We were encountering RDS (Resistance to Drain and Source) fall-outs
after Power Cylce (PRCL- 5K Cylcles).
All tests passed (TMCL, HAST, HTRB, HTGB) except this PRCL test.
The failure was the On resistance of the device which is already above the
limits required
by the Specs (but the device still functional).
Does anybody out there experinced this kind of fall-outs?
Would you agree that die attach voids could be a factor of the RDS
fall-outs?
But why not during prime class testing? And not fail during TMCL?
Or are there any experience that more than 10 % voids can cause failures
on Electrical performance?
I hope you can share your experiences
God Bless You All
thanks
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|