Hello technet.
This is our first design using silver filled via. We have used two different
PCB fab. A total of 7 lots have been done and the yield seen at our pcb fab
house has not improved (15%).
The major problem we have is generalized delamination after reflow (not
localized) that seems to happen around layers 4-5. Our pcb. Fab is currently
investigating on the causes. Until now , no satisfactory explanations has
been given to us.
* Have some of you been faced against the same problem (delamination
On silver filled via).
* Any possible Causes/solutions
* Any theories on the most probable cause (design/process/material
compatibility ...)
At this time, product release has been delayed.
Your help in this matter would be appreciated.
Board specification
Dimension : 6.5X9 inch board. 0.070" thickness
Sub sequential buildup Layer 5 to 12 with a total of 16 layers.
Silver epoxy filled via using dupont CB100 .
Qty of 7000 silver filled Via of 0.008"
Qty of 1000 silver filled Via of 0.010"
The populated boards has a very high thermal mass: 8 BGA . current of 96
Amps.
Impedance controlled and Burried capacitance
Line/Spacing : 0.003" / 0.005"
Best regards
Michel Arbour
Kontron
Tel. : 450-437-4661 ext. 2287
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|