Fellow TechNetters:

   What is the acceptable guideline for IMC Formation thickness on OSP after 2x rework..   IPC-4555 is still pending.  I've heard of 3-5 microns on first pass and 5-10 microns on 2x RW.   All comments/suggestions welcomed.

Victor,