IR is tricky in that the emisivity of the part plays a large role in its
ability to absorb IR energy.  Max component temp's that I have generally seen
max out at 140C.  You might want to try using a connector with a different
emisivity coefficient.

If you can't get enough energy to the joints, you could also consider press-
fit connectors.

Frank

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2