TECHNET Archives

March 2003

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Arbour, Michel" <[log in to unmask]>
Date:
Mon, 10 Mar 2003 13:45:56 -0500
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Arbour, Michel" <[log in to unmask]>
Parts/Attachments:
text/plain (44 lines)
Hello technet.
This is our first design using silver filled via. We have used two different
PCB fab. A total of 7 lots have been done and the yield seen at our pcb fab
house has not improved (15%).
The major problem we have is generalized delamination after reflow (not
localized) that seems to happen around layers 4-5. Our pcb. Fab is currently
investigating on the causes. Until now , no satisfactory explanations has
been given to us.
*       Have some of you been faced against the same problem (delamination
On silver filled via).
*       Any possible Causes/solutions
*       Any theories on the most probable cause (design/process/material
compatibility ...)

At this time, product release  has been delayed.
Your help in this matter would be appreciated.

Board specification
Dimension : 6.5X9 inch board.  0.070" thickness
Sub sequential buildup Layer 5 to 12 with a total of 16 layers.
Silver epoxy filled via using dupont CB100 .
Qty of 7000 silver filled Via of 0.008"
Qty of 1000 silver filled Via of 0.010"
The populated boards has a very high thermal mass:  8 BGA . current of 96
Amps.
Impedance controlled and Burried capacitance
Line/Spacing : 0.003" / 0.005"

Best regards
Michel Arbour
Kontron
Tel. : 450-437-4661 ext. 2287

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2