TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="us-ascii"
Old-Return-Path:
Date:
Tue, 14 May 1996 09:48:39 -0400
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
From [log in to unmask] Thu May 16 12:
58:43 1996
X-Mailing-List:
<[log in to unmask]> archive/latest/4127
X-Sender:
gary@gateway
TO:
Poh Kong Hui <[log in to unmask]>
Return-Path:
<TechNet-request>
Status:
O
X-Loop:
Resent-Message-ID:
<"mZNF_.0.J94.Wa9cn"@ipc>
Subject:
From:
Gary Ferrari <[log in to unmask]>
Received:
by ipc.org (Smail3.1.28.1 #2) id m0uJL7s-0000CeC; Tue, 14 May 96 09:31 CDT
Cc:
X-Mailer:
Windows Eudora Light Version 1.5.2
Message-Id:
Parts/Attachments:
text/plain (43 lines)
Is there any corrrelation with the gritty sodler joints and dip connections
to either the power or ground planes?

At 09:10 PM 5/14/96 +0800, Poh Kong Hui wrote:
>Dear Technet,
>
>Whenever, I'm running a 100% through-hole board, that is densely populated
>with mainly DIP components, and a only few capacitors and resistors., 20 to
>30% of the solder joints are gritty. 
>
>It had never happened to board of mixed technology.
>I have sent the solder for lab. analysis, and the result is within the
>recommended specification.
>
>The Board is :-
>10 x 10 sq.inch
>4 layers 
>
>The wave-solder Machine used :-
>The wave-solder machine used is SEHO 2000 - a full-blown nitrogenous tunnel.
>The solder pot temperature is set at 245 deg.cel or 473 deg.F.
>The top side temperature is measured at about 194 deg.F / 90 deg.C.
>Conveyor speed is set 0.90 metre/minute.
>The solid content of the flux is 1%.
>
>Could anybody advise me why this is happening, and how to solve it. Our
>rework operators are touching every gritty joint.
>
>
>Poh Kong Hui
>Nera Electronics
>
>
Regards,

Gary Ferrari