TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Dave Hoover <[log in to unmask]>
Date:
Tue, 5 Oct 1999 11:31:37 -0700
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Dave Hoover <[log in to unmask]>
Parts/Attachments:
text/plain (77 lines)
Here's an answer from some time back......5 '96

Groovy
-----------------------------------------------------------------------
Bob Holmes said....

The TCE of FR-4 is non-isotropic and it varies with resin content and
temperature.  Resin has a much higher TCE than glass, so in-plane TCE is
severely restrained by glass.  Out-of-plane, the glass provides little
restrain
and the TCE can be 50 ppm/C or higher. In the plane of the glass cloth, low
resin materials such as the FR-4 used for DSR can have a TCE as low as 14 or
15
ppm/C. The higher resin content cores used in an MLB can have an in-plane
TCE
as high as 20 ppm/C.  As an approximation I usually use 17ppm/C as an
average
in-plane value.  This matches copper and if a PWB contains a lot of copper
it
will tend to move the TCE toward this value.

Near Tg, the in-plane TCE begins to rise until the material reaches a
temperature slightly above Tg.  At that point, the modulus of the resin
drops
dramatically and the glass cloth begins to dominate.  This increases the
out-of-plane TCE and reduces the in-plane TCE.  Values of in-plane CTE in
the
range of 10 ppm/C can be observed at this point.

Robert R Holmes PhD
Lucent Technologies (formerly AT&T)
[log in to unmask]

-----Original Message-----
From: John Brewer [mailto:[log in to unmask]]
Sent: Tuesday, October 05, 1999 10:17 AM
To: [log in to unmask]
Subject: [TN] FR-4 Coeff of thermal expansion? Material Data?


Can anyone point me to

(specifically) coeff of thermal expansions for FR4
(generally) material properties for same?

Thanks!
John

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2