja * EMC.Ver #2.5.02 ] -- > >Is it a big problem running gold connectors in your wave solder? Will it >contaminate your pot? Or is this just a myth? > >Doesn't alot of the gold just end up being dross? >-- >Tony Bugeja, P.Eng. E-Mail: [log in to unmask] >Process Engineer Phone: (204) 631-7241 >C-Mac Electronics Fax: (204) 631-7294 >1455 Mountain Ave >Wpg., Mb. R2X 2Y9 > >################################################################ >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c >################################################################ >To subscribe/unsubscribe, send a message to [log in to unmask] with following >text in the body: >To subscribe: SUBSCRIBE TechNet <your full name> >To unsubscribe: SIGNOFF TechNet >################################################################ >Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional >information. >For the technical support contact Dmitriy Sklyar at [log in to unmask] or >847-509-9700 ext.311 >################################################################ > > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################