It appears the Bow & Twist on a raw card/board is straight forward. " Push down on one side at a time and measure the deflection with a dial indicator on the opposite side". How about a finished assembly fully populated with BGA heat sinks and DIMM cards. The connector leads keep the card/board from laying flat on a flat plate. Even raised with three equal thickness spacers and locked at one side. The heaviest part of the card/board will drop. Victor, -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D. Sent: Monday, July 13, 2009 2:57 PM To: [log in to unmask] Subject: Re: [TN] Maximum Allowable Bow & Twist for PWB-PCB That is described in the test method referred to earlier. The bare PWB is easy, put it on a tool grade flat plate. Push down on one side at a time and measure the deflection with a dial indicator on the opposite side. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee parker Sent: Monday, July 13, 2009 1:37 PM To: [log in to unmask] Subject: Re: [TN] Maximum Allowable Bow & Twist for PWB-PCB Bev and Richard How do you suggest we measure to local bow and twist? Best regards Lee J. L. Parker Ph. D. JLP Consultants LLC 804 779 3389 ----- Original Message ----- From: Bev Christian<mailto:[log in to unmask]> To: [log in to unmask]<mailto:[log in to unmask]> Sent: Monday, July 13, 2009 12:53 PM Subject: Re: [TN] Maximum Allowable Bow & Twist for PWB-PCB Richard, Correct as usual, Richard. This was always a big deal at Nortel where completed circuit packs would have to be slotted into card cages. Bev On vacation ----- Original Message ----- From: Stadem, Richard D. <[log in to unmask]<mailto:[log in to unmask]>> To: [log in to unmask]<mailto:[log in to unmask]> <[log in to unmask]<mailto:[log in to unmask]>>; Bev Christian Sent: Mon Jul 13 11:06:30 2009 Subject: RE: [TN] Maximum Allowable Bow & Twist for PWB-PCB Bev, I totally agree with you, but the point they are getting at in IPC 2221 is that no section of the PWB should have more than .75% per inch as a rate of warpage, extending in both the X and Y directions, after reflow. This is because if you have more warpage than that you are putting a stress on the resultant solder joints that leads to a reduction in reliability, especially with a lead-free joint and also especially if you need to straighten the CCA when mounting it into a chassis or frame. I think this specification, like so many others that were based on leaded solder, should be revisited for unleaded solders. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian Sent: Friday, July 10, 2009 3:24 PM To: [log in to unmask]<mailto:[log in to unmask]> Subject: Re: [TN] Maximum Allowable Bow & Twist for PWB-PCB I contend this is old school and if you aren't measuring warpage at reflow temperatures how do you know you aren't suffering from head on pillow? I suggest the term head in pillow be dropped because you don't actually put your head IN a pillow. Bev RIM PS Waiting for my Dewism. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard Sent: Friday, July 10, 2009 4:20 PM To: [log in to unmask]<mailto:[log in to unmask]> Subject: Re: [TN] Maximum Allowable Bow & Twist for PWB-PCB IPC-2221 5.2.4 ... Unless otherwise specified by master drawing, max bow and twist shall be 0.75% for boards that use surface mount components and 1.5% for all other board technologies. ... Values are measured as per IPC-TM-650 Method 2.4.22 Genny Gibbard, P. Eng Manufacturing Engineer, Vecima PTS dept. x.4229 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez Sent: July 10, 2009 2:15 PM To: [log in to unmask]<mailto:[log in to unmask]> Subject: [TN] Maximum Allowable Bow & Twist for PWB-PCB What is the maximum allowable Bow & Twist value? Not able to locate in IPC-2221, 2222, & 6012A Victor, --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/cont entpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/cont entpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/cont entpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/cont entpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------