It has been our procedure to bake flex circuits (Kapton) for 2 hours at 
100 degrees C. prior to assembly and solder reflow in order to drive off 
any entrained moisture. 
A question has come up as to what is the recommended length of time the 
parts can remain in the asssembly environment prior to a re-bake being 
necessary. 
We would appreciate hearing what the conventional wisdom is from you 
TechNetters.

Regards

Sherman Banks
[log in to unmask]
408/481-6047

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2