TECHNET Archives

January 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"David D. Hillman" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 17 Jan 2008 13:38:21 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (75 lines)
Hi Werner - Yep, we do have that information. The solderability of the 
SnCu IMC's (e.g. Cu3Sn and Cu6Sn5) is documented in the book  The 
Mechanics of Solder Alloy Wetting & Spreading, Yost, Hosking, Frear, ISBN 
0-442-01752-9 (data from NIST and Rockwell) using both wetting balance and 
SERA analysis techniques. Just my opinion, but I believe much of the 
data/discussions/conclusions in those data sets is applicable to the Au/Sn 
IMC phase.

Dave



Werner Engelmaier /* <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
01/17/2008 09:36 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]


To
[log in to unmask]
cc

Subject
Re: [TN] SV: [TN] SV: [TN] Solderability of Tin-Gold Intermetallic






Hi All,
We know that Cu6Sn5 is non-solderable after oxidation. However, I do not 
know 
whether we really KNOW that it is solderable prior to that, and we know 
even 
less about the solderability of AuSn4, Ag3Sn, or for that matter Sn3Ni4.



Werner



**************
Start the year off right.  Easy ways to stay in shape.
 
http://body.aol.com/fitness/winter-exercise?NCID=aolcmp00300000002489

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2