Define "quick".  The shortest quality control SIR test that I know of is an
unpublished 24 hour test used by AT&T.  It is essentially the Bellcore 35/90
test for 24 hours and no bias.  This spot test is used to monitor the
process.  Same Bellcore pass/fail requirements.  We have done some of AT&T's
overflow testing in the past and it seems to work well if you have an
established baseline.

Doug Pauls
CSL

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2