TECHNET Archives

August 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 7 Aug 2013 10:25:24 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Inge Hernefjord <[log in to unmask]>
Subject:
From:
Inge Hernefjord <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="ISO-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (78 lines)
Much noise for a single void. 30% tells me it wasn't from the soldering
process but existed even before. With other words a defect ball. The
failure seems to be far out from Weibull's cc, i.e. <6S, so it's not worth
much more jogging.

Inge


On 30 July 2013 20:25, David D. Hillman <[log in to unmask]>wrote:

> Hi Leland - I love the supplier's comment as the existence of the 30% void
> demonstrates the statement to not be true. Was the 30% void an observation
> or was it associated with an component failure? Do you have open microvias
> in the pads? Also -  the JSTD-001 committee is revising the BGA void
> criteria to 30% based on a series of test results submitted to the
> committee.
>
> Dave
>
>
>
> From:   Leland Woodall <[log in to unmask]>
> To:     <[log in to unmask]>
> Date:   07/30/2013 01:19 PM
> Subject:        [TN] Singular 30% Void and Oversize Ball Diameter
> Sent by:        TechNet <[log in to unmask]>
>
>
>
> Folks,
>
> We run thousands of boards a day, and almost every one carries a BGA.  We
> inspect each with inline X-ray.
>
> Last week, we had one single ball to fail for a 30% void and an oversize
> diameter.  We contacted the supplier, and they said their process was
> incapable of sending out such a defect.
>
> We've never had a void over 5%, and even those are incredibly rare.
>
> What within our process might have caused this, and do you agree with the
> statement of the supplier?  How do you recommend we analyze the failure?
>
> Thanks in advance for your help!
>
> Leland
>
> ________________________________
>
> ?Confidentiality Notice:
> This transmission (including any attachments) may contain confidential
> information belonging to the sender and is intended only for the use of
> the party or entity to which it is addressed. If you are not the intended
> recipient, you are hereby notified that any disclosure, copying,
> distribution, retention or the taking of action in reliance on the
> contents of this transmission is strictly prohibited. If you have received
> this transmission in error, please immediately notify the sender and erase
> all information and attachments.?
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2