You've a real uphill climb then. Most heaters use welded leads. You can get
away with "soft solders" if you use a length of the heater lead (usually a
poor thermal conductor) to get the soft solder interconnect into a cooler
area.
Wayne
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of McGlaughlin, Jeffrey A
Sent: Wednesday, April 01, 2015 10:51 AM
To: [log in to unmask]
Subject: Re: [TN] HIGH Temperature Solder
Unfortunately welding and brazing are not going to work for this
application. Working on a cable interface inside of a heater unit.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick
Sent: Wednesday, April 01, 2015 10:33 AM
To: [log in to unmask]
Subject: Re: [TN] HIGH Temperature Solder
How about welding??
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of McGlaughlin, Jeffrey A
Sent: Wednesday, April 01, 2015 10:20 AM
To: [log in to unmask]
Subject: [TN] HIGH Temperature Solder
I need to spec a high temperature wire solder for hand soldering. I need to
have a solidus of greater than 250 degrees C. Is 90Pb10Sn my best/only
choice or is there something else I should look at?
Jeffrey McGlaughlin, C.I.D.
Engineering Designer
Avionics Systems & Tech Refersh
Office: 614.424.7582| Fax: 614.458.7582
[log in to unmask]<mailto:[log in to unmask]>
Battelle
505 King Avenue
Columbus Ohio 43201-2693
http://www.battelle.org<http://www.battelle.org/>
Connect with Battelle
Facebook<http://www.facebook.com/battelle> |
LinkedIn<http://www.linkedin.com/company/battelle>
Twitter<http://www.twitter.com/Battelle> |
YouTube<http://www.youtube.com/user/battelleinnovations>
This message is intended only for the use of the individual or entity to
which it is addressed, and may contain information that is privileged,
confidential and/or otherwise exempt from disclosure under applicable law.
If the reader of this message is not the intended recipient or the employee
or agent responsible for delivering the message to the intended recipient,
any disclosure, dissemination, distribution, copying or other use of this
communication or its substance is prohibited. If you have received this
communication in error, please return to the sender and delete from your
computer system.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|