TECHNET Archives

December 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Victor Hernandez <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 11 Dec 2009 15:29:06 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (275 lines)
It appears the Bow & Twist on a raw card/board is straight forward.  "
Push down on one side at a time and measure the deflection with a dial
indicator on the opposite side".   How about a finished assembly fully
populated with BGA heat sinks and DIMM cards.   The connector leads keep
the card/board from laying flat on a flat plate.   Even raised with
three equal thickness spacers and locked at one side.   The heaviest
part of the card/board will drop.

Victor,
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Monday, July 13, 2009 2:57 PM
To: [log in to unmask]
Subject: Re: [TN] Maximum Allowable Bow & Twist for PWB-PCB

That is described in the test method referred to earlier. 
The bare PWB is easy, put it on a tool grade flat plate. Push down on
one side at a time and measure the deflection with a dial indicator on
the opposite side. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee parker
Sent: Monday, July 13, 2009 1:37 PM
To: [log in to unmask]
Subject: Re: [TN] Maximum Allowable Bow & Twist for PWB-PCB

Bev and Richard

How do you suggest we measure to local bow and twist?

Best regards
Lee
J. L. Parker Ph. D.
JLP Consultants LLC
804 779 3389

  ----- Original Message ----- 
  From: Bev Christian<mailto:[log in to unmask]> 
  To: [log in to unmask]<mailto:[log in to unmask]> 
  Sent: Monday, July 13, 2009 12:53 PM
  Subject: Re: [TN] Maximum Allowable Bow & Twist for PWB-PCB


  Richard,
  Correct as usual, Richard. This was always a big deal at Nortel where
completed circuit packs would have to be slotted into card cages. 
  Bev
  On vacation

  ----- Original Message -----
  From: Stadem, Richard D.
<[log in to unmask]<mailto:[log in to unmask]>>
  To: [log in to unmask]<mailto:[log in to unmask]>
<[log in to unmask]<mailto:[log in to unmask]>>; Bev Christian
  Sent: Mon Jul 13 11:06:30 2009
  Subject: RE: [TN] Maximum Allowable Bow & Twist for PWB-PCB

  Bev, I totally agree with you, but the point they are getting at in
IPC
  2221 is that no section of the PWB should have more than .75% per inch
  as a rate of warpage, extending in both the X and Y directions, after
  reflow. This is because if you have more warpage than that you are
  putting a stress on the resultant solder joints that leads to a
  reduction in reliability, especially with a lead-free joint and also
  especially if you need to straighten the CCA when mounting it into a
  chassis or frame.
  I think this specification, like so many others that were based on
  leaded solder, should be revisited for unleaded solders.

  -----Original Message-----
  From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
  Sent: Friday, July 10, 2009 3:24 PM
  To: [log in to unmask]<mailto:[log in to unmask]>
  Subject: Re: [TN] Maximum Allowable Bow & Twist for PWB-PCB

  I contend this is old school and if you aren't measuring warpage at
  reflow temperatures how do you know you aren't suffering from head on
  pillow?

  I suggest the term head in pillow be dropped because you don't
actually
  put your head IN a pillow.

  Bev
  RIM

  PS Waiting for my Dewism.

  -----Original Message-----
  From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard
  Sent: Friday, July 10, 2009 4:20 PM
  To: [log in to unmask]<mailto:[log in to unmask]>
  Subject: Re: [TN] Maximum Allowable Bow & Twist for PWB-PCB

  IPC-2221 5.2.4 
  ...
  Unless otherwise specified by master drawing, max bow and twist shall
be
  0.75% for boards that use surface mount components and 1.5% for all
  other board technologies.
  ...
  Values are measured as per IPC-TM-650 Method 2.4.22 


  Genny Gibbard, P. Eng 
  Manufacturing Engineer, Vecima
  PTS dept. x.4229 

  -----Original Message-----
  From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
  Sent: July 10, 2009 2:15 PM
  To: [log in to unmask]<mailto:[log in to unmask]>
  Subject: [TN] Maximum Allowable Bow & Twist for PWB-PCB

  What is the maximum allowable Bow & Twist value?   Not able to locate
in
  IPC-2221, 2222, & 6012A

  Victor,

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
  unsubscribe, send a message to
[log in to unmask]<mailto:[log in to unmask]> with following text in
  the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
or
  (re-start) delivery of Technet send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET
  Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
  posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET
Technet Digest Search the
  archives of previous posts at:
http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please
  visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/cont
entpage.asp?Pageid=4.3.16> for
  additional information, or contact Keach Sasamori at
[log in to unmask]<mailto:[log in to unmask]> or
  847-615-7100 ext.2815
  -----------------------------------------------------

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 15.0
  To unsubscribe, send a message to
[log in to unmask]<mailto:[log in to unmask]> with following text
  in
  the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to
  [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or
(MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to
  [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
  Search the archives of previous posts at:
  http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
  Please visit IPC web site
 
http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/cont
entpage.asp?Pageid=4.3.16> for additional
  information, or contact Keach Sasamori at
[log in to unmask]<mailto:[log in to unmask]> or 847-615-7100
  ext.2815
  -----------------------------------------------------

  ---------------------------------------------------------------------
  This transmission (including any attachments) may contain confidential
  information, privileged material (including material protected by the
  solicitor-client or other applicable privileges), or constitute
  non-public information. Any use of this information by anyone other
than
  the intended recipient is prohibited. If you have received this
  transmission in error, please immediately reply to the sender and
delete
  this information from your system. Use, dissemination, distribution,
or
  reproduction of this transmission by unintended recipients is not
  authorized and may be unlawful.

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 15.0
  To unsubscribe, send a message to
[log in to unmask]<mailto:[log in to unmask]> with following text
  in
  the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to
  [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or
(MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to
  [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
  Search the archives of previous posts at:
  http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
  Please visit IPC web site
 
http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/cont
entpage.asp?Pageid=4.3.16> for additional
  information, or contact Keach Sasamori at
[log in to unmask]<mailto:[log in to unmask]> or 847-615-7100
  ext.2815
  -----------------------------------------------------

  ---------------------------------------------------------------------
  This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public information. Any use of this information by anyone other than
the intended recipient is prohibited. If you have received this
transmission in error, please immediately reply to the sender and delete
this information from your system. Use, dissemination, distribution, or
reproduction of this transmission by unintended recipients is not
authorized and may be unlawful.

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 15.0
  To unsubscribe, send a message to
[log in to unmask]<mailto:[log in to unmask]> with following text in
  the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
  Search the archives of previous posts at:
http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
  Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/cont
entpage.asp?Pageid=4.3.16> for additional information, or contact Keach
Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100
ext.2815
  -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2