TECHNET Archives

October 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Mike Fenner <[log in to unmask]>
Reply To:
Date:
Wed, 13 Oct 2004 12:44:09 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (272 lines)
I think this maybe choice of words. What you describe as moist could be wet,
and dry ones could be solid. I think that's what I mean or am I just
generalising from tantalum capacitors to the whole world?

Regards 

Mike 




-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
Sent: Wednesday, October 13, 2004 8:25 AM
To: [log in to unmask]
Subject: Re: [TN] Aluminum electrolytic Cap's


Hey, wait a minute, Joyce. I haven't seen a WET elco for at least 50
years. All elcos today, to the best of my knowledge, are dry and neither
need nor have venting. A wet elco literally has liquid in them and, if
you shake them, you can hear/feel it slopping around. Wet elcos had the
advantage they were self-healing. I think the last manufacturer was
possibly Philips in the 1940s.

Dry elcos are not really dry, but have a moist absorbent material
between the electrodes, but they are not self-healing, therefore do not
generate gas. The dielectric is a pre-anodised layer on the anode,
before the capacitor is wound, so there is no electrolysis within the
case and no gas generation. The moist layer is actually there just as a
contact from the cathode to the thin dielectric.

And if what you say were true, there would be two problems:
a) you could not have hermetic components
b) if the component were vented, the small amount of moisture in the
absorbent layer would be lost by evaporation and the elco would become
pF, instead of uF!

Brian

Joyce Koo wrote:

> Disagree on the the coating... although the coating may be softer
initially,
> the acrylic coating can be hardened during the life of the product, may be
> interfere the venting mechanism.  Agree with your customer, it should not
be
> coated (see attached).
>
> my 1.6 cents.
>                             jk
>
> "In the operation of a wet electrolytic capacitor a certain amount of gas
is
> generated from the electrolysis of the electrolyte and unless means is
> provided for the purpose quite high pressures may be built up inside the
> container. For this reason it has been found necessary to provide the
covers
> with some form of vent. In practically all instances this vent takes the
> form of a thin sheet of gum rubber which is perforated by a very small
hole.
> The thickness of the rubber and the size of the perforation determine the
> pressures at which venting action will occur. In practice it is desirable
to
> obtain venting action at the lowest pressure which will prevent actual
> leakage or escape of electrolyte through the perforation. "
>
>
>
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Brian Ellis
> Sent: Monday, October 11, 2004 2:32 AM
> To: [log in to unmask]
> Subject: Re: [TN] Aluminum electrolytic Cap's
>
>
> I see no reason why hermetically sealed elcos cannot be conformally
> coated. If an elco generates pressure, it is because it is already in a
> fault condition and should therefore be changed, anyway.
>
> Brian
>
> Lum Wee Mei wrote:
>
>>Hello,
>>
>>Since we are on electrolytic cap, how about conformal coating (acrylic) on
>
> them?
>
>>We have been coating them since day one as no one has instructed that
>>electroltic cap cannot be coated.
>>
>>Recently, there have been opinion that we cannot coat them as there will
>
> be no
>
>>gap for the pressure to escape - similar to the below issue?
>>
>>What are your opinions?
>>
>>Regards,
>>Wee Mei
>>
>>
>>Quoting Brian Ellis <[log in to unmask]>:
>>
>>
>>
>>>It depends on what cleaning medium you are using. If you are using a
>>>halogenated solvent and just a microgram penetrates inside the casing,
>>>you will see customers complaining of failures after 6 months to 2
>>>years. This is well-known and was publicised by Sprague in the 1960s.
>>>This company recommended using only hermetically sealed elcos if
>>>cleaning in halogenated solvents. They also tested aqueous cleaning and
>>>determined zero effect by aqueous cleaning, including with saponifiers
>>>which could cause superficial corrosion of the outer case. However,
>>>IMHO, it always makes sense with aqueous cleaning to have each stage
>>>slightly warmer (say 5 deg C) than the previous one, so that you always
>>>have positive pressure inside the cans while they are wet, to prevent
>>>the ingress of contaminated water.
>>>
>>>Brian
>>>
>>>Scott Lefebvre wrote:
>>>
>>>
>>>
>>>>We have a problem with the plastic disk coming off after being process
>>>
>>>through our In-Line PCB washer.  What concerns if any should I have.
>>>
>>>
>>>>---------------------------------------------------
>>>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>>>>To unsubscribe, send a message to [log in to unmask] with following text
in
>>>>the BODY (NOT the subject field): SIGNOFF Technet
>>>>To temporarily halt or (re-start) delivery of Technet send e-mail to
>>>
>>>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>>>
>>>
>>>>To receive ONE mailing per day of all the posts: send e-mail to
>>>
>>>[log in to unmask]: SET Technet Digest
>>>
>>>
>>>>Search the archives of previous posts at:
>
> http://listserv.ipc.org/archives
>
>>>>Please visit IPC web site
>
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>
>>>for additional information, or contact Keach Sasamori at [log in to unmask]
or
>>>847-509-9700 ext.5315
>>>
>>>
>>>>-----------------------------------------------------
>>>>
>>>>
>>>
>>>---------------------------------------------------
>>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>>>To unsubscribe, send a message to [log in to unmask] with following text in
>>>the BODY (NOT the subject field): SIGNOFF Technet
>>>To temporarily halt or (re-start) delivery of Technet send e-mail to
>>>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>>>To receive ONE mailing per day of all the posts: send e-mail to
>>>[log in to unmask]: SET Technet Digest
>>>Search the archives of previous posts at:
http://listserv.ipc.org/archives
>>>Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>>>for additional information, or contact Keach Sasamori at [log in to unmask]
or
>>>847-509-9700 ext.5315
>>>-----------------------------------------------------
>>>
>>
>>
>>---------------------------------------------------
>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>>To unsubscribe, send a message to [log in to unmask] with following text in
>>the BODY (NOT the subject field): SIGNOFF Technet
>>To temporarily halt or (re-start) delivery of Technet send e-mail to
>
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>
>>To receive ONE mailing per day of all the posts: send e-mail to
>
> [log in to unmask]: SET Technet Digest
>
>>Search the archives of previous posts at: http://listserv.ipc.org/archives
>>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
>
>>-----------------------------------------------------
>>
>>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------


:::::::::::::::::::::::::::

This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.

:::::::::::::::::::::::::::

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2