Wayne Thayer <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (123 lines)
Scary! How can you guarantee the temperature won't get close to reflow of
the high temperature alloy? As I noted previously, I find it easier to
create good thermal isolation than to split hairs on the thermal model of an
area which gets anywhere near reflow.

Wayne

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of McGlaughlin, Jeffrey A
Sent: Wednesday, April 01, 2015 1:17 PM
To: [log in to unmask]
Subject: Re: [TN] HIGH Temperature Solder

Cost is not a primary concern(to be spoken like a true government
contractor) ;-D

The final product is considered Life Support/Mission Critical and failure is
not acceptable.
This design however is pushing the limit of what I consider solderable. I
have recommended We review a press-fit for production on it but and getting
pushback from the Mech Eng.

Jeff
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
Sent: Wednesday, April 01, 2015 12:59 PM
To: [log in to unmask]
Subject: Re: [TN] HIGH Temperature Solder

come on, Jeff, you can always go after Au-Sn...
                  jk;-)
> Hi Jeff - here are a couple of other choices:
>
> 10Sn88Pb2Ag
>
>
>
> 1Sn97.5Pb1.5Ag
>
>
>
> 97Pb3Ag
>
>
> Nothing wrong with you 90Pb10Sn either. Make sure you select a flux 
> core that has good thermal stability as your soldering temperatures 
> are much hotter than what you deal with when using the Sn63Pb37 alloy. 
> Also consider what the cleaning (or not cleaning) issues you may have 
> to deal with.
>
>
> Dave Hillman
>
> Rockwell Collins
>
> [log in to unmask]
>
> On Wed, Apr 1, 2015 at 9:20 AM, McGlaughlin, Jeffrey A < 
> [log in to unmask]> wrote:
>
>> I need to spec a high temperature wire solder for hand soldering. I 
>> need to have a solidus of greater than 250 degrees C. Is 90Pb10Sn my 
>> best/only choice or is there something else I should look at?
>>
>> Jeffrey McGlaughlin, C.I.D.
>> Engineering Designer
>> Avionics Systems & Tech Refersh
>> Office: 614.424.7582| Fax: 614.458.7582 
>> [log in to unmask]<mailto:[log in to unmask]>
>>
>> Battelle
>> 505 King Avenue
>> Columbus Ohio 43201-2693
>> http://www.battelle.org<http://www.battelle.org/>
>>
>> Connect with Battelle
>> Facebook<http://www.facebook.com/battelle> | LinkedIn< 
>> http://www.linkedin.com/company/battelle>
>> Twitter<http://www.twitter.com/Battelle> | YouTube< 
>> http://www.youtube.com/user/battelleinnovations>
>>
>> This message is intended only for the use of the individual or entity 
>> to which it is addressed, and may contain information that is 
>> privileged, confidential and/or otherwise exempt from disclosure 
>> under applicable law.
>> If the reader of this message is not the intended recipient or the 
>> employee or agent responsible for delivering the message to the 
>> intended recipient, any disclosure, dissemination, distribution, 
>> copying or other use of this communication or its substance is 
>> prohibited. If you have received this communication in error, please 
>> return to the sender and delete from your computer system.
>>
>>
>>
>>
>> _____________________________________________________________________
>> _ This email has been scanned by the Symantec Email Security.cloud 
>> service.
>> For more information please contact helpdesk at x2960 or 
>> [log in to unmask] 
>> _____________________________________________________________________
>> _
>>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask] 
> ______________________________________________________________________
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

ATOM RSS1 RSS2