Hi Richard,
My experience from Shercon is null, little better about PA.
Must be primed with polyurethane/rubber solution + 5% of isocyanate
cure.Before this, you should of course do the standard degreasing plus
grinding the surface of the PA with grit 600-1200.
PA can also be primed with phenol-resorcinol glue. Same pre-treatment.
It's twenty years since I was involved in the above, many new methods may
exist today.
Inge
On 6 August 2013 06:17, Stadem, Richard D. <[log in to unmask]>wrote:
> Do you think the silicone adhesive on Kapton and Shercon tapes can create
> a manufacturing issue during conformal coating or for sensitive electronics?
> Doug, I would be especially interested in your respected input on this
> question.
>
> This message and/or attachments may include information subject to GDC4S
> S.P. 1.8.6 and GD Corporate Policy 07-105 and are intended to be accessed
> only by authorized recipients. Use, storage and transmission are governed
> by General Dynamics and its policies. Contractual restrictions apply to
> third parties. Recipients should refer to the policies or contract to
> determine proper handling. Unauthorized review, use, disclosure or
> distribution is prohibited. If you are not an intended recipient, please
> contact the sender and destroy all copies of the original message.
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|