All,
Does anyone have any data on the relationship between solder balls (no 
clean flux w/ N2) and various solder masks?
Some of our lines run OK and some do not for the same mask. The hard 
part to understand is that a mask will run poorly on one line and OK on 
another. My feeling is that the mask is statistically significant, but 
not necessarily the major contributor. All DOE have shown no sweet spot, 
but of course going to aqueous or eliminating N2 have shown positive 
results. 
The other variable that has completely eliminated solder balls is to 
shorten leads to ~.080". This went over poorly with the connector 
people.