Hi Jim. My two cents worth are with regards to AVXs Transguard series of
components. They have a PdPtAg terminations the reference document is available
at
http://www.avxcorp.com/docs/techinfo/smttrsgd.pdf
We ended up using a secondary process and touched up the "questionable"
connections.
Alex
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Thursday, May 09, 2002 7:41 AM
To: [log in to unmask]
Subject: [TN] RePalladium Leads
- I have, as a consultant, dealt with a couple of cases of "non-wetting"
and/or "poor wetting" on palladium leads. Microsectional analysis ultimately
disclosed that "wetting" had occurred, but the visual cues customarily
associated with wetting of tin/lead solders were not in evidence. Faced with
the conventional "footprint in the mud" connection characteristics my
recommendation would be to conduct destructive physical analysis on a couple
of representative examples and confirm/deny the presence of wetting. You may
end up changing flux to achieve satisfactory wetting or you may need to
"calibrate" your inspection crew (not an easy chore). Hope the above helps
some.
Regards, Jim Moffitt, Moffitt Consulting, Noblesville, IN
--------------------------------------------------------------------------------
-
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
--------------------------------------------------------------------------------
-
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|