     Hi Pat-
     
     You don't need a special solder but rather a better flux. Nickel oxide 
     is very tough to solder because of the nature of the oxide itself 
     (very dense, coherent, etc.). You need to investigate using a more 
     active flux that can breakup the oxide. Warning -the more active the 
     flux, the more problems with corrosion. Work with your flux supplier 
     and find something a bit stronger than you are using now.
     
     
     Dave Hillman
     Rockwell Collins
     [log in to unmask]


______________________________ Reply Separator _________________________________
Subject: ASSY: SMT Soldering to Nickle pads
Author:  [log in to unmask] at ccmgw1
Date:    11/18/96 2:56 PM


Hello All:
     
Can anyone tell me about soldering SMT parts to Nickle plated copper pads. 
Is there a special solder alloy that I should use?
     
     
-Pat-
     
-------------
Patrick McGuine
Nicolet Instrument
[log in to unmask]
(608) 276-6334
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2