This is how we specify IWT.

IMMERSION WHITE TIN WITH A MINIMUM THICKNESS OF 0.65 MICRONS WITH A MAXIMUM
  THICKNESS OF 1.5 MICRONS

Steve Collins



                    "Marsico, James"
                    <James.Marsico@D        To:     [log in to unmask]
                    P.AIL.COM>              cc:
                    Sent by: TechNet        Subject:     Re: [TN] More about white tin (another question)
                    <[log in to unmask]
                    >


                    02/08/01 10:54
                    AM
                    Please respond
                    to "TechNet
                    E-Mail Forum.";
                    Please respond
                    to "Marsico,
                    James"






Is the immersion tin process the same as electroless plating?  How would
one
specify the IWT process on a board drawing?  Is there a Mil spec or
industry
spec which can be referenced?
Jim Marsico
Senior Engineer
Production Engineering
AIL/Electronics Systems Group
An EDO Company
[log in to unmask] <mailto:[log in to unmask]>

        -----Original Message-----
        From:   <Rudy Sedlak> [SMTP:[log in to unmask]]
        Sent:   Thursday, February 08, 2001 9:08 AM
        To:     [log in to unmask]
        Subject:        Re: [TN] More about white tin (another question)

        Ken:

        IWT, aka, immersion Tin, can be applied to any Copper based
substrate.  The
        plating process depends on Copper as a basis, and actually
dissolves
some
        Copper in the plating process.  IWT will always be more expensive
than
        electroplating, at least per pound of Tin Deposited, however the
relative
        cost per square foot depends on how much Tin you are
electroplating.
        Generally, IWT is a relatively expensive process, but since so
little Tin is
        deposited, on such a small area on printed circuit boards, it
becomes a
        detail cost.

        Rudy Sedlak
        RD Chemical Company


----------------------------------------------------------------------------

-----
        Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
        Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315

----------------------------------------------------------------------------

-----

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2