Steve,
Unbelievable as this may seem they look as if they were dropped or
something was dropped on them!!!
David A. Douthit
Manager
LoCan LLC
Steve Gregory wrote:
> Got some more results from failure analysis. Went to level 2 on one of
> the parts that looked okay with x-ray and found this...again go to:
>
> http://www.stevezeva.homestead.com
>
> and look at "Chipped Chips 1-4"...
>
> We sure as hell didn't cause this...and as far as Phil's comment about
> a ESD event causing the broken wire bonds, it was the opinion of a
> gentleman at the failure analysis lab, that yes, broken wire bonds can
> be caused by ESD, but the board would need to be struck by a lightning
> bolt basically, to cause that kind of severe damage.
>
> My big question is; how in the hell does this CRAP get into the
> market?
>
> We're spending more than a few dollars getting this failure analysis
> done...I wonder how many companies would spend the money to do this?
> Or just go ahead and rework these failed devices?
>
> I'll tell you, this REALLY sucks...I think most of you can appreciate
> the time that we now have to spend reworking, cleaning, re-inspecting,
> and then re-testing the assemblies that these parts are used on...
>
> -Steve Gregory-
>
>
> --------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV
> 1.8e To unsubscribe, send a message to [log in to unmask] with following
> text in the BODY (NOT the subject field): SIGNOFF Technet To
> temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
> per day of all the posts: send e-mail to [log in to unmask]: SET Technet
> Digest Search the archives of previous posts at:
> http://listserv.ipc.org/archives Please visit IPC web site
> http://www.ipc.org/html/forum.htm for additional information, or
> contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|