Mike Fenner <[log in to unmask]>
Parts/Attachments:
text/plain (106 lines)
SMART Group in UK through Bob Willis have loads of movies and CD on this and
other topics. Contact Tony Gordon on [log in to unmask]

Mike Fenner
Indium Corporation of Europe
T: + 44 1908 580 400
F: + 44 1908 580 411
M: + 44 7810 526 317
W: www.indium.com


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Bill Butman
Sent: Thursday, August 16, 2001 6:58 PM
To: [log in to unmask]
Subject: Re: [TN] Looking for short movie of a BGA self-centering


Hi Julien,

Check the following:  Pace, Inc.  9893 Brewers Court,
Laurel, MD 20723.  Tel 301-490-9860


I remember seeing the "self centering" of a BGA on a
Pace Film.

Jack Crawford at IPC may also be of help.  ("Your up",
Jack)

Thanx
Bill
--- Julien Bouchard <[log in to unmask]>
wrote:
> Hi everybody,
>         I already see in a presentation a short
> movie of a bga under x-ray that was
> reflowing and offset from his pads and you can see
> the BGA self-centering
> itself very well. I built a formation program for
> the rework and i looking
> for a movie or an animation like this to well
> explain the self-centering
> effect of BGA. Anybody got something ? Thank you.
>
> Julien Bouchard ing. stag.
> Matrox - Spicialiste de procidis
> Email : [log in to unmask]
>
>
----------------------------------------------------------------------------
-----
> Technet Mail List provided as a free service by IPC
> using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask]
> with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the
> following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line
> Resources & Databases > E-mail Archives
> Please visit IPC web site
> (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at
> [log in to unmask] or 847-509-9700 ext.5315
>
----------------------------------------------------------------------------
-----


=====
Bill Butman
Circuit Technology Center
45 Research Drive
Haverhill, MA 01832

__________________________________________________
Do You Yahoo!?
Make international calls for as low as $.04/minute with Yahoo! Messenger
http://phonecard.yahoo.com/

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2