I appreciate you for your input Francis, The non uniformity I mentioned in my previous
mail is within the same PR opening. The current ranges we use are in mAs and we plate at
about 6 to 10 mA/cm2
thanks again,
Yasmeen
Francis Lai wrote:
> nishath yasmeen wrote:
>
> > We are seeing non uniform plated copper deposits in very small areas on
> > silicon wafers from the acid copper plating bath.
> >
> > I can understand the non uniformity across areas which are large (
> > inches) but these areas measure in micron range. The thickness profile
> > of this area looks like a staircase on the profilometer. Is this a flow
> > problem? Does this depend on the current density?
> > What other factors do I need to consider for uniformity improvement?
> >
> > Any suggestions will be greatly appreciated.
> > Thanks,
> > Yasmeen
> >
> > ##############################################################
> > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> > ##############################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> > the body:
> > To subscribe: SUBSCRIBE TECHNET <your full name>
> > To unsubscribe: SIGNOFF TECHNET
> > ##############################################################
> > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> > information.
> > If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> > 847-509-9700 ext.5365
> > ##############################################################
>
> Dear Yasmeen:
>
> I would regard your case as pattern plating. In pattern plating, the current densities
> on each area vary. Smaller area will take more current and plate more while lager area
> will take less current and plate less. I suggest you to use current density of 10
> mA/cm**2. If you are plating areas measuring in microns, you need a power supply which
> can provide currents in mA for the acid plating bath.
>
> Please correct me if I am wrong!!!!!
>
> Francis
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|