Greeting mighty TechNetters.
Here's a common question, I think, but not common enough that I found it in a search.
Scenario-Small PWB fab shop. Customer wants vias (no larger than .016 inch) plugged to prevent light, vacuum, you name it, from escaping through. Must be plugged from at least one side, and tented on the other. We build it on an 16x18 panel, probably .063 finished thickness with 1/1 outers. LPI and SMOBC ink are applied manually at this time. (squeegee, squeegee, bake [or tack]) We have not come up with a reliable process. New equipment is probably not an option yet, unless its like a bigger squeegee. (ha ha).
Any assistance is appreciated.
Steve MacDonald
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|