Check out _Electronic Packaging Materials and Their Properties_, by Pecht et
al, published by CRC Press. It shows it depends on resin fraction and varies
from 12-20 ppm/deg C in plane, and 60-80 ppm/deg C in the "z-axis". (Don't
forget the units...a lesson NASA recently re-learned the hard way!)
Hope that helps.
Timothy Reeves
ECD Circuit Board Division
13626 South Freeman Road
Mulino, OR 97042
[log in to unmask]
(503) 829-9108 (800) 228-8198 FAX (503) 829-5482
> ----------
> From: John Brewer
> Sent: Tuesday, October 5, 1999 10:16 AM
> Subject: FR-4 Coeff of thermal expansion? Material Data?
>
> Can anyone point me to
>
> (specifically) coeff of thermal expansions for FR4
> (generally) material properties for same?
>
> Thanks!
> John
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|