You've a real uphill climb then. Most heaters use welded leads. You can get away with "soft solders" if you use a length of the heater lead (usually a poor thermal conductor) to get the soft solder interconnect into a cooler area. Wayne -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of McGlaughlin, Jeffrey A Sent: Wednesday, April 01, 2015 10:51 AM To: [log in to unmask] Subject: Re: [TN] HIGH Temperature Solder Unfortunately welding and brazing are not going to work for this application. Working on a cable interface inside of a heater unit. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick Sent: Wednesday, April 01, 2015 10:33 AM To: [log in to unmask] Subject: Re: [TN] HIGH Temperature Solder How about welding?? -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of McGlaughlin, Jeffrey A Sent: Wednesday, April 01, 2015 10:20 AM To: [log in to unmask] Subject: [TN] HIGH Temperature Solder I need to spec a high temperature wire solder for hand soldering. I need to have a solidus of greater than 250 degrees C. Is 90Pb10Sn my best/only choice or is there something else I should look at? Jeffrey McGlaughlin, C.I.D. Engineering Designer Avionics Systems & Tech Refersh Office: 614.424.7582| Fax: 614.458.7582 [log in to unmask]<mailto:[log in to unmask]> Battelle 505 King Avenue Columbus Ohio 43201-2693 http://www.battelle.org<http://www.battelle.org/> Connect with Battelle Facebook<http://www.facebook.com/battelle> | LinkedIn<http://www.linkedin.com/company/battelle> Twitter<http://www.twitter.com/Battelle> | YouTube<http://www.youtube.com/user/battelleinnovations> This message is intended only for the use of the individual or entity to which it is addressed, and may contain information that is privileged, confidential and/or otherwise exempt from disclosure under applicable law. If the reader of this message is not the intended recipient or the employee or agent responsible for delivering the message to the intended recipient, any disclosure, dissemination, distribution, copying or other use of this communication or its substance is prohibited. If you have received this communication in error, please return to the sender and delete from your computer system. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________