TECHNET Archives

September 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 28 Sep 2000 12:40:21 EDT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Mike Sewell <[log in to unmask]>
Parts/Attachments:
text/plain (29 lines)
We're going through the same scenario right now and for the next ~18,000
assys.  Same TH board that Steve G. has taken such a liking to.  Massive
amounts of cut/clip/rotate leads are required on this one.  The problem is
primarily with the DIP ICs on this board as they are laid out very close and
have tracks running between the rows of leads on the bottom.  If the design
isn't "locked in stone"  I'd suggest re-routing traces or perhaps adding
another layer to cover the problem traces/conductors.  If that isn't an
option, you might stuff those parts loose formed and pretrimmed - provided
its only a few per bd giving you trouble.  Reducing the lead protrusion
should make the lead less likely to bend in the field as more of the lead
will be supported by the solder joint...

Regards,
Mike Sewell

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2